EFFECTS OF HEAT TREATMENT ON POSITRON ANNIHILATION OF GLASSY BPSCCO
ZHANG Hong Shanghai Institute of Metallurgy; Academia Sinica
Cite this article: 

ZHANG Hong Shanghai Institute of Metallurgy; Academia Sinica. EFFECTS OF HEAT TREATMENT ON POSITRON ANNIHILATION OF GLASSY BPSCCO. Acta Metall Sin, 1992, 28(2): 77-81.

Download:  PDF(471KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effects of isochronal annealing on the positron annihilation of glassy Bi_(1.6)Pb_(0.4)Sr_(1.9)Ca_2Cu_(3.1)O_y(BPSCCO) have been reported. It is shown that the crystallization in- fluences obviously the positron annihilation characteristics of BPSCCO. A maximum is found inthe region of crystallization temperature in curves of mean lifetime and peak / wing ratio, one of Doppler lineshape parameter, with annealing temperature; the bulk lifetime of positron annihi-lation in the glassy state is longer than that in the crystalline one. Positron annihilation spectroscopy could be used for studying structure of glassy BPSCCO and its change with heattreatment.
Key words:  Bi oxide superconductor      positron annihilation      glassy state      crystallization     
Received:  18 February 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I2/77

1 Komatsu T, Sato R, Hirose C, Matusita K, Yamashita T. Jpn J Appl Phys, 1988; 27: L2293
2 Ibara Y, Nasu H, Imara T, Osaka Y. Jpn J Appl Phys, 1989; 28: L37
3 Sato R, Komatsu T, Matusita K, Yamashita T. Jpn J Appl Phys, 1989; 28: L583
4 Abe Y, Hosono H, Hosoe M, Iwase J, Kubo Y. Appl Phys Lett, 1988; 53: 1341
5 LeBeau S E, Righi J, Ostenso J E, Sanders S C, Finnemore D K. Appl Phys lett, 1988; 55: 292

6 Kirkengaard P, Edlrup M. Comput Phys Commun, 1972: 3: 240
7 Paul A, Sigru R M, Dauwe C, Dorikens-Vanpraet L, Dorikens M. J Phys C: Solid State Phys, 1974; 7: 2180
8 Singh Y P, West R N, Paul A. J Phys C: Solid State Phys, 1976; 9: 305
9 Yavari A R, Lejay P. J Cryst Growth, 1988; 91: 290
10 Usmar S G, Rawson H, West R N. In: Coleman P G, Sharma S C, Diana L M eds., Positron Annihilation, Proc 6th Int Conf, The University of Texas at Arlington, April 3--7, 1982, Amsterdam: North-Holland, 1983: 660
11 Shiotani N. In: Coleman P G, Sharma S C, Diana L M eds., Positron Annihilation, Proc 6th Int Conf, The University of Texas at Arlington, April 3--7, 1982, Amsterdam: North-Holland, 1983: 561
12 Morse P, Corbel C. In: Brandt W, Dupasquier A eds., Positron Solid-State Physics, Amsterdam: North-Holland, 1983: 679
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[3] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[4] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[5] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[6] GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong. Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy[J]. 金属学报, 2022, 58(6): 799-806.
[7] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[8] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[9] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[10] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[11] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[12] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[13] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[14] JIANG Jufu, ZHANG Yihao, LIU Yingze, WANG Ying, XIAO Guanfei, ZHANG Ying. Research on AlSi7Mg Alloy Semi-Solid Billet Fabricated by RAP[J]. 金属学报, 2021, 57(6): 703-716.
[15] LI Yanmo, GUO Xiaohui, CHEN Bin, LI Peiyue, GUO Qianying, DING Ran, YU Liming, SU Yu, LI Wenya. Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel[J]. 金属学报, 2021, 57(3): 363-374.
No Suggested Reading articles found!