| DAMPING PROPERTIES OF MARTENSITE AND MARTENSITIC TRANSFORMATION IN CuZnAl ALLOYS |
| CHENG Yixuan;CHEN Jiqin;FANG Xiaomin;Lu Weiping Zhejiang University; Hangzhou |
|
Cite this article:
CHENG Yixuan;CHEN Jiqin;FANG Xiaomin;Lu Weiping Zhejiang University; Hangzhou. DAMPING PROPERTIES OF MARTENSITE AND MARTENSITIC TRANSFORMATION IN CuZnAl ALLOYS. Acta Metall Sin, 1991, 27(3): 56-60.
|
|
|
Abstract The internal friction as martensite state is believed to be an M/Minterface one, which can be explained as an expression deduced from the theory ofdislocation internal friction. The internal friction in the region of martensitic trans-formation consists of two parts, including ones of the M/M interface and of thephase transformation. The later is further composed of two portions, the majorproduced by reverse martensitic transformation and the other from stress-inducedmartensite. It was also found that the degradation of dampling properties of theCuZnAl alloys is related to the dislocation, which is introduced from the excitingprocess, and tends to a stable value after certain excitements.
|
|
Received: 18 March 1991
|
1 Delaey L, Aernodt E. Proc ICOMAT 86, Nara, Japan, 1986, Japan Inst Metals, 1987: 926 2 Granato A, Luecke K. J Appl Phys, 1956, 27: 583 3 魏大可,陈继勤,程饴萱.机械工程材料,1989;13(3) :30 4 Dejonghe W, De Batist R, Delaey L. Scr Metall, 1976; 10: 1125 5 胡丽丽,程饴萱,陈继勤.浙江大学学报,1989;23(1) :105 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|