| PREPARATION OF TANTALUM BY ELECTRO-DEOXIDATION IN A CACL2-NACL MELT |
|
Cite this article:
. PREPARATION OF TANTALUM BY ELECTRO-DEOXIDATION IN A CACL2-NACL MELT. Acta Metall Sin, 2006, 42(3): 285-289 .
|
|
|
Abstract Tantalum was prepared by electro-deoxidation in a CaCl2-NaCl melt at 800℃. Ta2O5 powders were compacted in to pellets and sintered, and then conducted as a cathode, while a high-density graphite rod as an anode. It was investigated that the porosity and micro-morphology of the sintered Ta2O5 cathode affected the rate of the electro-chemical reduction and the purity of the product. The results showed that high porosity can increase the rate and extent of electro-deoxidation. The diffusion seemed to play an important role in the reduction process.
|
|
Received: 29 June 2005
|
|
|
[1] He J L. Eng Sci, 2001; 3(12): 85 (何季麟.中国工程科学, 2001;3(12):85) [2] Cardonne S M, Kumar P, Michaluk C A, Schwartz H D . Int J Refract Met Hard Mater, 1995; 13: 187 [3] Liu S Y. Rare Met Cem Carbides, 1998; 26(2): 55 (刘世友.稀有金属与硬质合金, 1998;26(2):55) [4] He J L. Chin J Rare Met, 2003; 27(1): 23 (何季麟.稀有金属,2003;27(1):23) [5] Ye F W. Mater Rev, 1997; 11(2): 27 (叶方伟.材料导报,1997;11(2):27) [6] Hu Z W, Li Z K, Zhang T J , Zhang X M. Rare Met Cem Carbides, 2003; 31(3): 34 (胡忠武,李中奎,张廷杰,张小明.稀有金属与硬质合金,2003; 31(3):34) [7] He J L . Chin J Nonferrous Met, 2004; 14(S1): 291 (何季麟.中国有色金属学报, 2004;14(专辑s1):291) [8] 《A Handbook for Extractive Metallurgy of Nonferrous Metals》Editorial Committee. A Handbook for Extractive Metallurgy of Nonferrous Metals-Zr, Hf, Nb, Ta, V. Vol.2, Beijing: Metallurgical Industry Press, 2002: 223 《有色金属提取冶金手册》编辑委员会.有色金属提取冶金手 册——稀有高熔点金属(下).北京;冶金工业出版社,2002: 223) [9] Chen G Z, Fray D J, Farthing T W. Nature, 2000; 407: 361 [10] Chen G Z, Gordo E, Fray D J. Metall Mater Trans, 2004; 35B: 223 [11] Gordo E, Chen G Z, Fray D J. Electrochim Acta, 2004; 49: 2195 [12] Yan X Y, Fray D J. Metall Mater Trans, 2002; 33B: 685 [13] Yan X Y, Fray D J. J Electrochem Soc, 2005; 152: D12 [14] Muir Wood A J, Copcutt R C, Chen G Z, Fray D J. Adv Eng Mater, 2003; 5: 650 [15] Fray D J, Farthing T W, Chen Z. UK International Patent, PCT/GB99/01781, 1998 [16] Liang Y J, Che Y C, Liu X X, Li N J. Thermochemical Properties of Inorganic Substance. Shenyang: Northeastern University Press, 1993: 467 (梁英教,车荫昌,刘晓霞,李乃军.无机物热力学数据手册. 沈阳:东北大学出版社, 1993:467) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|