Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel
AN Xudong1,2, ZHU Te1, WANG Qianqian1,2, SONG Yamin1, LIU Jinyang1, ZHANG Peng1, ZHANG Zhaokuan1, WAN Mingpan2(), CAO Xingzhong1()
1.Institute of High Energy Physics, Chinese Academy of Sciences, Beijing 100049, China 2.College of Materials and Metallurgy, Guizhou University, Guiyang 550025, China
Cite this article:
AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel. Acta Metall Sin, 2021, 57(7): 913-920.
The formation of hydrogen-induced defects in 316 stainless steel and the interaction between hydrogen and defects are crucial aspects to understand the failure law of the hydrogen-induced mechanical properties. Introducing various types of hydrogen sinks, such as interfaces and dislocations, is a popular method for reducing the concentration of residual hydrogen and curbing the mobility of hydrogen atoms in materials. In this work, positron annihilation spectroscopy and thermal desorption spectroscopy (TDS) were used to measure the distribution of hydrogen-induced defects and hydrogen content in deformed 316 stainless steel with hydrogen charging. In particular, the influence of dislocations on the formation of hydrogen-induced defects and the hydrogen retention behavior in the specimens were experimentally investigated. The results show that the S-parameter increases upon hydrogen charging, and the W-parameter is negatively correlated with the S-parameter. The S-parameter value of the deformed sample was found to be larger than that of the annealed sample, indicating that the introduction of hydrogen results in the formation of vacancy defects in the sample. Additionally, hydrogen atoms may gather together to form a large number of volume defects near dislocations. The S-W curves show that the (S, W) point for the sample containing dislocations aggregates towards the surface after hydrogen charging, due to the hindered dislocation motion. In the deformed samples with low hydrogen charge current density, the vacancy formation rate was found to be slow, and the combination of excess hydrogen and vacancies was observed to give rise to hydrogen-vacancy clusters (HmVn), where n > m. The TDS results show that both the activation energy for hydrogen desorption and the amount of hydrogen retention increase due to the presence of dislocations.
Fund: National Key Research and Development Program of China(2019YFA0210002);Natural Science Foundation of China(11775235、U1732265)
About author: WAN Mingpan, associate professor, Tel: 18984135926, E-mail: mpwan@gzu.edu.cn. CAO Xingzhong, professor, Tel: (010)88233393, E-mail: caoxzh@ihep.ac.cn.
Table 1 Annealing conditions and electrochemical hydrogen charging parameters of austenitic 316 stainless steel
Fig.1 S-E (a) and ΔS-E (b) curves of 316 stainless steel samples after hydrogen charging under different annealing conditions and hydrogen charging conditions of electrochemical cathode (S—the positron and free electron annihilation information, E—the positron incident energy, ΔS—the increment of S, ΔS2—the difference of S parameters between No.1 and No.2, ΔS4—the difference of S parameters between No.3 and No.4)
Fig.2 S-W curves of hydrogen charging of austenitic 316 stainless steel at different annealing conditions (W—the annihilation information between positrons and high-momentum electrons)
Fig.3 S-E (a) and ΔS-E (b) curves of austenitic 316 stainless steel under different hydrogen charging conditions after annealing at 500oC for 1 h (ΔS5— the difference of S parameters between No.3 and No.5, ΔS6—the difference of S parameters between No.3 and No.6)
