| Lamellar Orientation Control of TiAl Alloys by Directional Solidification with a seed technique |
| ;;; |
| 西北工业大学 |
|
Cite this article:
;. Lamellar Orientation Control of TiAl Alloys by Directional Solidification with a seed technique. Acta Metall Sin, 2007, 43(12): 1287-1292 .
|
|
|
Abstract By using a seed crystal, the TiAl/Ti3Al lamellar orientation was aligned parallel to the growth direction in directionally solidified Ti-47Al alloys. The solidification behavior of hypo-peritectic and hyper-peritectic alloys in TiAl equilibrium phase diagram was studied, and the composition range of successful seeding of TiAl alloys was also determined. Through the lamellar microstructure examination of Ti-47Al alloys directionally solidified from Ti-43Al-3Si seed under the conditions of different growth rates, it was found that a successful seeding requires that the solid/liquid interface must be planer during solidification. This can be achieved by growing crystals at a sufficiently high thermal gradient in the liquid and at a sufficiently low growth rate. It showed that the seeding process easily failed if cells or dendrites formatted, new grains would nucleated or α grains with a preferred growth orientation of <0001> would protrude to the liquid, then the lamellar direction was changed.
|
|
Received: 28 March 2007
|
|
|
[1]Loria E A.Intermetallics,2000;8:1339 [2]Tang J C,He Y H,Liu W S,Zhou K C,Zhang J H,Lu S Q,Huang B Y.Rare Met Mater Eng,2003;32:209 (唐建成,贺跃辉,刘文盛,周科朝,张俊红,鲁世强,黄伯云.稀有金属材料与工程,2003;32:209) [3]Li C G,Fu H Z,Yu Q.Materials in Aerospace.Beijing: National Defence Industry Press,2002:16 (李成功,傅恒志,于翘.航空航天材料.北京:国防工业出版社,2002:16) [4]Guo F A,Vincent J,Zhang Y G,Chen C Q.Rare Met Mater Eng,2001;30:105 (郭富安,Vincent J,张永刚,陈昌麒.稀有金属材料与工程,2001;30:105) [5]Dong L M,Cui Y Y,Yang R.Acta Metall Sin,2002;38: 643 (董利民,崔玉友,杨锐.金属学报,2002;38:643) [6]Zhang Y G,Shi Y F,Chen G L.Intermetallics Struc- tural Materials.Beijing:National Defence Industry Press, 2001:716 (张水刚,饰雅芳,陈国良.结构材料与金属间化合物.北京:国防工业出版社,2001:716) [7]Yamaguchi M,Johnson D R,Lee H N,Inui H.Inter-metallics,2000;8:511 [8]Johnson D R,Masuda Y,Inui H,Yamaguchi M.Acta Mater,1997;45:2523 [9]Johnson D R,Inui H,Yamaguchi M.Acta Mater,1996; 44:2523 [10]Luo W Z,Shen J,Li Q L,Man W W,Zheng X Q,Liu L, Fu H Z.Acta Metall Sin,2006;42:1238 (罗文忠,沈军,李庆林,满伟伟,郑循强,刘林,傅恒志.金属学报,2006;42:1238) [11]Zheng X Q,Shen J,Ding H S,Chen R R,Xu X.Mater Rev,2005;19(3):118 (郑循强,沈军,丁宏升,陈瑞润,许雄.材料导报,2005;19(3):118) [12]Sun F S,Froes F H.Mater Sci Eng,2003;A345:262 [13]Kim M C,Oh M H,Lee J H,Inui H,Yamaguchi M,Wee D M.Mater Sci Eng,1997;A239-240:570 [14]Jung I S,Kim M C,Lee J H,Oh M H,Wee D M.Inter- metallics,1999;7:1247 [15]Hunziker O,Vandyoussefi M,Kurz W.Acts Mater,1998; 46:6325 [16]Li S M,Liu L,Li X L,Fu H Z.Acts Metall Sin,2004;40: 20 (李双明,刘林,李晓历,傅恒志.金属学报,2004;40:20) [17]Fu H Z,Li X Z,Liu C,Su Y Q,Li S M,Guo J J.Chin J Nonferrous Met,2005;15:495 (傅恒志,李新中,刘畅,苏彦庆,李双明,郭景杰.中国有色金属学报,2005;15:495) [18]Fu H Z,Su Y Q,Guo J J,Xu D M.Acts Metall Sin,2002; 38:1127 (傅恒志,苏彦庆,郭景杰,徐达鸣.金属学报。2002;38:1127) [19]Liu C,Su Y Q,Li X Z,Guo J J,Jia J,Fu H Z.Acta Metall Sin,2005;41:260 (刘畅,苏彦庆,李新中,郭景杰,贾均,傅恒志.金属学报,2005;41:260) [20]Johnson D R,Inui H,Yamaguchi M.Intermetsllics,1998; 6:647 [21]Luo W Z,Shen J,Li Q L,Man W W,Fu H Z.Acts Metall Sin,2007;43:897 (罗文忠,沈军,李庆林,满伟伟,傅恒志.金属学报,2007;43:897) [22]Rutter J W,Chalmers B.Can J Phys,1953;31:29 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|