| STUDY OF HYPERFINE-FIELD ON NEW HIGH STRENGTH HIGH FRACTURE TOUGHNESS STEEL G99 |
| GENG Ping;ZENG Meiguang;QIAN Cunfu;CHAO Yuesheng (Sciences College; Northeastern University; Shenyang 110006) |
|
Cite this article:
GENG Ping;ZENG Meiguang;QIAN Cunfu;CHAO Yuesheng (Sciences College; Northeastern University; Shenyang 110006). STUDY OF HYPERFINE-FIELD ON NEW HIGH STRENGTH HIGH FRACTURE TOUGHNESS STEEL G99. Acta Metall Sin, 1998, 34(2): 216-220.
|
|
|
Abstract Variations of hyperfine-field with tempering temperature for high strength high fracture toughness steel G99 were studied by Mossbauer spectroscopy. The precipitation of alloy carbides was observed and analyzed by TEM and EDS. The results show that the distribution ofhyperfine-field and the quality of carbides and austenite within steel G99 vary with increasing tempering temperature. These are mainly caused by the increase of Fe atoms neighboring with Co or Ni, the decrease of Fe atoms neighboring with Cr or Mo, the solution of cementite, the precipitation of alloy carbides and the arising of reverted austenite. The important factors that the steel G99 has superior combinstion of strength and toughness are the precipitation of fine alloy carbides M2C, the arising in small amouats of reverted austenite, and well-distributed Co and Ni atoms in tempered martensite.
|
|
Received: 18 February 1998
|
1Garrison W M Jr, Moody N R. Metall Trans, 1987; 18A: 1257 2 Handerhan K J, Garrison W M Jr, Moody N R. Metall Trans A, 1989; 20A: 105 3 Ayer R, Machmeier P M. Metall Trans A, 1993; 24A: 1943 4凌斌,钟平,钟炳文,古宝珠.金属学报,1995;31:A209 (Ling B, Zhong P, Zhong B W, Gu B Z. Acta Metall Sin, 1995; 31: A209) 5李士著,穆斯堡尔谱学方法学与数据处理,兰州:兰州大学出版社,1990:33(Li S.Mossbauer Spectrum Methods and Data Treatment , Langhou:Lanzhou University,Press.1990:33) 6 Mathalone Z, Roy M, Pipman J.J Appl Phys, 1971; 42: 687 7苏杰.冶金工业部钢铁研究总院博士学位论文,1995 (Su J. Doctor thesis, Central Iron & Steel Research Institute, MMI, 1995) 8 Mendis E F, Andesrson L W. Phys Rev Lett, 1967; 19: 1434 9 Shirly D A, Rosenblum S S, Matthias E. Phys Rev, 1968; 170: 363 10Vincze I, Campbell I A.J Phys F: Metal Phys, 1973; 3: 647 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|