| MICROSTRUCTURES AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED JOINTS OF ALUMINIUM ALLOY THICK PLATE WITH DIFFERENT WELDING STATES |
| XU Weifeng1; LIU Jinhe1;LUAN Guohong2; DONG Chunlin2 |
1.School of Materials and Engineering; Northwestern Polytechnical University; Xi’an 710072
2.China FSW Center; Beijing 100024 |
|
Cite this article:
XU Weifeng LIU Jinhe LUAN Guohong DONG Chunlin. MICROSTRUCTURES AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED JOINTS OF ALUMINIUM ALLOY THICK PLATE WITH DIFFERENT WELDING STATES. Acta Metall Sin, 2009, 45(4): 490-496.
|
|
|
Abstract Compared to fusion welding processes used in joining structural aluminum alloy, the friction stir welding (FSW) is an emerging solid state welding process which can lead to less distortion and residual stress owing to low heat input characteristic. In order to apply FSW in the aerospace field, the 2219 aluminum alloy in Al–Cu series, which has high–strength–weight ratio, resistance to stress corrosion cracking and superior cryogenic properties, and is an ideal material in the construction of liquid cryogenic rocket fuel tanks, has been welded in O condition (full annealing). Microstructures of weld nugget zones and mechanical properties of the slices in the three kinds of thick plate FSW joints, which are the flaw–free joint, the joint with flaw and the flaw–free joint after post weld heat treatment (PWHT), were studied. The tensile testing shows that the tensile strength σb and yield strength σ0.2 decrease from 160.8 and 96.8 MPa of the top part of the flaw free joint to 146 and 86 MPa of the bottom part, respectively, σb and σ0.2 decrease from 132.9 and 94 MPa of the top part of the joint with flaw to 126 and 78.8 MPa of the bottom part, respectively. σb of the middle of the flaw–free joint after PWHT is 243.8 MPa and σ0.2 of the top of the flaw–free joint after PWHT is 123.3 MPa, they are higher than those of the other parts. increases from 6.7%, 4.8% and 7.5% of the top parts of the flaw–free joint, joint with flaw and flaw–free joint after PWHT to 10.1%, 8.5% and 14% of the bottom parts of the joints, respectively. For the PWHT (500 ℃/50 min + 160℃/20 h) flaw–free joint, grains are more uniform and finer along the thickness direction in weld nugget zone, fractographs present deep dimples, most of the failure is ductile fracture, and the microhardness distribution has no obvious fluctuation. For the joint with flaw the mechanical properties decrease sharply, fractograph exhibits a ductile–brittle fracture morphology and the microhardnesses in slices are lower than those of the flaw–free joints.
|
|
Received: 13 October 2008
|
|
|
| Fund: Supported by China FSW Center Foundation(No. CFSWT–050410–55) |
| [1] Trzil J J. Weld J, 1969; 44: 395
[2] Nunes A C. Weld J, 1984; 63(9): 27
[3] Cabibbo M, McQueen H J, Evangelista E, Spigarelli S, Paola M D, Falchero A. Mater Sci Eng, 2007; A460–461:86
[4] Elangovan K, Balasubramanian V. Mater Sci Eng, 2007; A459: 7
[5] Peel M, Steuwer A, Preuss M, Withers P J. Acta Mater, 2003; 51: 4791
[6] Chen Y C, Liu H J, Feng J C. Trans Nonferrous Met Soc China, 2005, 15: 75
[7] Xu W F, Liu J H, Luan G H, Dong C L. Acta Metall Sin, 2008; 44: 1404
(徐韦锋, 刘金合, 栾国红, 董春林. 金属学报, 2008; 44: 1404)
[8] Zhang Z, Zhang H W. J Mater Process Technol, 2009; 209(1): 241
[9] Hassan Kh A A, Norman A F, Price D A, Prangnell P B. Acta Mater, 2003; 51: 1923
[10] Ren S R, Ma Z Y, Chen L Q. Acta Metall Sin, 2008; 44: 626
(任淑荣, 马宗义, 陈礼清. 金属学报, 2008; 44: 626)
[11] Tweed J H, Knott J F. Acta Metall, 1987; 35: 1401 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|