Acta Metall Sin  1998, Vol. 34 Issue (2): 221-224    DOI:
Current Issue | Archive | Adv Search |
POSITRON ANNIHILATION STUDY ON THE EFFECT OF MISCH METAL IN Al-Fe-V-Si-Mm ALLOYS
JIA Wei;XIONG Lianggue;ZENG Meiguang;WANG Jiangiang (Department of Materials Science; College of Science; Northeastern University; Shenyang 110006)(International Center for Materials Physics; Institute of Matal Research; The Chinese Academy of Sciences;Shenyang 110015)
Cite this article: 

JIA Wei;XIONG Lianggue;ZENG Meiguang;WANG Jiangiang (Department of Materials Science; College of Science; Northeastern University; Shenyang 110006)(International Center for Materials Physics; Institute of Matal Research; The Chinese Academy of Sciences;Shenyang 110015). POSITRON ANNIHILATION STUDY ON THE EFFECT OF MISCH METAL IN Al-Fe-V-Si-Mm ALLOYS. Acta Metall Sin, 1998, 34(2): 221-224.

Download:  PDF(368KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The positron lifetime spectra of several Al-Fe-V-Si-Mm alloys with different content of Misch metal was measured, and the effect of the amount of Misch metal on the positron lifetime in Al-Fe-V-Si-Mm alloys was discussed.
Key words:  positron annihilation      Misch metal(Mm)      Al-Fe-V-Si alloy     
Received:  18 February 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I2/221

