Abstract Using an industrial pulsed DC plasma chemical vapor deposition set-up, Ti-Si-C-N
coatings were deposited on substrate of high speed steel. The effect of SiCl4 flow rate on chemical composition, microstructure and phases in Ti-Si-C-N coatings was explored by means of XRD, XPS, TEM and SEM. It is suggested that Ti-Si-C-N coatings are of nanocomposite structure composed of nc-Ti(C, N)/a-C/a-Si3N4. The crystalline sizes are in the range of 2-25 nm. When nitrogen content in the coatings was very low, Ti(C, N) changed to TiC and the surface morphologies of Ti-Si-C-N coatings changed from granular grains to strip-shaped grains.
|
|
Received: 31 January 2005
|
|
|
[1] Ma D Y,Ma S L, Xu K W. Surf Coat Technol, 2004; 184:182 [2] Ma D Y, Ma S L, Xu K W.Acta Metall Sin,2004;40: 1037 (马大衍,马胜利,徐可为.金属学报, 2004;40:1037) [3] Ma D Y, Ma S L , Xu K W. Acta Metall Sin,2003;39: 1047 (马大衍,马胜利,徐可为.金属学报, 2003;39:1047) [4] Heim D, Holler F, Mitterer C. Surf Coat Technol,1999; 116: 530 [5] Veprek S. Thin Solid Films,1995;268:64 [6] Ma D Y, Ma S L, Xu K W. Tribology, 2003; 215: 476 (马大衍,马胜利,徐可为.摩擦学报,2003;23:476) [7] Ma S L, Ma D Y, Xu K W. Tribology, 2003; 23: 179 (马胜利,马大衍,徐可为.摩擦学报, 2003;23:179) [8] Veprek S. Vaccum, 2002;67:443 [9] Ma S L, Xu K W. Acta Metall Sin, 2004;40:669 (马胜利,徐可为.金属学报,2004;40:669) [10] Ma S L, Xu K W, Jie W. J Vac Sci Technol, 2004; 22B: 1694 [11] Karvankova P. Doctor Degree Thesis,Technical Univer sity Munich, Germany, 2003 [12] Niu X P. Master Degree Thesis, Xi'an Jiaotong University, 2004 (牛新平.西安交通大学硕士学位论文, 2004) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|