| Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure |
Shixin XU1,2,3( ), Wei YU2, Shujia LI1, Kun WANG1, Qisong SUN1 |
1 Research Institute of Technology, Shougang Group Co., Ltd., Beijing 100043, China 2 Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083, China 3 Beijing Key Laboratory of Green Recyclable Process for Iron and Steel Production, Shougang Group Co., Ltd., Beijing 100043, China |
|
Cite this article:
Shixin XU, Wei YU, Shujia LI, Kun WANG, Qisong SUN. Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure. Acta Metall Sin, 2018, 54(8): 1113-1121.
|
|
|
Abstract As a new steel, nanobainite steel has favourable strength and good plasticity, but the bainite transformation needs a longer time, so as to severely slow production efficiency down. So, the research of acceleration methods of bainite transformation is of significance. In this work, in order to accelerate the bainite transformation rate, the 20% compression pre-deformation at 300~850 ℃ and isothermal transformation at 300 ℃ were conducted on a thermal simulator. The effects of pre-deformation temperature on nanobainite transformation kinetics and microstructure of the medium carbon nanobainite steel were investigated. The results showed that pre-deformation process obviously shortened the incubation time of bainite transformation. Low pre-deformation temperature could accelerate bainite transformation at whole isothermal region, while high pre-deformation temperature accelerated bainite transformation at the initial stage, and hindered bainite transformation at later stage. Bainite ferrite lath thickness was increased with decreasing pre-deformation temperature. The pre-deformation process increased the frequency of small angle grain boundary of bainite transformation microstructure, and the frequency of small angle grain boundary of low pre-deformation temperature was higher than that of high pre-deformation temperature. The kinetic parameters n of bainite transformation was calculated by the analytical model, the model of nucleation and growth were identified, the pre-deformation process changed the nucleation position of bainite transformation. The crystal corner nucleation was mainly obtained through low pre-deformation temperature, and the crystal edge and the crystal face nucleation were mainly obtained through high pre-deformation temperature.
|
|
Received: 30 November 2017
|
|
|
| Fund: Supported by Key Projects in the National Science & Technology Pillar Program during the 12th Five-Year Plan Period (No.2012BAE03B01) |
| [1] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Design of novel high-strength bainitic steels: Part 1[J]. Mater. Sci. Technol., 2001, 17: 512 | | [2] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Design of novel high-strength bainitic steels: Part 2[J]. Mater. Sci. Technol., 2001, 17: 517 | | [3] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Very strong low temperature bainite[J]. Mater. Sci. Technol., 2002, 18: 279 | | [4] | Caballero F G, Bhadeshia H K D H. Very strong bainite[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 251 | | [5] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Mechanical properties of low-temperature bainite [J]. Mater. Sci. Forum, 2005, 500-501: 285 | | [6] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Development of hard bainite[J]. ISIJ Int., 2003, 43: 1238 | | [7] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Acceleration of low-temperature bainite[J]. ISIJ Int., 2003, 43: 1821 | | [8] | Umemoto M, Furuhara T, Tamura I.Effects of austenitizing temperature on the kinetics of bainite reaction at constant austenite grain size in Fe-C and Fe-Ni-C alloys[J]. Acta Metall., 1986, 34: 2235 | | [9] | Bhadeshia H K D H. Nanostructured bainite[J]. Proc. R. Soc., 2010, 466A: 3 | | [10] | Yoozbashi M N, Yazdani S, Wang T S.Design of a new nanostructured, high-Si bainitic steel with lower cost production[J]. Mater. Des., 2011, 32: 3248 | | [11] | Bhadeshia H K D H, David S A, Vitek J M, et al. Stress induced transformation to bainite in Fe-Cr-Mo-C pressure vessel steel[J]. Mater. Sci. Technol., 1991, 7: 686 | | [12] | Matsuzaki A, Bhadeshia H K D H, Harade H. Stress affected bainitic transformation in a Fe-C-Si-Mn alloy[J]. Acta Metall. Mater., 1994, 42: 1081 | | [13] | Shipway P H, Bhadeshia H K D H. The effect of small stresses on the kinetics of the bainite transformation[J]. Mater. Sci. Eng., 1995, A201: 143 | | [14] | Xu Z Y.Effect of stress on bainitic transformation in steel[J]. Acta. Metall. Sin., 2004, 40: 113(徐祖耀. 