| Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding |
WANG Haifeng1,2, ZHANG Zhiming1, NIU Yunsong2( ), YANG Yange2( ), DONG Zhihong2, ZHU Shenglong2, YU Liangmin1, WANG Fuhui3 |
1.Frontiers Science Center for Deep Ocean Multispheres and Earth System, and Key Laboratory of Marine Chemistry Theory and Technology, Ministry of Education, Ocean University of China, Qingdao 266100, China 2.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3.Shenyang National Key Laboratory for Materials Science, Northeastern University, Shenyang 110819, China |
|
Cite this article:
WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui. Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding. Acta Metall Sin, 2023, 59(10): 1355-1364.
|
|
|
Abstract Titanium alloys are used in the aerospace industries, chemical industries, biomedicine, marine ships and other fields because of their high strength-to-weight ratio, good corrosion resistance, and biocompatibility. However, titanium alloys have low hardness and poor wear resistance, which limit their applications, especially under sliding contact. Plasma nitriding (PN) is an effective method for improving titanium alloy's tribological properties. PN can produce a composite layer composed of TiN and Ti2N to improve the friction and wear properties of titanium alloy. However, the high temperature in the nitriding treatment results in a brittle “α-stabilized layer” (a continuous layer of α phase titanium enriched with interstitial nitrogen atoms) and unfavorable phase transformations in the substrate that can impair the fracture toughness, ductility, and fatigue properties. In this study, a low-temperature plasma-composite treatment, consisting of plasma oxidizing and oxynitriding, has been developed to improve the hardness and wear resistance of Ti-6Al-4V alloy. The effect of the preoxidation process on the surface microstructure, phase composition, and wear performance of titanium alloy was studied. The microstructure and phase composition of the plasma-composite layer were observed using SEM, TEM, XRD, and other methods. The results showed that the composite layer of titanium alloy treated using plasma-composite-treatment is composed of compound and diffusion layers, and the phase is TiO2 (rutile) and TiN0.26. Microhardness and wear-resistance properties of the composite layer were characterized using microhardness tester, nanoindentation, and reciprocating-friction tester. The plasma-composite treatment can increase infiltration depth of the diffusion layer, surface hardness, elastic modulus, and wear resistance of the titanium alloy more than the traditional nitriding process.
|
|
Received: 15 October 2021
|
|
|
| Fund: National Key Research and Development Program of China(2019YFC0312100);National Natural Science Foundation of China(51701223);Civil Aircraft Special Scientific Research Project(MJ-2017-J-99) |
Corresponding Authors:
NIU Yunsong, senior engineer, Tel: (024)23992860, E-mail: ysniu@imr.ac.cn; YANG Yange, associate professor, Tel: (024)23881473, E-mail: ygyang@imr.ac.cn
|
| 1 |
Zhu Z S, Shang G Q, Wang X N, et al. Microstructure controlling technology and mechanical properties relationship of titanium alloys for aviation applications [J]. J. Aeronaut. Mater., 2020, 40(3): 1
|
|
朱知寿, 商国强, 王新南 等. 航空用钛合金显微组织控制和力学性能关系 [J]. 航空材料学报, 2020, 40(3): 1
|
| 2 |
Chen J, Yan F Y, Wang J Z. Corrosion wear properties of TC4 titanium alloy in artificial seawater [J]. Tribology, 2012, 32(1): 1
|
|
陈 君, 阎逢元, 王建章. 海水环境下TC4钛合金腐蚀磨损性能的研究 [J]. 摩擦学学报, 2012, 32(1): 1
|
| 3 |
Wang M F, Lu X, Hou W L. Investigation on fatigue characteristics of TC4 titanium alloy tibia plate [J]. Agric. Equip. Veh. Eng., 2018, 56(3): 28
|
|
王孟飞, 卢 曦, 侯文亮. TC4钛合金胫骨板的疲劳特性研究 [J]. 农业装备与车辆工程, 2018, 56(3): 28
|
| 4 |
Ali M M, Raman S G S, Pathak S D, et al. Influence of plasma nitriding on fretting wear behaviour of Ti-6Al-4V [J]. Tribol. Int., 2010, 43: 152
doi: 10.1016/j.triboint.2009.05.020
|
| 5 |
Shen H Y, Wang L. Formation, tribological and corrosion properties of thicker Ti-N layer produced by plasma nitriding of titanium in a N2-NH3 mixture gas [J]. Surf. Coat. Technol., 2020, 393: 125846
