| MONTE--CARLO SIMULATION ON THE PRIMARY CRYSTALLIZATION OF BINARY AMORPHOUS SYSTEM |
| CHEN Jianqi; WANG Weimin; ZHANG Liang; BIAN Xiufang |
| Key Laboratory of Liquid Structure and Heredity of Materials; Ministry of Education; Shandong University; Jinan 250061 |
|
Cite this article:
CHEN Jianqi; WANG Weimin; ZHANG Liang; BIAN Xiufang. MONTE--CARLO SIMULATION ON THE PRIMARY CRYSTALLIZATION OF BINARY AMORPHOUS SYSTEM. Acta Metall Sin, 2004, 40(7): 741-744 .
|
|
|
Abstract The primary crystallization of binary system was simulated by the Monte--Carlo method. The crystallized phase radius is a linear relationship with the square root of the time, which corresponds exactly with academic formula. The simulated results of the primary crystallization patterns show that the crystallized aggregation degree has a good relativity with the diffusion parameter, and nucleation parameters, while the growth parameter affects the circinal degree
strongly.
|
|
Received: 22 July 2003
|
|
|
[1] Lu K. PhD Dissertation, Institute of Metal Research, The Chinese Academic of Sciences, Shenyang, 1989(卢柯.中国科学院金属研究所博士学位论文,沈阳,1989) [2] Ye F, Lu K. J Non-Crystalline Solids, 2000; 262: 228 [3] Landau D P, Binder K. A Guide to Monte Carlo Simulation in Statistic Physics, Cambridge University Press, 2000 [4] Karma A. Phys Rev Lett, 1987; 59: 71 [5] Liu J M, Liu Z G. Mater Lett, 1997; 32: 67 [6] Wang W M, Liu J M, Chen X Y, Liu Z G. J Cryst Growth,2002; 240: 313 [7] Das A, Mittemeijer E J. Metall Mater Trans A, 2000; 31A:2049 [8] Luborsky F E. Translated by Ke C, Tang Y C, Luo Y, He K Y. Amorphous Metallic Alloys, Beijing: Metallurgy Industry Press, 1989: 210(Luborsky F E著,柯成,唐与谌,罗阳,何开元译.非晶态金属合金.北京:冶金工业出版社, 1989:210) [9] Feng D. Physics of Metals, Phase Transformation. Vol.4, Beijing: Science Press, 1998: 156(冯端.金属物理学.第2卷,北京:科学出版社,1998:156) [10] Das A, Mittemeijer E J. Philos Mag A, 2001; 81: 2725P |