应力对钢中贝氏体相变的影响[J]. 金属学报, 2004, 40: 113) | | [15] | Gong W, Tomota Y, Koo M S, et al.Effect of ausforming on nanobainite steel[J]. Scr. Mater., 2010, 63: 819 | | [16] | Gong W, Tomota Y, Adachi Y, et al.Effects of ausforming temperature on bainite transformation, microstructure and variant selection in nanobainite steel[J]. Acta Mater., 2013, 61: 4142 | | [17] | Ohtsuka H.Effects of strong magnetic fields on bainitic transformation[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 279 | | [18] | Bhadeshia H K D H, Edmonds D V. The bainite transformation in a silicon steel[J]. Metall. Trans., 1979, 10A: 895 | | [19] | Xu Q K.A study of the incomplete phenomenon of bainite transformation in a low carbon Fe-C-Mo alloy[J]. J. Chongqing Univ., 1987, (3): 59(徐启昆. 铁碳钼合金贝氏体转变不完全现象的研究[J]. 重庆大学学报, 1987, (3): 59) | | [20] | Johnson W A, Mehl R F.Reaction kinetics in process of nucleation and growth[J]. Trans. AIME, 1939, 135: 416 | | [21] | Avrami M.Kinetics of phase change. I General theory[J]. J. Chem. Phys., 1939, 7: 1103 | | [22] | Avrami M.Kinetics of phase change. II Transformation-time relations for random distribution of nuclei[J]. J. Chem. Phys., 1940, 8: 212 | | [23] | Avrami M.Granulation, phase change, and microstructure kinetics of phase change. III[J]. J. Chem. Phys., 1941, 9: 177 | | [24] | Sidel S M, Santos F A, Gordo V O, et al.Avrami exponent of crystallization in tellurite glasses[J]. J. Therm. Anal. Calorim., 2011, 106: 613 | | [25] | Quidort D, Bréchet Y J M. The role of carbon on the kinetics of bainite transformation in steels[J]. Scr. Mater., 2002, 47: 151 | | [26] | Liu F, Sommer F, Mittemeijer E J.An analytical model for isothermal and isochronal transformation kinetics[J]. J. Mater. Sci., 2004, 39: 1621 | | [27] | Liu F, Sommer F, Bos C, et al.Analysis of solid state phase transformation kinetics: Models and recipes[J]. Int. Mater. Rev., 2007, 54: 193 | | [28] | Liu F, Sommer F, Mittemeijer E J.Analysis of the kinetics of phase transformations; roles of nucleation index and temperature dependent site saturation, and recipes for the extraction of kinetic parameters[J]. J. Mater. Sci., 2007, 42: 573 | | [29] | Christian J W.The Theory of Transformations in Metals and Alloys[M]. 3rd Ed., Oxford: Elsevier Ltd., 2002: 546 | | [30] | Quidort D, Brechet Y J M. A model of isothermal and non isothermal transformation kinetics of bainite in 0.5% C steels[J]. ISIJ Int., 2002, 42: 1010 | | [31] | Zhang Z M, Cai Q W, Yu W, et al.Continuous cooling transformation behavior and kinetic models of transformations for an ultra-low carbon bainitic steel[J]. J. Iron Steel Res. Int., 2012, 19: 73 | | [32] | Wang Q C, Yang Z G, Li Z D.A theoretical analysis on effect of deformation above Ae3 to the nucleation of proeutectoid ferrite transformation[J]. Acta. Metall. Sin., 2007, 43: 344(王启超, 杨志刚, 李昭东. Ae3温度以上变形对先共析铁素体相变形核影响的理论分析[J]. 金属学报, 2007, 43: 344) | | [33] | Bhadeshia H K D H, Honeycombe R W K. Steels: Microstructure and Properties[M]. 3rd Ed., Oxford: Elsevier Ltd., 2006: 129 | | [34] | Legros M, Dehm G, Arzt E, et al.Observation of giant diffusivity along dislocation cores[J]. Science, 2008, 319: 1646 | | [35] | Bhadeshia H K D H. Bainite in Steels [M]. 2nd Ed., Cambridge: Cambridge University Press, 2001: 124 | | [36] | Singh S B, Bhadeshia H K D H. Estimation of bainite plate-thickness in low-alloy steels[J]. Mater. Sci. Eng., 1998, A245: 72 | | [37] | Hase K, Garcia-Mateo C, Bhadeshia H K D H. Bainite formation influenced by large stress[J]. Mater. Sci. Technol., 2004, 20: 1499 |
|