| STUDY OF (Ti,Al)N COATINGS ON SiCp/Al SUBSTRATE |
| ZHENG Jingdi; ZOU Yousheng; SONG Guihong; GONG Jun; LIU Yue; SUN Chao; WEN Lishi |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
ZHENG Jingdi; ZOU Yousheng; SONG Guihong; GONG Jun; LIU Yue; SUN Chao; WEN Lishi. STUDY OF (Ti,Al)N COATINGS ON SiCp/Al SUBSTRATE. Acta Metall Sin, 2004, 40(7): 745-748 .
|
|
|
Abstract (Ti,Al)N coatings with interlayers were deposited on SiCp/2024Al composites by arc ion plating at different negative bias voltages. The phase constitution, lattice constant and the composition of the coatings prepared at different negative bias voltages were analyzed. It is shown that (Ti, Al)N
coatings have preferred orientation
changed from (111) to (200) and (220)
with increasing of negative bias voltage. The
coating with Ti interlayer exhibits well adherence to the substrate compared with TiAl interlayer. To gain thick coating with 105 um, the (Ti, Al)N coating with a gradient nitrogen component was designed.
|
|
Received: 02 July 2003
|
|
|
[1] Lloyd D J. Inter Mater Rev, 1994; 39(1) : 1 [2] Palmers J, Stappen M V. Surf Coat Technol, 1995; 76/77:363 [3] Shew B Y, Huang J L. Surf Coat Technol, 1995; 71(1) : 30 [4] Cheng Y H, Tay B K, Lau S P, Shi X, Chua H C. ThinSolid Films, 2000; 379: 76 [5] Sant S B, Gill K S. Surf Coat Technol, 1994; 68/69: 152 [6] Mclntyre D, Greene J E, Hansson G, Sundgren J E, MnzW D. J Appl Phys, 1990; 67: 1542 [7] Sundgren J E, Hentzell H T G. J Vac Sci Technol, 1986;A4(5) : 2259 [8] Lee D N. J Mater Sci, 1989; 24: 4375 [9] Tian M B, Liu D L. Handbook of Science and Technologyof Films, Beijing: China Machine Press, 1980: 402(田民波,刘德令.薄膜科学与技术手册.北京:机械工业出版社,1980:402) [10] Starling C M D, Branco J R T. Thin Solid Films, 1997; 308-309: 436 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|