| INFLUENCE OF SULFUR CONTENT AND MICROSTRUCTURE OF PIPELINE STEELS ON MECHANICAL PROPERTY AND H2S-RESISTANT BEHAVIOR |
| shen zhuo;Yu-hai Li;;; |
| 沈阳理工大学 |
|
Cite this article:
shen zhuo; Yu-hai Li. INFLUENCE OF SULFUR CONTENT AND MICROSTRUCTURE OF PIPELINE STEELS ON MECHANICAL PROPERTY AND H2S-RESISTANT BEHAVIOR. Acta Metall Sin, 2008, 44(2): 215-221 .
|
|
|
Abstract Developing high strength pipeline steels with good sulfide stress cracking (SSC) resistance is a hot topic of pipeline research. In this paper, the role of sulfur content on mechanical properties and SSC resistance of four pipeline steels, with different sulfur contents, i.e. 5, 17, 50,100 ppm respectively, was investigated; and the role of microstructure on these properties was discussed as well. The results showed that high sulfur content, more than 100 ppm, led to the formation of II type MnS inclusion and worsened fracture toughness, but it did not have bad influence on tensile properties and SSC resistance. Furthermore, coarsen carbonnitride, inclusion and even pearlite are potential hydrogen traps, but these are not the most important factors that influence SSC resistance of pipeline steel. Dislocations, especially motional dislocations without pinning effects of finely dispersed precipitates in acicular ferrite are hydrogen carrier and mainly transportation means of hydrogen, which results in the relatively poor SSC resistance of acicular ferrite microstructure.
|
|
Received: 25 April 2007
|
[1]Gao H L.The Pipeline Steel:Microstructure,Mechani- cal Property and Welding Ability.Xi'an:Shaanxi Science and Technology Press,1995:4 (高惠临编著.管线钢——组织、性能、焊接行为.西安:陕西科学技术出版社,1995:4) [2]Zhao M C,Yang K,Shan Y Y.Mater Sci Eng,2002;A335: 14 [3]Yoshie A,Fujioka M,Watanabe Y,Nishioka K,Morikawa H.ISIJ Int,1992;32:395 [4]Bott I D S,Souza L F G D,Eixeira J C G,Rios P R. Metall Mater Trans,2005;36A:443 [5]Hwang B,Kim Y G,Lee S,Kim N J,Yoo J Y.Metall Mater Trans,2005;36A:371 [6]Domizzi G,Anteri G,Garcia J O.Corros Sci,2001;43: 325 [7]Nakai Y,Kurahashi H,Emi T,Haida O.Trans ISIJ,1979; 19:401 [8]Ravi K,Ramaswamy V.Mater Sci Eng,1990;A129:87 [9]Pressouyer G M,Blondeau R,Primon G,Gadiou L.In: Interrante C G,Pressouyre G M eds,Current Solution to Hydrogen Problems in Steels,Metals Park,OH:ASM, 1982:212 [10]NACE Standard TM0177-96,Method B-NACE Standard Bent-Beam Test,1996 [11]Zhao M C,Shan Y Y,Qu J B,Yang K,Gao S,Zheng L. Acta Metall Sin,2001;37:179 (赵明纯,单以银,曲锦波,杨柯,高珊,郑磊.金属学报,2001;37:179) [12]Zhong Y,Wang Z J,Shan Y Y,Yang K.Chin J Mater Sci,2003;17:304 (钟勇,王忠军,单以银,杨柯.材料研究学报,2003;17:304) [13]Muddle B C,Cizek P,Wynne B P,Davies C H.Pro- ceedings from Materials Solution'97 on Accelerated Cool- ing/Direct Quenching of Steels,Indianapolis,Indiana: ASM International,1997:15 [14]Sharma U,Ivey D G.2000 International Pipeline Confer- ence,Calgary,Canada:ASME,2000:193 [15]Brown A,Jones C L.Corrosion,1984;40:3301 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|