EFFECT OF COMPOSITION AND THERMAL TREATMENT ON PHASE CONSTITUENT AND ORDER STATE OF CuAlNi ALLOYS
GUI Jianian;REN Qiang;WANG Renhui Wuhan University
Cite this article: 

GUI Jianian;REN Qiang;WANG Renhui Wuhan University. EFFECT OF COMPOSITION AND THERMAL TREATMENT ON PHASE CONSTITUENT AND ORDER STATE OF CuAlNi ALLOYS. Acta Metall Sin, 1991, 27(3): 61-66.

Download:  PDF(2616KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of the composition and thermal treatment on the phaseconstituent, the size of B2- and DO_3 derived domains and martensitic thermoelasticbehaviour in three CuAlNi alloys has been studied by means of metallography,TEM and X-ray diffraction analysis. It is shown that the martensite type changesfrom 18R_1 to 2H structure and the transition temperature decreases with the increaseof the Al content. Moreover, the size of the B2- and DO_3, derived domainsdecreases with the increase of the cooling rate.
Key words:  CuAlNi alloy      shape memory alloy      martensitic transformation     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/61

1 褚幼义.全国形状记忆合金学术讨论会论文集,北京,1988
2 刘锦文,刘海飞.全国形状记忆合金学术讨论会论文集,北京,1988
3 Wang Renhui Zhao Yuechao. Gui Jianian. J Electron Microsc Tech. 1987; 7: 293
4 宫崎修一,大塚和弘.见:舟久保熙康编,形状记忆合金 东京:产业图书株式会社,1984:100
5 Kennon N F. Dunne D P, Middleton L. Metall Trans, 1982; 13A: 551
6 罗常红.武汉大学硕士学位论文.1988
7 Gui Jianian Luo Changhong, Zhang Hege, Hu Wei, Wang Renhui. J Mater Sci. 1990; 25: 1675;
[1] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[2] YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi. Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 55-74.
[3] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[4] ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong. Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy[J]. 金属学报, 2022, 58(8): 1065-1071.
[5] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[6] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[7] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[8] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite[J]. 金属学报, 2021, 57(7): 921-927.
[9] YE Junjie, HE Zhirong, ZHANG Kungang, DU Yuqing. Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy[J]. 金属学报, 2021, 57(6): 717-724.
[10] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[11] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[12] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[13] CHEN Xiang,CHEN Wei,ZHAO Yang,LU Sheng,JIN Xiaoqing,PENG Xianghe. Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. 金属学报, 2020, 56(3): 361-373.
[14] CHEN Lei , HAO Shuo , MEI Ruixue , JIA Wei , LI Wenquan , GUO Baofeng . Intrinsic Increment of Plasticity Induced by TRIP and Its Dependence on the Annealing Temperature in a Lean Duplex Stainless Steel[J]. 金属学报, 2019, 55(11): 1359-1366.
[15] Lishan CUI, Daqiang JIANG. Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching[J]. 金属学报, 2019, 55(1): 45-58.
No Suggested Reading articles found!