Abstract The structural ceramics can be classified as oxide ceramics, nitride ceramics and carbide ceramics, which all possess low density, high anti-wearability and strong ability of anti-high temperature erosion, so they are a kind of materials that can be used in severe environments. Their compositions, crystal structures and properties were simply introduced, and the present research progress as well as application was also reviewed.
|
|
Received: 09 October 2008
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.50375064) and “985 Project” of Jilin University |
| [1] Yin Y S, Zhang J D. Al2O3 Ceramic and Its Composites.Beijing: Chemical Industry Press, 2001: 1
(尹衍升, 张景德. 氧化铝陶瓷及其复合材料. 北京: 化学工业出版社, 2001: 1)
[2] Jiang D L. Fine Ceramic Materials. Beijing: China Logistics Publishing House, 2000: 48
(江东亮. 精细陶瓷材料. 北京: 中国物资出版社, 2000: 48)
[3] Wang L S. Special Ceramic. 2nd Ed., Changsha: Central South University of Technology Press, 2005: 146
(王零森. 特种陶瓷. 第2版, 长沙: 中南工业大学出版社, 2005: 146)
[4] Zhen W Y, Chen C D, Chen Z C. Inorg Chem Ind, 2000;32(1): 18
(郑文裕, 陈潮钿, 陈仲丛. 无机盐工业, 2000; 32(1): 18)
[5] Yin Y S, Li J. ZrO2 Ceramic and Its Composites. Beijing: Chemical Industry Press, 2004: 7
(尹衍升, 李嘉. 氧化锆陶瓷及其复合材料. 北京: 化学工业出版社, 2004: 7)
[6] Lange F F. J Mater Sci, 1982; 17: 240
[7] Rieth P H, Reed J S, Naumann AW. Am Ceram Soc Bull, 1976; 55: 717
[8] Chen D Q. China Ceram Ind, 1994; 1(2): 24
(陈达谦. 中国陶瓷工业, 1994; 1(2): 24)
[9] Zhang Y L, Ma J P. Handbook of Applied Ceramic Materials. Beijing: Chemical Industry Press, 2006: 319
(张玉龙, 马建平. 实用陶瓷材料手册. 北京: 化学工业出版社, 2006: 319)
[10] Wu M M, Xiao J J. Foshan Ceram, 2004; 14(5): 30
(吴明明, 肖俊建. 佛山陶瓷, 2004; 14(5): 30)
[11] Fan X M, Zhang C, Jiang D Y. Engineering Ceramic and Its Application. Beijing: China Machine Press, 2006: 56
(樊新民, 张骋, 蒋丹宇. 工程陶瓷及其应用. 北京: 机械工业出版社, 2006: 56)
[12] Du G C, Chen Y. Tool Eng, 2003; 37(9): 40
(杜国臣, 陈营. 工具技术, 2003; 37(9): 40)
[13] Yin S. Modern Ceramics and Its Application. Beijing: Beijing Science and Technology Press, 1990: 163
(殷声. 现代陶瓷及其应用. 北京: 北京科学技术出版社, 1990: 163)
[14] Oyama Y, Kamigaito O. Jpn J Appl Phys, 1971; 10: 1637
[15] Jack K H, Wilson W I. Nature Phys Sci, 1972; 238: 28
[16] Cai Y J, Liu J X, Shi F, Ma T C, Yang D Z. J Dalian Inst Light Ind, 1999; 18: 187
(蔡英骥, 刘敬肖, 史非, 马铁成, 杨大智. 大连轻工业学院学报, 1999; 18: 187)
[17] Du X H, Zhang G R, Sui Z T. China Ceram, 1997; 33(4): 39
(都兴红, 张广荣, 隋智通. 中国陶瓷, 1997; 33(4): 39)
[18] Xie P, Xue X X, Qu Y C, Wang Y J. Ceram Eng, 1998; 32(4): 38
(谢朋, 薛向欣, 瞿玉春, 王彦吉. 陶瓷工程, 1998; 32(4): 38)
[19] Jiang T, Xue X X, Yang J D. Refractories, 2001; 35(4): 45
(姜涛, 薛向欣, 杨建东. 耐火材料, 2001; 35(4): 45)
[20] She J H, Jiang D L. Ceram Eng, 1998; 32(3): 3
(佘继红, 江东亮. 陶瓷工程, 1998; 32(3): 3) |