Fig.4 W-E (a) and ΔW-E (b) curves of austenitic 316 stainless steel under different hydrogen charging conditions after annealing at 500oC for 1 h (ΔW—the increment of W, ΔW4—the difference of W parameters between No.3 and No.4, ΔW5—the difference of W parameters between No.3 and No.5, ΔW6—the difference of W parameters between No.3 and No.6)
Fig.5 XRD spectra of austenitic 316 stainless steel under different hydrogen charging conditions after annealing at 500oC for 1 h
Fig.6 S-W curves of austenite 316 stainless steel under different hydrogen charging conditions after annealing at 500oC for 1 h
Machida A, Saitoh H, Hattori T, et al. Hexagonal close-packed iron hydride behind the conventional phase diagram [J]. Sci. Rep., 2019, 9: 12290
2
Nagumo M, Nakamura M, Takai K. Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels [J]. Metall. Mater. Trans., 2001, 32A: 339
3
Song J, Curtin W A. Atomic mechanism and prediction of hydrogen embrittlement in iron [J]. Nat. Mater., 2013, 12: 145
4
Momida H, Asari Y, Nakamura Y, et al. Hydrogen-enhanced vacancy embrittlement of grain boundaries in iron [J]. Phys. Rev., 2013, 88B: 144107
5
Weber S, Martin M, Theisen W. Impact of heat treatment on the mechanical properties of AISI 304L austenitic stainless steel in high-pressure hydrogen gas [J]. J. Mater. Sci., 2012, 47: 6095
6
Ioka I, Ishijima Y, Usami K, et al. Radiation hardening and IASCC susceptibility of extra high purity austenitic stainless steel [J]. J. Nucl. Mater., 2011, 417: 887
7
Katsura R, Morisawa J, Kawano S, et al. Post-irradiation annealing effect on helium diffusivity in austenitic stainless steels [J]. J. Nucl. Mater., 2004, 329-333: 668
8
Marchi C S, Michler T, Nibur K A, et al. On the physical differences between tensile testing of type 304 and 316 austenitic stainless steels with internal hydrogen and in external hydrogen [J]. Int. J. Hydrogen Energy, 2010, 35: 9736
9
Elhoud A M, Renton N C, Deans W F. Hydrogen embrittlement of super duplex stainless steel in acid solution [J]. Int. J. Hydrogen Energy, 2010, 35: 6455
10
Liu Z B, Liang J X, Su J, et al. Research and application progress in ultra-high strength stainless steel [J]. Acta Metall. Sin., 2020, 56: 549
Jin S X, Cao X Z, Cheng G D, et al. Thermally promoted evolution of open-volume defects and Cu precipitates in the deformed FeCu alloys [J]. J. Nucl. Mater., 2018, 501: 293
12
Ohkubo H, Sugiyama S, Fukuzato K, et al. Positron-lifetime study of electrically hydrogen charged Ni, austenitic stainless steel and Fe [J]. J. Nucl. Mater., 2000, 283-287: 858
13
Canter K F, Mills Jr A P, Berko S. Efficient positronium formation by slow positrons incident on solid targets [J]. Phys. Rev. Lett., 1974, 33: 7
14
Nagai Y, Takadate K, Tang Z, et al. Positron annihilation study of vacancy-solute complex evolution in Fe-based alloys [J]. Phys. Rev., 2003, 67B: 224202
15
Zhang T C, Wang H T, Li Z C, et al. Positron annihilation investigation of embrittlement behavior in Chinese RPV steels after Fe-ion irradiation [J]. Acta Metall. Sin., 2018, 54: 512
Eldrup M, Singh B N. Study of defect annealing behaviour in neutron irradiated Cu and Fe using positron annihilation and electrical conductivity [J]. J. Nucl. Mater., 2000, 276: 269
18
Deng W, Ruan X D, Huang Y Y, et al. Effects of twin size on the dislocation configuration during cyclic deformation of polycrystalline twin copper [J]. Acta Metall. Sin., 2005, 41: 33
Chen Y Q, Wu Y C, Wang Z, et al. Positron annihilation study on interaction between hydrogen and defects in AISI 304 stainless steel [J]. Radiat. Phys. Chem., 2007, 76: 308
20
Würschum R, Farber P, Dittmar R, et al. Thermal vacancy formation and self-diffusion in intermetallic Fe3Si nanocrystallites of nanocomposite alloys [J]. Phys. Rev. Lett., 1997, 79: 4918
21
Wu Y C, Jean Y C. Hydrogen-induced defects of AISI 316 stainless steel studied by variable energy Doppler broadening energy spectra [J]. Phys. Status Solidi, 2004, 201A: 917
