| SCC OF X70 PIPELINE STEEL IN SIMULATED ACID SOIL ENVIRONMENT |
| LIU Zhi-yong;Xiaogang LI |
| 北京科技大学腐蚀与防护中心 |
|
Cite this article:
LIU Zhi-yong; Xiaogang LI. SCC OF X70 PIPELINE STEEL IN SIMULATED ACID SOIL ENVIRONMENT. Acta Metall Sin, 2008, 44(2): 209-214 .
|
|
|
Abstract In order to study the SCC susceptibility of X70 pipeline steel in solutions which simulated the acid soil environment of Yingtan, China, slow strain rate testing (SSRT), microstructural observation of fracture areas by SEM and potentiodynamic polarization curves were used here. SCC did occur in the as-received material, with a transgranular cracking mode charged with different cathodic potential.The applied cathodic polarization potential played a important role in facilitating the occurrence of SCC.X70 pipeline steel was little sensitive to SCC in a athodic potential condition, but tended to be attacked by pits and uniform corrosion. However, as the applied cathodic potential droped, a combined electrochemical reaction of athode and cathode controlled the SCC behaviour of X70 steel, and as the applied cathodic potential droped further, cathodic reaction controlled SCC origination of X70 only. At the combined electrochemical condition, cracks occurred with pits together, which were more crowded than those at single cathodic condition at which cracks originated by themselves.
|
|
Received: 14 June 2007
|
[1]Yang W.Corros Prot,2003;24:461 (杨武.腐蚀与防护,2003;24:461) [2]Fang B Y,Wang J Q.Acta Metall Sin,2001;37:454 (方丙炎,王俭秋,金属学报,2001;37:454) [3]Jack T R,Erno B,Krist K.Corrosion,2000;362:10 [4]Huang C B,Li G F,Yang W.Corros Prot,2005;26:1 (黄春波,李光福,杨武.腐蚀与防护,2005;26:1) [5]Manfredi C,Otegui J L.Eng Failure Anal,2002;9:495 [6]Xu C C,Chi L,Hu G,Huang J,Wang Z S.J Chin Soc Corros Prot,2005;25:20 (许淳淳,池琳,胡钢,黄杰,王紫色.中国腐蚀与防护学报,2005;25:20) [7]Chin D T,Sabde G M.Corrosion,1999;55:229 [8]Qiao L J,Luo J L,Mao X.Corrosion,1998;54:115 [9]Parkins R N,Blanchard Jr W K,Delanty B S.Corrosion, 1994;50:394 [10]Van Boven G,Chen W,Rogge R.Acta Mater,2007;55: 29 [11]Li X G,Du C W,Liu Z Y.Corrosion Behavior and Ex- premential Study of X70.Beijing:Science Press,2006: 13 (李晓刚,杜翠薇,刘智勇.X70钢的腐蚀行为与实验研究.北京:科学出版社,2006:13) [12]Parkins R N.Corros Sci,1980;20:147 [13]Nesic S,Postlethwaite J,Olsen S.Corrosion,1996;52: 280 [14]Gu B,Luo J,Mao X.Corrosion,1999;55:96 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|