| Grain Boundary Character Distributions (GBCD) of Cold-Rolled Pb--Ca--Sn--Al Alloy |
| WANG Weiguo; ZHOU Bangxin; FENG Liu; ZHANG Xin; XIA Shuang |
| School of Mechanical Engineering ; Shandong University of Technology; Zibo 255049 |
|
Cite this article:
WANG Weiguo; ZHOU Bangxin; FENG Liu; ZHANG Xin; XIA Shuang. Grain Boundary Character Distributions (GBCD) of Cold-Rolled Pb--Ca--Sn--Al Alloy. Acta Metall Sin, 2006, 42(7): 715-721 .
|
|
|
Abstract Grain boundary character distribution (GBCD) of cold-rolled Pb-Ca-Sn-Al alloy during recovery and recrystallization was investigated by means of electron back scatter diffraction (EBSD).The results indicate straight ∑3 boundaries of over 60% (length fraction of total boundaries, the same as follows) are introduced in the alloy during recovery. Such boundaries are not distributed in the network of general high angle boundaries (HABs) and the GBCD are not optimized. Conversely, in the recrystallization, apart from ∑3 boundaries of over 65% , a fairly amount of ∑9 and ∑27 coincidence site lattice (CSL) boundaries are appeared. ∑9 and ∑27 boundaries along with a great deal of curved ∑3 boundaries are located in the network of HABs and the GBCD are optimized. Further discussion pointed out the straight ∑3 boundaries formed in recovery are <111>60°coherent twin boundaries, they are stable and immobile. While, the ∑3 boundaries developed in recrystallization comprised of not only coherent twin boundaries but also most of incoherent ones. The migration of incoherent ∑3 boundaries as well as the interaction between them result in the formation of ∑9,∑27 and other ∑3n (n is a positive integer) boundaries, and it is the root of GBCD optimization.
|
|
Received: 05 September 2005
|
|
|
[1] Palumbo G, Erb U. MRS Bull, 1999; 11: 27 [2] Watanabe T. Res Mech, 1984; 11: 47 [3] Lin P, Palumbo G, Erb U,Aust K T.Scr Metall Mater, 1995; 33: 1387 [4] King W E,Schwarts A J. Scr Mater, 1997; 38: 449 [5] Lehockey E M, Limoges D, Palumbo G, Sklarchuk J,Tomantschger K, Vincze A. J Power Source,1999;78:79 [6] Shimada M, Kokawa H, Wang Z J, Sato Y S,Karibe I.Acta Mater, 2002; 50: 2331 [7] Brandon D G, Ralph B,Ranganathan S, Wald M S. Acta Metall, 1964; 12: 813 [8] Randle V, Davies H, Cross I. Current Opinion Solid StateMater Sci, 2001; 5: 3 [9] Davies H, Randle V. J Microscopy, 2002; 205: 253 [10] Randle V, Davies P, Hulm B. Philos Mag, 1999; 79A: 305 [11] Randle V. Scr Mater, 2001; 44: 2789 [12] Randle V, Hu Y. J Mater Sci, 2005; 40: 3243 [13] Ke T S. Solid State Theory of Internal Friction. Beijing:Science Press, 2000: 460 (葛庭燧.固体内耗理论基础.北京:科学出版社,2000:460) [14] Kuhlmann-Wilsdorf D. Mater Sci Eng, 1989; A113: 1 [15] Yu Y N. The Principles of Metal Science. Beijing: Metallurgical Industry Press , 2000: 409 (余永宁.金属学原理.北京:冶金工业出版社,2000:409) [16] Hu H. Recovery and Recrystallization of Metals.New York: Chapman & Hall, 1963: 344 [17] Thomoson C B,Randle V.Acta Mater,1997;45:4909 [18] Randle V.Acta Mater,1999; 47: 4187 [19] Kumar M,Schwarts A J,King W E.Acta Mater,2002;50: 2599 [20] Don J,Majumdar S. Acta Metall, 1984; 34: 961 [21] Lee D S, Ryoo S H, Hwang S K. J Mater Eng, 2003; 354A: 106 [22] Palumbo G, Aust K T. In: Weiland H, Wolf D eds., Grain Growth in Polycrystalline,Warrendale, PA: TMS, 1998:311 [23] Watanabe T. Bull Jpn Inst Met, 1992; 31: 138 [24] Xia S, Zhou B X, Chen W J, Wang W G. Acta Metall Sin,2006; 42: 129 (夏爽,周邦新,陈文觉,王卫国.金属学报,2006;42:129) [25] Harase J. Can Metall Q, 1995; 34: 185K |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|