| MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS ALLOYS Co_(90-x)Cr_xZr_(10) |
| HU Fengxia;CHEN Jinchang;SHEN Baogen;GUO Huiqun Institute of Physics; Academia Sinica; Beijing; Beijing Teacher's College; Institute of Physics; Academia Sinica; Beijing |
|
Cite this article:
HU Fengxia;CHEN Jinchang;SHEN Baogen;GUO Huiqun Institute of Physics; Academia Sinica; Beijing; Beijing Teacher's College; Institute of Physics; Academia Sinica; Beijing. MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS ALLOYS Co_(90-x)Cr_xZr_(10). Acta Metall Sin, 1992, 28(2): 71-76.
|
|
|
Abstract Curie temperature of amorphous alloys Co_(90-x)Cr_xZr_(10)decreases linearly with increasing x. Average magnetic moment per magnetic atom Co or Cr is 1.51 μB or --3.62 μB respectively. The temperature dependence of spontaneous magnetization at low temperatureis in agreement with Bloch's T~(3/2) law. The spin wave stiffness constant decreases with increasing x from 4 to 20. The range of interaction is 2--3 atoms for x=4 and neighbourest atom for x=20. The crystallization temperature increases monotonically with increasing x. It may be related toaverage number of outer electrons per atom. The crystalline phase components of heat-treated alloys were analyzed by X--ray diffration and thermomagnetic measurement.
|
|
Received: 18 February 1992
|
1 Mizoquchi T, Yamauchi K, Miyajima H. In: Hooper H O, De Graaf A M eds., Amorphous Magnetism, 1973: 325 2 詹文山,沈保根,赵见高.物理学报,1985;34:1613 3 Vind Nielsen H J. J Magn Magn Mater, 1979; 12: 187 4 Hiroyoshi H, Fukamichi K. Phys Lett, 1981; 85A: 242 5 Shen B G, Xu R F, Zhao J G, Zhao J G, Zhan W S. Phys Rev, 1991; B43: 11005 6 沈保根,詹文山,赵见高,陈金昌.物理学报,1988;37:804 7 Wong J. In: Guntherodt H J, Beck H eds., Glassy Metals I, Berlin: Springer-Verlag, 1981: 71 8 詹文山,沈保根,赵见高.物理学报,1985;34:1613 9 沈保根,沃峰,杨林原,赵见高,郭慧群,詹文山,陈金昌.物理学报,1990;39:1488 10 Altounian Z, Batalla E, Stom-Olsen J O. J Appl Phys, 1986: 59: 2364} |