1Davis L A, Das S K, Li J C M, Zedalis M S. Inter,J Rapid Solidifi, 1994; 8: 110
2 Das S K and Froes F H. In: Liebermain H H ed., Rapidly Solidified Alloys, Marcel Dekker Inc, 1993: 339
3曾梅光,王建强,钱存富,张宝金,陈秀芳94秋季中国材料讨论会文集,1994;12:660(Zeng M G,Wang J Q,Qian C F,Zhang B J,Chen X F. ’94 C-MRS Materials Conference Proceedings.1994;12:660)
4 Kirgarrd P, Eldtup M, Mogensen O E, Peterson N. Comput Phys Commun,1981; 23: 307
5 Sui M L, Xiong L Y, Deng W, Lu K, Pain S, He Y Z.J Appl Phys, 1991;69: 4451
6 Sui M L, Lu K, Deng W, Xiong L. Y, Patu S, He Y Z. Phys Rev 1991; 44B: 6466
7Liu X D,Wang J T,Zhu J.J Mater Sci,1994;29:929
8 Wang J Q, Chao Y S, Zeng M G, Zhang B J, Chen X F.J Rare Earth, 1996; 14: 201
9Lu K.Mater,Sci Eng,1996;R16:161
10 MacKenziet I K. In: Brandt W, Dupasquier A eds, Positron Solid-state Physics, North-Holland Publishing CO, 1983: 200
11 Schaefer H E,Wurschum R,Birringer R,Gleiter H. Phys Rev,1988;38:9545T
[1] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[2] TIAN Xuefen, LIU Xiang, GONG Min, ZHANG Peiyuan, WANG Kang, DENG Aihong. Defect Evolution in H/He Neutral Beam Irradiated W-ZrC Alloy Using Positron Annihilation Spectroscopy[J]. 金属学报, 2021, 57(1): 121-128.
[3] Tianci ZHANG, Haitao WANG, Zhengcao LI, Henk SCHUT, Zhengming ZHANG, Ming HE, Yuliang SUN. Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation[J]. 金属学报, 2018, 54(4): 512-518.
[4] Kang WANG,Aihong DENG,Min GONG,Xiaobo LU,Yuanyuan ZHANG,Xiang LIU. Effect on Microstructure of Tungsten Under Helium Ions Irradiation with Multiple Energy[J]. 金属学报, 2017, 53(1): 70-76.
[5] LIU Yang, XIANG Wei, WANG Boyu. EFFECT OF IRRADIATION WITH PULSED ION BEAM ON THE MICROSTRUCTURE OF TiH2[J]. 金属学报, 2013, 49(10): 1269-1274.
[6] WANG Xiaoyong, PAN Tao, WANG Hua, SU Hang,LI Xiangyang, CAO Xingzhong. INVESTIGATION OF THE TOUGHNESS OF LOW CARBON TEMPERED MARTENSITE IN THE SURFACE OF Ni-Cr-Mo-B ULTRA-HEAVY PLATE STEEL[J]. 金属学报, 2012, 48(4): 401-406.
[7] WANG Boyu XIANG Wei TAN Xiaohua DAI Jingyi CHENG Liang QIN Xiubo. EFFECT OF D+ BEAM IRRADIATION ON Ti FILM[J]. 金属学报, 2010, 46(7): 810-813.
[8] ZHANG Lanzhi; WANG Baoyi; WANG Danni; WEI Long; LIN Junpin; WANG Wenjun. STUDIES OF Nb–TiAl ALLOY BY POSITRON ANNIHILATION TECHNIQUES[J]. 金属学报, 2007, 43(3): 269-272 .
[9] Jian Zhang. STUDY OF HYDROGEN EMBRITLLEMENT IN Fe-Ni BASED ALLOY THROUGH POSITRON ANNIHILATION LIFETIME TEST[J]. 金属学报, 2006, 42(5): 469-473 .
[10] DENG Wen; RUAN Xiangdong; HUANG Yuyang; ZHOU Yin'e; ZHU Yingying; ZHU Yingying. Effects Of Twin Size On The Dislocation Configuration During Cyclic Deformation Of Polycrystalline Twin Copper[J]. 金属学报, 2005, 41(1): 33-.
[11] WANG Jianqiang; ZENG Meiguang;CAO Yuesheng;ZHANG Baojin (Northeastern University; Shenyang 110006) HU Zhuangqi (State Kce Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1996-03-06; in revised form 1996-06-05). MICROSTRUCTURAL MOSSBAUER SPECTRUM ANALYSIS OF RAPIDLY SOLIDIFIED Al-Fe-V-Si ALLOYS[J]. 金属学报, 1997, 33(4): 359-363.
[12] ZHAO Faru; WANG Baoyi (Lanzhou University; Lanzhou 730000); TONG Zhichen (Shanghai Mechanical Engineering Collnge; Shanghai 200040); WANG Tianmin (Lanzhou University; Lanzhou 730000;Lanzhou Institute of Chemistry-Physics;Chinese Academy of Sciences; Lanzhou 730000)(Manuscript received 1996-05-10; in revised form 1996-1 1-27). HYDROGEN INDUCED-IN DEFECT AND RECOVERY BEHAVIOUR IN POLYCRYSTALLINE NICKEL[J]. 金属学报, 1997, 33(4): 345-351.
[13] XIONG Liangyue1;2); CHEN Jian1); HU Zhuangqi1)(Institute of Metal Research; Chinese Acdemy of Sciences; Shenyang 110015)(International Center for Materials Physics; Chinese Academy of Sciences;Shenyang 110015). POSITRON LIFETIME SPECTRA OF DUCTILE NiAl-Fe INTERMETALLIC ALLOYS[J]. 金属学报, 1996, 32(11): 1189-1193.
[14] CHEN Longqing;SHEN Ningfu(Zhengzhou Institute of Technology; Zhengzhou;450002); SUN Guoxiong (Southeast University; Nanjing 210018)(Manuscript received 1994-10-25). FORMATION CONDITIONS OF MASSIVE PHASE IN RAPIDLY SOLIDIFIED Al-Fe-V-Si ALLOY[J]. 金属学报, 1995, 31(19): 295-299.
[15] GU Yuefong; DENG Wen; GUO Jianting; (Institute of Meial Research; Chinese A cademy of Sciences; Shenyang 110015)XIONG Liangyue; LIN Dongliang (Institute of Metal Research; Chinese A cademy Sciences. Shenyang 110015)(Shanghai Jiaoiong University; Shanghai 200030). PAT STUDY OF EFFECT OF Zr ON DEFECTS IN Ni_3Al ALLOY[J]. 金属学报, 1995, 31(17): 238-240.
No Suggested Reading articles found!