BRITTLE-DUCTILE TRANSITION OF ANNEAL-EMBRITTLED Fe_(75)Si_(10)B_(15) METALLIC GLASS
WANG Longbao State Key Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang;
Cite this article:
WANG Longbao State Key Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang;. BRITTLE-DUCTILE TRANSITION OF ANNEAL-EMBRITTLED Fe_(75)Si_(10)B_(15) METALLIC GLASS. Acta Metall Sin, 1992, 28(2): 64-70.
Abstract Studies were made of the effect of mechanical pulverization on relaxation,crystallization and brittle--ductile transition of the anneal--embrittled Fe_(75)Si_(10)B_(15) metallic glass ribbon. Results show that the Curie temperature, T_c, decreases and the total enthalpy of relaxa-tion increases gradually with variation of pulverized time. DSC traces reveal an extra exothermicpeak, T_(x_1), and a distinct glass transition endothermic peak, T_(g_1), with increasing pulverizedtime, T_c, T_(x_1), and T_(g_1) decrease simultaneously, and the exothermic peak area correspondingto T_(x_1) increases gradually. The surface slip--steps of flaky particles and their corresponding shear are produced by pulverizing the pre--embrittled amorphous glass. The lost ductility of theglass may restore during annealing.
1 Gerling R, Schimansky F P, Wagner R. Acta Metall, 1987; 35: 1001. 2 Davies H A, Small C J. J Less-Common Met, 1988; 140: 185 3 Chen H S, Inoue A, Masumoto T. J Mater Sci, 1985; 20: 2417 4 Donovan P E, Stobbs W M. Acta Metall, 1981; 29: 1419 5 Li J C M. In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals 4, Vol. Ⅱ, Proc 4th Int Conf Rapidly Quenched Metals, Sendai, Augest 24--28, 1981, The Japan Inst Metals, 1982: 1335 6 Eckert J, Schultz L, Hellstern E, Urban K. J Appl Phys, 1988; 64: 3224 7 Trudeau M L, Schulz R. Phys Rev lett, 1990; 64: 99 8 Steif P S, Spaepen F, Hutchinson J W. Acta Metall, 1982; 30: 44