MICROSTURE AND PITTING CORROSION RESISTANCE OF UNS S32304 DUPLEX STAINLESS STEELS WELDED JOINT WITH PLASMA-ARC WELDING
HONG Jufeng, TAN Hua, CHEN Lindou, LI Jing, LI Li, JIANG Yiming
1) Department of Materials Science, Fudan University, Shanghai 200433
2) The Center of Analysis and Measurement, Fudan University, Shanghai 200433
Cite this article: 

HONG Jufeng TAN Hua CHEN Lindou LI Jing LI Li JIANG Yiming. MICROSTURE AND PITTING CORROSION RESISTANCE OF UNS S32304 DUPLEX STAINLESS STEELS WELDED JOINT WITH PLASMA-ARC WELDING. Acta Metall Sin, 2011, 47(11): 1445-1449.

Download:  PDF(2897KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Microstructure and pitting corrosion resistance of UNS S32304 duplex stainless steels welded joint with plasma-arc welding (PAW) were studied by means of OM, SEM, energy dispersive X-ray spectroscopy (EDX) and potentiostatic electrochemical technique. The results show that the microstructures of the heat-affected zone (HAZ) and fusion zone differ from the base metal greatly, with ferrite fraction greater than 70\%. Furthermore, a lot of nitrides are precipitated at the interface between ferrite and austenite phases and inside the ferrite grains. Consequently, pitting corrosion resistance of the welded joint declines obviously and pitting preferentially occurs at ferrite phase in the high temperature HAZ near the fusion line.
Key words:  duplex stainless steel      plasma-arc welding      microstructure      pitting corrosion     
Received:  17 May 2011     
Fund: 

Supported by National Natural Science Foundation of China (Nos.50871031, 51071049, 51131008 and 51134010), and Shanghai Principal Project of Advanced Technology Industry

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00314     OR     https://www.ams.org.cn/EN/Y2011/V47/I11/1445

[1] Cvijovic Z, Radenkovic G. Corros Sci, 2006; 48: 3887

[2] Liou R Y, Hsieh R I, Tsai WT. Corros Sci, 2002; 44: 2841

[3] Xu J L, Deng B, Sun T, Li J, Jiang Y M. Acta Metall Sin, 2010; 46: 380

(徐菊良, 邓博, 孙 涛, 李 劲, 蒋益明. 金属学报, 2010; 46: 380)

[4] Gooch T G. In: Lula ed., Duplex Stainless Steels. Metals Park, Ohio: ASM, 1983: 573

[5] Baeslack III W A, Lippold J C, Nelson D E. Weld J, 1986; 66: 241

[6] Ogawa T, Koseki T. Weld J, 1989; 68: 181

[7] Sridhar N, Flasche L H, Kolts J. Mater Perform, 1984; 23: 52

[8] Capello E, Chiarello P, Previtali B, Vedani M. Mater Sci Eng, 2003; A351: 334

[9] Deng B, Wang Z Y, Jiang Y M, Sun T, Xu J L, Li J. Corros Sci, 2009; 51: 2969

[10] Nowacki J, Lukojc A. Mater Charact, 2006; 56: 436

[11] Sathicrchinda M, Pettersson R, Wessman S, Pan J S. Corros Sci, 2010; 52: 179

[12] Nillson J O, Huhtala T, Jonsson P, Karlsson L, Wilson A. Metall Mater Trans, 1996; 27A: 2196

[13] Garzon C M, Ramirez A J. Acta Mater, 2006; 54: 3321

[14] Ramirez A J, Lippold J C, Brandi S D. Metall Mater Trans, 2003; 34A: 1575

[15] Craig E. Weld J, 1988; 67: 19

[16] Wang Y, Chen Q. J Mater Process Technol, 2002; 120: 270

[17] Urena A, Otero E, Utrilla M V, M´unez C J. J Mater Process Technol, 2007; 182: 624

[18] Deng B, Jiang Y M, Liao J X, Hao Y W, Zhong C, Li J. Appl Surf Sci, 2007; 253: 7369

[19] Tan H, Jiang Y M, Deng B, Sun T, Xu J L, Li J. Mater Charact, 2009; 60: 1049

[20] Tavares S S M, Scandian C, Pardal J M, Luz T S, Silva F J. Eng Fail Anal, 2010; 17: 1500

[21] Liou H Y, Hsieh R I, Tsai W T. Mater Chem Phys, 2002; 74: 33

[22] Weber L, Uggowitzer P J. Mater Sci Eng, 1998; A242: 222

[23] Perren R A, Suter T A, Uggowitzer P J, Weber L, Magdowski R, Bohni H, Speidel M O. Corros Sci, 2001; 43: 707

[24] Kordatos J D, Fourlaris G, Papadimitriou G. Scr Mater, 2001; 44: 401

[25] Cervo R, Ferro P, Tiziani A, Zuzzhi F. J Mater Sci, 2010; 45: 4378

[26] Ha H Y, Kwon H S. Electrochim Acta, 2007; 52: 2175
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[11] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!