doi: 10.1016/j.surfcoat.2020.125846
|
| 6 |
Nolan D, Huang S W, Leskovsek V, et al. Sliding wear of titanium nitride thin films deposited on Ti-6Al-4V alloy by PVD and plasma nitriding processes [J]. Surf. Coat. Technol., 2006, 200: 5698
doi: 10.1016/j.surfcoat.2005.08.110
|
| 7 |
Kang J J, Wang M Z, Yue W, et al. Tribological behavior of titanium alloy treated by nitriding and surface texturing composite technology [J]. Materials, 2019, 12: 301
doi: 10.3390/ma12020301
|
| 8 |
Borisyuk Y V, Oreshnikova N M, Berdnikova M A, et al. Plasma nitriding of titanium alloy Ti5Al4V2Mo [J]. Phys. Procedia, 2015, 71: 105
doi: 10.1016/j.phpro.2015.08.322
|
| 9 |
Marin E, Offoiach R, Regis M, et al. Diffusive thermal treatments combined with PVD coatings for tribological protection of titanium alloys [J]. Mater. Des., 2016, 89: 314
doi: 10.1016/j.matdes.2015.10.011
|
| 10 |
Raveh A, Hansen P L, Avni R, et al. Microstructure and composition of plasma-nitrided Ti-6Al-4V layers [J]. Surf. Coat. Technol., 1989, 38: 339
doi: 10.1016/0257-8972(89)90095-9
|
| 11 |
Grill A, Raveh A, Avni R. Layer structure and mechanical properties of low pressure r.f. plasma nitrided Ti-6Al-4V alloy [J]. Surf. Coat. Technol., 1990, 43-44: 745
doi: 10.1016/0257-8972(90)90017-7
|
| 12 |
Farokhzadeh K, Edrisy A. Fatigue improvement in low temperature plasma nitrided Ti-6Al-4V alloy [J]. Mater. Sci. Eng., 2015, A620: 435
|
| 13 |
Balasubramanian K, Bragadeesvaran S R, Adarsh S A, et al. Surface properties of Ti-6Al-4V alloy treated by plasma ion nitriding process [J]. Mater. Today: Proc., 2021, 45: 957
|
| 14 |
Qian J, Farokhzadeh K, Edrisy A. Ion nitriding of a near-β titanium alloy: Microstructure and mechanical properties [J]. Surf. Coat. Technol., 2014, 258: 134
doi: 10.1016/j.surfcoat.2014.09.044
|
| 15 |
Yildiz F, Yetim A F, Alsaran A, et al. Plasma nitriding behavior of Ti6Al4V orthopedic alloy [J]. Surf. Coat. Technol., 2008, 202: 2471
doi: 10.1016/j.surfcoat.2007.08.004
|
| 16 |
Leyland A, Matthews A. On the significance of the H / E ratio in wear control: A nanocomposite coating approach to optimised tribological behaviour [J]. Wear, 2000, 246: 1
doi: 10.1016/S0043-1648(00)00488-9
|
| 17 |
Musil J, Jirout M. Toughness of hard nanostructured ceramic thin films [J]. Surf. Coat. Technol., 2007, 201: 5148
doi: 10.1016/j.surfcoat.2006.07.020
|
| 18 |
Banerjee D, Williams J C. Perspectives on titanium science and technology [J]. Acta Mater., 2013, 61: 844
doi: 10.1016/j.actamat.2012.10.043
|
| 19 |
Issariyapat A, Visuttipitukul P, Song T T, et al. Tensile properties improvement by homogenized nitrogen solid solution strengthening of commercially pure titanium through powder metallurgy process [J]. Mater. Charact., 2020, 170: 110700
doi: 10.1016/j.matchar.2020.110700
|
| 20 |
Zheng C L, Xu Z, Xie X S, et al. Study on plasma oxygen permeation of titanium [J]. J. Univ. Sci. Technol. Beijing, 2002, 24: 44
|
|
郑传林, 徐 重, 谢锡善 等. 钛等离子渗氧研究 [J]. 工程科学学报, 2002, 24: 44
|
| 21 |
Yetim A F, Yildiz F, Vangolu Y, et al. Several plasma diffusion processes for improving wear properties of Ti6Al4V alloy [J]. Wear, 2009, 267: 2179
doi: 10.1016/j.wear.2009.04.005
|
| 22 |
Yang S S, Yang F, Chen M H, et al. Effect of nitrogen doping on microstructure and wear resistance of tantalum coatings deposited by direct current magnetron sputtering [J]. Acta Metall. Sin., 2019, 55: 308
|
|
杨莎莎, 杨 峰, 陈明辉 等. N掺杂对磁控溅射Ta涂层微观结构与耐磨损性能的影响 [J]. 金属学报, 2019, 55: 308
|
| 23 |
Rastkar A R, Shokri B. A multi-step process of oxygen diffusion to improve the wear performance of a gamma-based titanium aluminide [J]. Wear, 2008, 264: 973
doi: 10.1016/j.wear.2007.07.001
|
| 24 |
Wei N A, Wei C B, Dai M J, et al. Effect of rare earth content on the microstructure and friction properties of Ti6Al4V alloy by plasma nitriding [J]. Surf. Technol., 2020, 49(3): 148
|
|
韦乃安, 韦春贝, 代明江 等. 稀土含量对Ti6Al4V钛合金等离子渗氮层组织和摩擦学性能的影响 [J]. 表面技术, 2020, 49(3): 148
|
| 25 |
Rastkar A R, Bell T. Characterization and tribological performance of oxide layers on a gamma based titanium aluminide [J]. Wear, 2005, 258: 1616
doi: 10.1016/j.wear.2004.11.014
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|