| EFFECT OF ALLOYING ELEMENT ON MECHANICAL PROPERTIES OF Fe_3AL AND FeAl ALLOYS |
| GUO Jianting;SUN Chao;TAN Minghui;LI Hui;LAI Wanhui Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Research;Academia Sinica; Shenyang 110015 |
|
Cite this article:
GUO Jianting;SUN Chao;TAN Minghui;LI Hui;LAI Wanhui Institute of Metal Research; Academia Sinica; Shenyang professor;Institute of Metal Research;Academia Sinica; Shenyang 110015. EFFECT OF ALLOYING ELEMENT ON MECHANICAL PROPERTIES OF Fe_3AL AND FeAl ALLOYS. Acta Metall Sin, 1990, 26(1): 20-25.
|
|
|
Abstract The effect of alloying elements such as Mo, Si or B and its stoichoi-metric composition on the tensile properties at room and elevated temperatures, andalso on the microstructure has been investigated. Two Fe aluminides were found tobe obviously strengthened by all of three elements, but seriously embrittled by Moand Si. An improvement over the plasicity of FeAl may be made by adding B. Thefracture surface is varied from intergranular to transgranular cleavage type. Theroom temperature plasticity of the Fe-rich Fe_3Al or Al-rich FeAl is much betterthan that of the stoichoimetric aluminides. An anomalous temperature dependenceon the yield strength of Fe_3Al in range of 400 to 550℃ or of FeAl in 400 to500℃ was found. Discussion has been carried out by the aspect of microstrutures.
|
|
Received: 18 January 1990
|
1 McKamey C G, Horton J A, Liu C T. In: Stoloff N S, Kccb C C, Liu C T, Izumi O eds., HighTemperature Ordered Intermctallic Alloys Ⅱ, Pittsburgh, Pennsylvania: Materials Research Society, 1987: 321--327 2 Marcinkowski M J, Taylor M E, Kayser F X. J Mater Sci, 1975; 10: 406--419 3 Mendiratta M G, Ehlers S K, Dimiduk D M, Kerr W B, Mazdiyasni S, Lipsitt H A. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys Ⅱ, Pittsburgh, Pennsylvania: Materials Research Society, 1987: 393--404 4 Mendiratta M G, Lipsitt H A. In: Koch C C, Liu C T, Stoloff N S eds., High-Temperature Ordered Intermetallic Alloys, Pittsburgh, Pennsylvania: Materials Reseaich Sceiely, 1985: 155--162 5 Vedula K, Stephens J R. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys Ⅱ, Pittsburgh, Pennsylvania: Materials Research Society, 1987: 281--391 6 李辉,刘祥,郭建亭,胡壮麒.金属学报,1979;25:A25--30 7 郭建亭,李辉,孙超,谭明晖,朱耀宵.机械工程学报,待发表 8 郭建亭,李辉,孙超,朱耀宵.金属学报,1989;25:A406--413 9 Inouye H. In: Koch C C, Liu C T, Stoloff N S eds., High-Temperature Ordered Intermetallic Alloys, Ⅱ Pittsburgh, Pennsylvania: Materials Research Society, 1985: 255--261 10 Stoloff N S, Davies R G. Acta Metall, 1964; 12: 473--476 |
| No Suggested Reading articles found! |
|
|