| EFFECTS OF THERMAL MECHANICAL TREATMENT ON THE MICROSTRUCTURES AND HARDNESS OF AN Al–Zn–Mg–Cu ALLOY PLATE |
| ZHANG Yunya 1,2, DENG Yunlai 1,2, WAN Li 1,2, ZHANG Xinming 1,2 |
1. School of Materials Science and Engineering, Central South University, Changsha 410083
2. Key Laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University, Changsha 410083 |
|
Cite this article:
ZHANG Yunya DENG Yunlai WAN Li ZHANG Xinming. EFFECTS OF THERMAL MECHANICAL TREATMENT ON THE MICROSTRUCTURES AND HARDNESS OF AN Al–Zn–Mg–Cu ALLOY PLATE. Acta Metall Sin, 2011, 47(10): 1270-1276.
|
|
|
Abstract The effects of thermal mechanical treatment (TMT: solution–quenching–precipitation–rolling) on the morphology and the amount of the precipitates in an Al–7.81Zn–1.81Mg–1.62Cu alloy plate and the effects of those particles on the microstructures, textures and hardness have been studied. During TMT, MgZn2 particles with nano/submicron scales significantly inhibit the migration of sub–grain/grain boundaries but would not induce particle simulated nucleation (PSN) recrystallization. An appropriate TMT process results in the remarkable diminish of recrystallization and increases Vickers hardness by 15%.
|
|
Received: 23 March 2011
|
| Fund: Supported by National Basic Research Program of China (No.2010CB731700) |
| [1] Williams J C, Starke E A. Acta Mater, 2003; 51: 5775[2] Chakrabarti D J, Liu J, Sawtell R R, Venema G B. Mater Forum, 2004; 28: 969[3] Liu J. Mater Sci Forum, 2006; 519: 1233[4] Senkov O N, Bhat R B, Senkova S V, Schloz J D. Metall Mater Trans, 2004; 36: 2115[5] Hideo Y, Yoshio B. Trans Jpn Inst Met, 1982; 23: 620[6] Robson J D. Mater Sci Eng, 2002; A338: 219[7] Robson J D, Prangnel P B. Acta Mater, 2001; 49: 599[8] Morere B, Maurice C, Driver J, Shahani R. Mater Sci Forum, 1996; 217–222: 517[9] Deng Y L, Wan L, Zhang Y, Zhang X M. J Alloys Compd, 2010; 498: 88[10] Xiong C X, Wan L, Deng Y L, Zhang X M. J Cent China Univ (Sci Technol), 2010; 41: 465(熊创贤, 万里, 邓运来, 张新明. 中南大学学报(自然科学版), 2010; 41: 465)[11] Bunge H J. Texture Analysis in Materials Science. London: Butterworths, 1982: 44[12] L¨ucke K, Pospiech J, Virnich K H, Jura J. Acta Metall, 1981; 29: 167[13] Hu H E, Zhen L, Yang L, Shao W Z, Zhang B Y. Mater Sci Eng, 2008; A488: 64[14] Zhen L, Hua H E, Wang X Y, Zhang B Y, Shao W Z. J Mater Process Technol, 2009; 209: 754[15] Li X Z, Hansen V, Gjonnes J, Wallenberg L R. Acta Metall, 1999; 47: 2651[16] Komura Y, Tokunaga K. Acta Crystallogr, 1980; B36: 1548[17] Stiller K, Warren P J, Hansen V, Angenete J, Gjonnes J. Mater Sci Eng, 1999; A270: 55[18] Engler O, Sachot E, Ehrstrom J C, Reeves A, Shahani R. Mater Sci Technol, 1996; 12: 717[19] Doherty R D, Hughes D A, Humphreys F J, Jonas J J, Juul Jensen D, Kassner M E, King W E, McNelley T R, McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238: 219[20] Humphreys F J, Hatherly M. Recrystallization and Related Phenomena. 2nd Ed., Oxford, London: Pergamon Press, 2004: 86[21] Zhang X M, Deng Y L, Liu Y, Tang J G, Zhou Z P. Acta Metall Sin, 2005; 41: 947(张新明, 邓运来, 刘瑛, 唐建国, 周卓平.金属学报, 2005; 41: 947)[22] Deng Y L, Zhang X M, Liang X, Zhang Y. Adv Mater Res, 2007; 15–17: 929[23] Humphreys F J. Met Sci, 1979; 13: 136[24] Ørsund R, Nes E. Scr Metall, 1988; 22: 665 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|