Abstract High entropy alloys (HEAs) origin from a new alloy design concept with multi-principal elements, which have attracted significant interests in the past decade. The high configurational entropy in HEAs results in simple solid solutions with fcc and bcc structures. Especially, the single solid solution CoCrFeNi alloy exhibits excellent properties in many aspects, such as mechanical properties, thermal stability, radiation resistance and corrosion resistance. The excellent corrosion resistance of CoCrFeNi alloy is ascribed to the single-phase structure and uniform element distribution coupled with much higher Cr content than stainless steel. The single-phase structure and uniform element distribution can prevent the occurrence of localized corrosion, and higher Cr content can protect the alloy surface better with the form of oxidation film. Moreover, the corrosion resistance of CoCrFeNi-based HEAs, such as CoCrFeNiAlx, CoCrFeNiCux, CoCrFeNiTix, have also been extensively investigated. In most CoCrFeNi-based HEAs, the elements of Co, Cr, Fe and Ni are with equal-atomic ratio. However, the equal-atomic ratio is not necessary to obtain satisfactory properties and to ensure the single fcc structure in Co-Cr-Fe-Ni system. Accordingly, it is essential to further consider the effect of alloying elements on the corrosion resistance in Co-Cr-Fe-Ni HEA. In this work, the effect of Co, Fe and Ni elements on the corrosion resistance of single fcc Co-Cr-Fe-Ni system with concentrated constitution but different atomic ratios in 3.5%NaCl solution are investigated by using LSCM and EIS. The potentiodynamic polarization results indicate that the increase of Fe and the decrease of Ni will decrease the passivation current density of the alloys when the Co and Cr contents are equal. With the increase of Co and the decrease of Ni, the alloys show smaller passivation current density and better corrosion resistance when the Fe and Cr contents are equal. With the decrease of Co and the increase of Fe and Ni, the alloys show higher corrosion potential and smaller corrosion tendency when the Cr content is constant. These results will be helpful for the design of corrosion resistant HEAs in NaCl aqueous solution.
|
|
Received: 22 September 2017
|
|
|
| Fund: Supported by National Key Research and Development Program of China (No.2016YFB0700300) and National Natural Science Foundation of China (Nos.51471133 and 51771149) |
| [1] | Zhang Y, Zuo T T, Tang Z, et al.Microstructures and properties of high-entropy alloys[J]. Prog. Mater. Sci., 2014, 61: 1 | | [2] | Murty B S, Yeh J W, Ranganathan S.High-Entropy Alloys[M]. London: Butterworth-Heinemann, 2014: 1 | | [3] | Yeh J W, Chen S K, Lin S J, et al.Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes[J]. Adv. Eng. Mater., 2004, 6: 299 | | [4] | Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213 | | [5] | Sohn S, Liu Y H, Liu J B, et al.Noble metal high entropy alloys[J]. Scr. Mater., 2017, 126: 29 | | [6] | Tsai M H, Yeh J W.High-entropy alloys: A critical review[J]. Mater. Lett., 2014, 2: 107 | | [7] | Shi Y Z, Yang B, Liaw P K.Corrosion-resistant high-entropy alloys: A review[J]. Metals, 2017, 7: 43 | | [8] | Xiang C, Wang J Z, Fu H M, et al.Corrosion behavior of several high-entropy alloys in high temperature high pressure water[J]. J. Chin. Soc. Corros. Prot., 2016, 36: 107(向超, 王家贞, 付华萌等. 