22
Zhu T, Jin S X, Gong Y H, et al. The influence of dislocation and hydrogen on thermal helium desorption behavior in Fe9Cr alloys [J]. J. Nucl. Mater., 2017, 495: 244
23
Zhu T, Cao X Z, Jin S X, et al. Helium retention and thermal desorption from defects in Fe9Cr binary alloys [J]. J. Nucl. Mater., 2015, 466: 522
24
Cao X Z, Xu Q, Sato K, et al. Thermal desorption of helium from defects in nickel [J]. J. Nucl. Mater., 2011, 412: 165
25
Munakata K, Shinozaki T, Inoue K, et al. Tritium release from lithium silicate pebbles produced from lithium hydroxide [J]. Fusion Eng. Des., 2008, 83: 1317
26
Gilbert E R, Garner F A. The influence of cold-work level on the irradiation creep and swelling of AISI 316 stainless steel irradiated as pressurized tubes in the EBR-II fast reactor [J]. J. Nucl. Mater., 2006, 367-370: 954
27
Zhang C X, Cao X Z, Li Y H, et al. Thermal evolution of vacancy-type defects in quenched FeCrNi alloys [J]. Appl. Phys., 2015, 119A: 1431
28
Gong Y H, Jin S X, Zhu T, et al. Helium self-trapping and diffusion behaviors in deformed 316L stainless steel exposed to high flux and low energy helium plasma [J]. Nucl. Fusion, 2018, 58: 046011
29
Koch T, Heinig K H, Jentschel M, et al. Study of interatomic potentials in ZnS—Crystal-GRID experiments versus ab initio calculations [J]. J. Res. Natl. Inst. Stand. Technol., 2000, 105: 81
30
Jin S X, Zhang P, Lu E Y, et al. Correlation between Cu precipitates and irradiation defects in Fe-Cu model alloys investigated by positron annihilation spectroscopy [J]. Acta Mater., 2016, 103: 658
31
Cao X Z, Song L G, Jin S X, et al. Advances in applications of positron annihilation spectroscopy to investigating semiconductor microstructures [J]. Acta Phys. Sin., 2017, 66: 027801
32
Hu Y C, Cao X Z, Li Y X, et al. Applications and progress of slow positron beam technique in the study of metal/alloy microdefects [J]. Acta Phy. Sin., 2015, 64: 247804
Zhu T, Jin S X, Guo L P, et al. Helium/hydrogen synergistic effect in reduced activation ferritic/martensitic steel investigated by slow positron beam [J]. Philos. Mag., 2016, 96: 253
34
Cao X Z, Zhang P, Xu Q, et al. Cu precipitates in Fe ion irradiated Fe-Cu alloys studied using positron techniques [J]. J. Phys.: Conf. Ser., 2013, 443: 012017
35
Xin Y, Ju X, Qiu J, et al. Vacancy-type defects and hardness of helium implanted CLAM steel studied by positron-annihilation spectroscopy and nano-indentation technique[J]. Fusion Eng. Des., 2012, 87: 432
36
Jena P, Ponnambalam M J, Manninen M. Positron annihilation in metal-vacancy-hydrogen complexes [J]. Phys. Rev., 1981, 24B: 2884
37
Zhang S S, Cizek J, Yao Z J, et al. Self healing of radiation-induced damage in Fe-Au and Fe-Cu alloys: Combining positron annihilation spectroscopy with TEM and ab initio calculations [J]. J. Alloys Compd., 2020, 817: 152765
38
Duportal M, Oudriss A, Feaugas X, et al. On the estimation of the diffusion coefficient and distribution of hydrogen in stainless steel [J]. Scr. Mater., 2020, 186: 282
39
Ishizaki T, Xu Q, Yoshiie T, et al. The Recovery of gas-vacancy-complexes in Fe irradiated with high energy H or He ions [J]. Mater. Trans., 2004, 45: 9
40
Cao X Z, Zhu T, Jin S X, et al. Detection of helium in irradiated Fe9Cr alloys by coincidence Doppler broadening of slow positron annihilation [J]. Appl. Phys., 2017, 123A: 177
41
Wang K, Deng A H, Gong M, et al. Effect on microstructure of tungsten under helium ions irradiation with multiple energy [J]. Acta Metall. Sin., 2017, 53: 70
Sato K, Ikemura K, Krsjak V, et al. Defect structures of F82H irradiated at SINQ using positron annihilation spectroscopy [J]. J. Nucl. Mater., 2016: 468: 281