Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (10): 1089-1094    DOI:
Current Issue | Archive | Adv Search |
THE OXIDATION OF Fe-2Ce and Fe-5Ce BINARY ALLOYS AT 600-800℃ IN AIR
ZENG Chaoliu; WANC Wen; F. C. Rizzo; WU Weitao(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals;The Chinese Academy of Sciences; Shenyang 110015)(Pontificia Universidade Catolica do Rio de Janeiro; Rio de Janeiro 38008; Brazil)Correspondent: ZENG Chaoliu; associate professor; Tel: (024)23915910; Fax: (024)23894149;E-mail: clzeng@icpm.syb.ac.cn
Cite this article: 

ZENG Chaoliu; WANC Wen; F. C. Rizzo; WU Weitao(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals;The Chinese Academy of Sciences; Shenyang 110015)(Pontificia Universidade Catolica do Rio de Janeiro; Rio de Janeiro 38008; Brazil)Correspondent: ZENG Chaoliu; associate professor; Tel: (024)23915910; Fax: (024)23894149;E-mail: clzeng@icpm.syb.ac.cn. THE OXIDATION OF Fe-2Ce and Fe-5Ce BINARY ALLOYS AT 600-800℃ IN AIR. Acta Metall Sin, 1998, 34(10): 1089-1094.

Download:  PDF(2006KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The okidation of pure Fe and Fe-Ce alloys containing 2 and 5 Ce (atomicfraction,%) has been studied at 600-800℃ in air. The okidstion curves of pure Fe at 600, 700and 800 ℃ follow the parabolic rate law. The oxidation curve of the Fe-5Ce at 800 ℃ followsthe approximately parabolic rate law, but includes two distinct parabolic stages at 600 and 700℃. The Fe-2Ce goes through an appropriately parabolic oxidstion at the three temperatures.The Fe-2Ce and Fe-5Ce alloys are oxidized slower than pure Fe at 700 and 800 ℃ except inthe initial oxidation stage of the Fe-5Ce at 700℃, while go through a faster oxidation thanpure Fe at 600 ℃. Besides three Fe chides, double chide CeFeO3 also forms in the inner part ofthe scale. Nevertheless, only Fe oxides and CeO2 form in the case of the oxidation at 600 ℃Moreover, FeO only accounts for a small part of the total Fe oxides. Additionally, the effect ofCe in the oxidation of the Fe-Ce alloys has been discussed.
Key words:  Fe      Ce      oxidation     
Received:  18 October 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I10/1089

1 Wood G C, Stott F H. In: Aspp R A ed., High Teoprature Corrostion, Houston, TX: NACE, 1983
2 Whittle D P, Stringer J. Philos Trans R Soc London, 1980; 295A: 309
3 Nagai H, Ishikaw S, Amano N, Shoji K. Trans J Inst Met, 1985; 26: 753
4 Rhys-Hones T N, Grabke H J, Kudielka H. Wich Korro, 1987; 38: 65
5 Papaiacovou P Hussey R J, Mitchell D F, Graham M J. Corms Sci,1990; 4/5: 451
6 Niu Y, Gesmundo F, Wu W T, Zeng C L, Viani F. Acta Metall Sin (Engl Lett), 1996; 9:1
7 Niu Y, Gesmundo F, Zeng C L, Wu W T, Viani F. Oxid Met, 1997; 48: 243
8 Niu Y, Gesmundo F, Cedello P, Yan R Y, Viani F, Wu W T. Corros Sci, 1997; 39: 1093
9 Castello P, Fu G Y, Niu Y, Gesmundo F, Viani F. Oxid Met, 1998; 49: 71
10 Gesmundo F, Niu Y, Viani F. Orid Met, 1995; 43: 379
11 Gesmundo F, Viani F, Niu Y. Oxid Met, 1994; 42: 409
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[4] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[5] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[6] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[7] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[8] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[9] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[10] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[11] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[12] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[13] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[14] ZHANG Bin, TIAN Da, SONG Zhuman, ZHANG Guangping. Research Progress in Dwell Fatigue Service Reliability of Titanium Alloys for Pressure Shell of Deep-Sea Submersible[J]. 金属学报, 2023, 59(6): 713-726.
[15] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
No Suggested Reading articles found!