几种高熵合金在核电高温高压水中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2016, 36: 107) | | [9] | Tang Z, Huang L, He W, et al.Alloying and processing effects on the aqueous corrosion behavior of high-entropy alloys[J]. Entropy, 2014, 16: 895 | | [10] | Kozak R, Sologubenko A, Steurer W.Single-phase high-entropy alloys—An overview[J]. Z. Kristallogr., 2015, 230: 55 | | [11] | Qiu Y, Thomas S, Gibson M A, et al.Corrosion of high entropy alloys[J]. NPJ Mater. Degrad., 2017, 1: 15 | | [12] | Wu Z, Bei H, Otto F, et al.Recovery, recrystallization, grain growth and phase stability of a family of FCC-structured multi-component equiatomic solid solution alloys[J]. Intermetallics, 2014, 46: 131 | | [13] | Chen Y Y, Hong U T, Yeh J W, et al.Selected corrosion behaviors of a Cu0.5NiAlCoCrFeSi bulk glassy alloy in 288 ℃ high-purity water[J]. Scr. Mater., 2006, 54: 1997 | | [14] | Chen Y Y, Duval T, Hong U T, et al.Corrosion properties of a novel bulk Cu0.5NiAlCoCrFeSi glassy alloy in 288 ℃ high-purity water[J]. Mater. Lett., 2007, 61: 2692 | | [15] | Hsu Y J, Chiang W C, Wu J K.Corrosion behavior of FeCoNiCrCux high-entropy alloys in 3.5% sodium chloride solution[J]. Mater. Chem. Phys., 2005, 92: 112 | | [16] | Lin C M, Tsai H L.Evolution of microstructure, hardness, and corrosion properties of high-entropy Al0.5CoCrFeNi alloy[J]. Intermetallics, 2011, 19: 288 | | [17] | Chou Y L, Yeh J W, Shih H C.Effect of molybdenum on the pitting resistance of Co1.5CrFeNi1.5Ti0.5Mox alloys in chloride solutions[J]. Corrosion, 2011, 67: 085002 | | [18] | Cheng J B, Liang X B, Xu B S.Effect of Nb addition on the structure and mechanical behaviors of CoCrCuFeNi high-entropy alloy coatings[J]. Surf. Coat. Technol., 2014, 240: 184 | | [19] | Shang C Y, Axinte E, Sun J, et al.CoCrFeNi(W1-xMox) high-entropy alloy coatings with excellent mechanical properties and corrosion resistance prepared by mechanical alloying and hot pressing sintering[J]. Mater. Des., 2017, 117: 193 | | [20] | Qiu X W, Wu M J, Liu C G, et al.Corrosion performance of Al2CrFeCoxCuNiTi high-entropy alloy coatings in acid liquids[J]. J. Alloys Compd., 2017, 708: 353 | | [21] | Wang P, Cai H N, Cheng X W.Effect of Ni/Cr ratio on phase, microstructure and mechanical properties of NixCoCuFeCr2-x (x=1.0, 1.2, 1.5, 1.8 mol) high entropy alloys[J]. J. Alloys Compd., 2016, 662: 20 | | [22] | Chou Y L, Yeh J W, Shih H C.The effect of molybdenum on the corrosion behaviour of the high-entropy alloys Co1.5CrFeNi1.5Ti0.5Mox in aqueous environments[J]. Corros. Sci., 2010, 52: 2571 | | [23] | Qiu X W, Liu C G.Microstructure and properties of Al2CrFeCoCuTiNix high-entropy alloys prepared by laser cladding[J]. J. Alloys Compd., 2013, 553: 216 | | [24] | He F, Wang Z J, Wu Q F, et al.Solid solution island of the Co-Cr-Fe-Ni high entropy alloy system[J]. Scr. Mater., 2017, 131: 42 | | [25] | Shang X L, Wang Z J, He F, et al.The intrinsic mechanism of corrosion resistance for FCC high entropy alloys[J]. Sci. China Technol. Sci., 2018, 61: 189 | | [26] | Hamdy A S, El-Shenawy E, El-Bitar T.Electrochemical impedance spectroscopy study of the corrosion behavior of some niobium bearing stainless steels in 3.5% NaCl[J]. Int. J. Electrochem. Sci., 2006, 1: 171 | | [27] | Kumar N, Fusco M, Komarasamy M, et al.Understanding effect of 3.5 wt.% NaCl on the corrosion of Al0.1CoCrFeNi high-entropy alloy[J]. J. Nucl. Mater., 2017, 495: 154 | | [28] | Shi Y Z, Yang B, Xie X, et al.Corrosion of AlxCoCrFeNi high-entropy alloys: Al-content and potential scan-rate dependent pitting behavior[J]. Corros. Sci., 2017, 119: 33 | | [29] | Kocijan A, Milo?ev I, Pihlar B.Cobalt-based alloys for orthopaedic applications studied by electrochemical and XPS analysis[J]. J. Mater. Sci.: Mater. Med., 2004, 15: 643 | | [30] | Sekine I, Chinda A.Comparison of the corrosion behavior of pure Fe, Ni, Cr, and type 304 stainless steel in formic acid solution[J]. Corrosion, 1984, 40: 95 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|