| [1] Pan J L. Electr Weld Mach, 2005; 35(9): 1(潘际銮. 电焊机, 2005; 35(9): 1)[2] Shan J G, Zhang J, Zheng S Q, Chen W Z, Ren J L. Acta Metall Sin, 2009; 45: 1006(单际国, 张靖, 郑世卿, 陈武柱, 任家烈. 金属学报, 2009; 45: 1006)[3] Chen Z H, Yan H G, Chen J HMagnesium Alloys. Beijing: Chemical Industry Press, 2004: 38(陈振华, 严红革, 陈吉华. 镁合金. 北京: 化学工业出版社, 2004: 38)[4] Zhao H, Debroy T. Weld J, 2001; 80(8): 204[5] Wahba M, Mizutani M, Kawahito Y, Katayama S. Mater Des, 2012; 33: 569[6] Shan J G, Zhang J, Zheng S Q, Chen W Z, Ren J L. Rare Met Mater Eng, 2009; 38(S3): 234(单际国, 张靖, 郑世卿, 陈武柱, 任家烈. 稀有金属材料与工程, 2009; 38(S3): 234)[7] Zhang J, Shan J G, Wen P, Ren J L. Chin J Lasers, 2011; 38(6): 1(张靖, 单际国, 温鹏, 任家烈. 中国激光, 2011; 38(6): 1)[8] Zhang J, Shan J G, Wen P, Ren J L. Trans China Weld Inst, 2011; 32(5): 17(张靖, 单际国, 温鹏, 任家烈. 焊接学报, 2011; 32(5): 17)[9] You G Q, Zhu J H, Guo Q, Long S Y. Spec Cast Nonferrous Alloys, 2009; 29: 729(游国强, 朱觉华, 郭 强, 龙思远. 特种铸造及有色合金, 2009; 29: 729)[10] Wu J T, You G Q, Guo Q, Long S Y. Hot Work Technol, 2011; 40(1): 117(武靖亭, 游国强, 郭强, 龙思远. 热加工工艺, 2011; 40(1): 117)[11] Shen J, You G Q, Long S Y, Pan F S. Mater Charact, 2008; 59: 1059[12] Min D, Shen J, Lai S Q, Chen J, Xu N, Liu H. Opt Laser Eng, 2011; 49(1): 89[13] Liao H M. Master Dissertation, Chongqing University, 2006(廖慧敏. 重庆大学硕士学位论文, 2006)[14] Xu S X, Wu S S, Li Q. Light Met, 2008; (8): 43(许四祥, 吴树森, 李庆. 轻金属, 2008; (8): 43)[15] Xu S X, Wu S S, Mao Y W. Spec Cast Nonferrous Alloys, 2007; 27: 11(许四祥, 吴树森, 毛有武. 特种铸造及有色合金, 2007; 27: 11)[16] Cao X, Jahazi M, Immarigeon J P, Wallace W. J Mater Process Technol, 2006; 171: 188[17] Yu K, Nakata K, Liao J. Sci Technol Weld Join, 2009; 14: 554[18] Renzhi M, Yoshio B. Chem Phys Lett, 2003; 370: 770[19] Tadao S, Hideo H, Tadashi E, Osamu F, Minoru L. J Mater Sci, 1981; 16: 1829[20] Jia Z, Zhang Z Q, Yue Q C, Cui J Z. Foundry, 2011; 60: 635(贾征, 张志强, 乐启炽, 崔建忠. 铸造, 2011; 60: 635)[21] Zeng K, Klassen T, Oelerich W, Bormann R. Int J Hydrogen Energ, 1999; 24: 989[22] Kimio K, Robert D, Pzhcke D. Metall Trans, 1985; 16B:359[23] Poirrer D K, Yeum K, Maples A L. Metall Trans, 1987;18: 1979[24] Wang X J, You G Q, Yang Z, Long S Y. Rare Met Mater Eng, 2012; 12 (accepted)(王向杰, 游国强, 杨智, 龙思远. 稀有金属材料与工程, 2012; 12 (已接收))[25] Chi C T, Chao C G, Liu T F, Wang C C. Sci Technol Weld Join, 2008; 13: 199[26] German D, Dmitriy D. Surface Phenomena in Fusion Welding Processes. German: CRC Press Taylor&Francis Group, 2006: 262[27] Triantafyllidis D, Li L, Stott F H. Appl Surf Sci, 2003; 208–209: 458 |