| IMPROVEMENT OF SHORT-FIBRE REINFORCED COMPOSITE MATERIALS WITH WEAK INTERFACE |
| SUN Xuekun;ZHOU Benlian;WANG Guodong (Institate of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(International Centre for Materials Physics; Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110015)(State Key Laboratory of Rolling and Automation; Northeastern University; Shenyang 110006) |
|
Cite this article:
SUN Xuekun;ZHOU Benlian;WANG Guodong (Institate of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(International Centre for Materials Physics; Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110015)(State Key Laboratory of Rolling and Automation; Northeastern University; Shenyang 110006). IMPROVEMENT OF SHORT-FIBRE REINFORCED COMPOSITE MATERIALS WITH WEAK INTERFACE. Acta Metall Sin, 1998, 34(2): 211-215.
|
|
|
Abstract The improvement of short-fibre reinforced composite materials under weak interface was discussed. Comparison between plain short-fibre model and dumbbell short-fibre model has been done. Effectivity of dumbbell model under different strength ratios of mains to fibre was discussed. born abate element analysis it was concluded that dumbbell model could well improve the performance of composite materials with weak interface. The lower strength ratio of mains to fibre, the better -improvement is.
|
|
Received: 18 February 1998
|
1Zhou B L, Shi C X. In: Kong M, Hung L eds, Proceedings of C-MRS Iuter, '90, Amsterdam: Elsevier Science Publishers, 1991: 137 2田晓滨.赵晓鹏周本濂.金属学报,1994;30:180(Tian x B,Zhao X P, Zhou B L. Acta Metall Sci,1994;30: 180) 3赵晓鹏,田晓滨,周本濂.金属学报,1994;30:187(Zhao X P, Tian X B, Zhou B L. Acta Metall Sin, 1994; 30: 187) 4 Fukuda H, Chai T W.J Comp Mater, 1981;15: 79 5 Chon C T, Sun C T.J Mater, Sci 1980; 15: 931 6 Broutman L J,Agarwal B D. Polymer Eng Sci 1974; 14: 581 7 Agarwal B D, Nansal R K. Fibre Sci Tech, 1979; 12: 149 8孙雪坤,郭燕阳,杜善义,林德春.复合材料学报,1997;14:116 (Sun X K, Guo Y Y, Du S Y, Lin D C. Acta Mater. Composite Sin 1997; 14: 116) 9Chang F K,Kutlu Z.J Comp Mater ,1989;23:11 10徐次达,华伯浩.固体力学有限元理论方法及程序,北京:水利电力出版社,1983 (Xu C D, Hua B H. Program and Finite Element Analysis Method of Solid Mechanics , Beijing, Water Conservancy & Elactric Power Publisher, 1983: 130)d |