Abstract Microstructure and mechanical properties of a cast Ni-32Al-28Cr-3Mo-4Ti eutectic alloy have been investigated. The results show that the alloy consists of NiAl and Cr(Mo) eutectic zone, as well as a small amount of primary NiAl and Ni2AlTi. Its compressive yield strength surpasses Dy-doped NiAl-Cr(Mo) eutectic alloy, and is comparable to NiAl-28Cr-5Mo-1Hf eutectic alloy, indicating the addition of Ti is benefit to the strength of NiAl-Cr(Mo) eutectic alloy. Similar to the relationship between minimum creep rate and applied stress, the creep rupture life at 1000℃ vs. applied stress fits linear dual-logarithmic relationship. Modified Monkman-Grant equation can be used to describe the relationship between creep rupture life and minimum creep rate. The fracture mechanism at room temperature is cleaving of NiAl and Cr(Mo) eutectic phases as well as stripping of NiAl/Cr(Mo) interface, while the formation and aggregation of microvoids on eutectic boundaries leads to crept fracture.
|
|
Received: 14 March 2006
|
|
|
[1]Cline H E,Walter J L,Lifshinand E,Russell R.Metall Trans,1971;2:189 [2]Cline H E,Walter J L.Metall Trans,1970;1:2907 [3]Cline H E,Walter J L,Koch E F,Osika L M.Acta Metall,1971;19:405 [4]Johnson D R,Chen X F,Oliver B F,Noebe R D,Whit- ??tenberger J D.Intermetallics,1995;3:99 [5]Yang J M,Jeng S M,Bain K,Amato R A.Acta Mater,1997;45:295 [6]Chen X F,Johnson D R,Noebe R D,Oliver B F.J Mater Res,1995;10:1159 [7]Raj S V,Locci I E,Whittenberger J D.In:Hember K J,Dimiduk D M,Clemens H,Darolia R,Inui H,Larsen J M,Sikka V K,Thomas M,Whittenberger J D,eds,Structural Intermetallics 2001,TMS,2001:785 [8]Whittenberger J D,Locci I E,Raj S V,Salem J A.Metall Mater Trans,2002;33A;1385 [9]Walston W S,Darolia R.In:Hember K J,Dimiduk D M,Clemens H,Darolia R,Inui H,Larsen J M,Sikka V K,Thomas M,Whittenberger J D,eds,Structural Intermetallics 2001,TMS,2001 [10]Darolia R.Intermetallics,2000;8:1321 [11]Guo J T,Cui C Y,Zhou L Z,Li G S.Acta Metall Sin,2002;38:1157(郭建亭,崔传勇,周兰章,李谷松.金属学报,2002;38:1157) [12]Cui C Y,Guo J T,Qi Y H,Ye H Q.Intermetallics,2002;10:1001 [13]Xu C M,Guo J T,Fu H Z.Acta Metall Sin,2004;40:57(徐春梅,郭建亭,傅恒志.金属学报,2004;40:57) [14]Polvani R S,Tzeng W S,Strutt P R.Metall Trans,1976;7A:33 [15]Zhang G Y.PhD Dissertation.Institute of Metal Research,Chinese Academy of Sciences,Shenyang,2004:39(张光业.中国科学院金属研究所博士学位论文,沈阳,2004:39) [16]Cui C Y,Chen Y X,Guo J T,Li D X,Ye H Q.Mater Eng,2001;1(1):3(崔传勇,陈玉喜,郭建亭,李斗星,叶恒强.材料工程,2001;1(1):3) [17]Guo J T.Ordered Intermetallic NiAl Alloys.Beijing:Science Press,2004:335(郭建亭.有序金属间化合物镍铝合金.北京:科学出版社,2004:335) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|