| THE ANALYSIS OF THE RELATIONSHIP BETWEEN IRON RESOURCE EFFICIENCY OF STEEL PRODUCTION PROCESS AND OF ITS UNIT PROCESS |
| daitiejun |
|
Cite this article:
daitiejun. THE ANALYSIS OF THE RELATIONSHIP BETWEEN IRON RESOURCE EFFICIENCY OF STEEL PRODUCTION PROCESS AND OF ITS UNIT PROCESS. Acta Metall Sin, 2006, 42(3): 280-284 .
|
|
|
Abstract Based on the concept of iron-flow diagram of steel production process, a relational expression between iron resource efficiency of steel production process and of its unit process has been derived. By using the data of a steel plant, the relationship between iron resource efficiency of steel production process and of its unit process was analyzed, and the influence of iron resource efficiency of unit process on iron resource efficiency of steel production process was discussed as examples.
|
|
Received: 30 August 2005
|
|
|
[1]Zhang S R.Res Iron Steel,2002;30(2):1 (张寿荣.钢铁研究,2002;30(2):1) [2] Zhang X Y.Metall Manag,2003;(8):14 (张训毅.冶金管理, 2003;(8):14) [3] Chen J B. Geol Seek, 2004; 19(1): 5 (陈甲斌.地质找矿论丛, 2004;19(1):5) [4] Kleijn R. J Ind Ecol, 1999; 3(2, 3): 8 [5] Ayres R U. Resour Conseru Recycling, 1997; 21: 145 [6] Huang S L, Hsu W L. Landscape Urban Plann, 2003; 63: 61 [7] Fischer-Kowalski M. J Ind Ecol, 1998; 2(1): 61 [8] Fischer-Kowalski M, Hyttler W. J Ind Ecol, 1998; 2(4): 107 [9] de Marco O, Lagioia G, Mazzacane E P. J Ind Ecol , 2000; 4(2): 55 [10] Maenpaa I, Juutinen A. J Ind Ecol, 2001; 5(1): 33 [11] Spatari S, Bertram M, Fuse A K, Graedel T E, Rechberger H. Ecol Econo, 2002; 42: 27 [12] Hekkert M P, Joosten L A J, Worrell E. Resour Conser Recycling, 2000; 30: 29 [13] Michaelis P, Jackson T. Resour Conseru Recycling, 2000; 29: 131 [14] Michaelis P, Jackson T. Resour Conseru Recycling, 2000; 29: 209 [15] Yin R Y. Metallurgical Process Engineering. Beijing: Metallurgical Industry Press, 2004: 115 (殷瑞钰.冶金流程工程学.北京:冶金工业出版社,2004:115) [16] Lu Z W, Cai J J, Yu Q B, Xie A G. Acta Metall Sin, 2000; 36: 370 (陆钟武,蔡九菊,于庆波,谢安国.金属学报,2000;36:370) [17] Lu Z W. Acta Metall Sin, 2002; 38: 58 (陆钟武.金属学报,2002;38:58) [18] Lu Z W, Dai T J. Iron Steel, 2005; 40(4): 1 (陆钟武,戴铁军.钢铁,2005;40(4):1) [19] Dai T J, Lu Z W. Acta Metall Sin, 2004; 40: 1127 (戴铁军,陆钟武.金属学报,2004;40:1127) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|