| Research on Grain Refinement Mechanism in Undercooled Fe75Ni25 Alloy |
| CHEN Yuzeng; YANG Gencang;LI Feng; LIU Ning; XIE Hui; ZHOU Yaohe |
| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
CHEN Yuzeng; YANG Gencang; LI Feng; LIU Ning; XIE Hui; ZHOU Yaohe. Research on Grain Refinement Mechanism in Undercooled Fe75Ni25 Alloy. Acta Metall Sin, 2006, 42(7): 703-707 .
|
|
|
Abstract The grain refinement mechanisms of undercooled Fe75Ni25 alloys were investigated by fluxing and cyclic superheating. Within the undercooling, T, range achieved, two kinds of grain refinement were observed. In combination with the calculation and the analysis of experiment results, the grain refinement mechanisms were elucidated. The results indicate that the first grain refinement, occurring if T>56K, can be ascribed to the breakup of dendrite-skeleton owing to remelting, whereas the second grain refinement was caused by recrystallization induced by the stress originating from the rapid solidification contraction with T>209K.
|
|
Received: 09 October 2005
|
|
|
[1] Herlach D M.Mater Sci Eng, 1994; R12: 177 [2] Walker J L.In: Pierre G L St,ed.,The Physical Chemistry of Process Metallurgy(Part 2),NY:Interscience, 1959: 845 [3] Li J F, Yang G C, Zhou Y H.Mater Res Bull,1998; 33: 141 [4] Dragnevski K I,Cochrane R F, Mullis A M. Mater Sci Eng, 2004; A375-377: 479 [5] Schwarz M,Karma A,Eckler K,Herlach D M.Phys Rev Lett, 1994; 73: 1380 [6] Liu Fe, Yang G C, Guo X F. Mater Sci Eng, 2001; A311:54 [7] Li J F, Liu Y C, Lu Y L, Yang G C, Zhou Y H. J Cryst Growth, 1998; 192: 462 [8] Eckler K, Norman A F, Gartner F, Greer A L, Herlach D M. J Cryst Growth, 1997; 173: 528 [9] Liu N, Yang G C, Chen Y Z, Zhou Y H. Prog Nat Sci,2006; 16(1): 120 (刘宁,杨根仓,陈豫增,周尧和,自然科学进展,2006;16(1): 120) [10] Jackson K A, Hunt J D, Uhlmann D R, Stewart T P.TMS-AIME, 1966; 236: 149 [11] Horvay G. Int J Heat Mass Transfer, 1965; 8: 195 [12] Kobayashi K F, Hogan L M. Met Forum, 1978; 1: 165 [13] Karma A. Int J Non-Equilib Process, 1998; 11: 201 [14] Mullis A M, Cochrane R F. J Appl Phys, 1997; 82: 1380 [15] Herlach D M, Eckler K, Karma A, Schwarz M. Mater Sci Eng, 2001; A304-306: 20 [16] Zambon A,Badan B,Eckler K, Gartner F,Norman A F,Greer A L,Herlach D M,Ramous E. Acta Mater,1998;46: 4657 [17] Chuang Y Y and Chang Y A. Met Trans, 1987; 18A: 733 [18] Chen Y Z, Yang G C, Liu F, Liu N, Xie H, Zhou Y H. J Cryst Growth, 2005; 282: 490 [19] Boettinger W J,Coriell S R,Trivedi R. In: Mehrabian R,Parrish P A, eds., Rapid Solidification Processing:Principles and Technologies IV, Baton Rouge, LA: Claitor's Pulishing Division,1988: 13 [20] Branders E A.Smithells Metals Reference Book. 6th ed.,London: Butterworths,1991 [21] Piccone T J, Wu Y, Shiohara Y, Flemings M C. Metall Trans, 1987; 18A: 925 [22] Aziz M J. J Appl Phys, 1982; 53: 1154 [23] Willnecker R, Herlach D M, Feuerbacher B. Appl Phys Lett, 1990; 56: 324 [24] Barth B, Eckler K, Herlach D M, Alexander H. Mater Sci Eng, 1991; A133: 790 [25] Powell G L F. TMS-AIME, 1969; 245: 1785O |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|