Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (3): 51-55    DOI:
Current Issue | Archive | Adv Search |
TRANSFORMATION HYSTERESIS AND STABILITYOF STRAIN MARTENSITE IN Ni_(47)Ti_(44)Nb_9 ALLOY
ZHANG Chunsheng;CAI Wei;ZHAO Liancheng (Harbin Institute of Technology
Cite this article: 

ZHANG Chunsheng;CAI Wei;ZHAO Liancheng (Harbin Institute of Technology. TRANSFORMATION HYSTERESIS AND STABILITYOF STRAIN MARTENSITE IN Ni_(47)Ti_(44)Nb_9 ALLOY. Acta Metall Sin, 1991, 27(3): 51-55.

Download:  PDF(1420KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The transformation hysteresis and stability of strain martensite inNi_(47)Ti_(44)Nb_9 alloy have been studied by means of tensile test under various temper-atures, electrical resistance measurement and TEM observation. It was shown thatthere is a characteristic deformation temperature and a strain range, in which thecritical yield stress for stress-induced transformation acquires optimum matchingwith the yield strength of the β-Nb particles. In this case, deformation effectivelyincreases the transformation hysteresis, while the strain recovery ratio remains use-fully high. The martensite with irregular fine twin substructure and martensitecontaining some dislocations as well as martensite intersected by the β-Nb particlespossess high stability.
Key words:  NiTiNb shape memory alloy      transformation hysteresis      strain martensite     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/51

1 Zhao L C, Duerig T W. Wayman C M. Proc of the MRS Int Meeting on Advanced Materials, Vol. 9, 1988: 171
2 Zhao L C, Duerig T W, Just S, Melton K N, Proft J L, Yu W, Wayman C M. Scr Metall, 1990; 24: 221
3 Zhang C S, Zhao L C, Duerig T W, Wayman C M. Scr Metall, 1990; 24: 1807
4 Warlimont H et al. J Mater Sci, 1974; 9: 1545
5 Mohamed H A, Washburn J. Metall Trans, 1976; 7A: 1041
[1] XIAO Fu ZHAO Xinqing XU Huibin JIANG Haichang RONG Lijian. DAMPING CAPACITY AND MECHANICAL PROPERTY OF
NiTiNb SHAPE MEMORY ALLOYS
[J]. 金属学报, 2009, 45(1): 18-24.
No Suggested Reading articles found!