ON THE DEGRADATION OF DUCTILITY INDUCED BY HYDROGEN IN MEDIUM CARBON STEELS
DU Jiaju;TONG Shihua Institute of Solid State Physics; Academia Sinica; Hefei
Cite this article: 

DU Jiaju;TONG Shihua Institute of Solid State Physics; Academia Sinica; Hefei. ON THE DEGRADATION OF DUCTILITY INDUCED BY HYDROGEN IN MEDIUM CARBON STEELS. Acta Metall Sin, 1989, 25(3): 70-72.

Download:  PDF(1290KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Optical microscope, SEM and IMMA investigation show that a strong interactionbetween hydrogen and calcium aluminate inclusions cotaining Mg may occur in medium carbonsteels. That causes the hydrogen accumulating around the inclusions and reducing the ductilityof the steel.
Key words:  hydrogen      inclusions      steel     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/70

1 李代钟,钢中的非金属夹杂物.北京,科学出版社.1983:45
2 Podgurski H H, Oriani R A. Metall Trans, 1972; 3: 2055
3 Pressouyre G M, Bernstein I M. Acta Metall, 1979; 27: 89
4 French I E, Weinrich P F, Weaver C W. Scr Matall, 1979; 13: 285
5 Ciszewski A, Radowski T, Smialowski M. In: Staehl R W, Hochmann J, Mccright R D. Slater J E eds., Stress Corrosion Cracking and Hydrigen Embrittlement of Iron Base Alloys, NACE-5, Houston: NACE, 1977: 671
6 Thompson A W, Bernstein I M. Adv Corros Sci Technol, 1979; 7: 53
7 Du Jiaju (杜家驹), Mao Ou (毛欧), Wang Xiang (王翔). In: Yan M G, Zhang S H, Zheng Z M eds., Mechanical Behaviour of Materials-V, Vol. Ⅱ, New York: Pergamon, 1987: 855q
[1] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[2] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[3] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[4] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[5] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[6] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[7] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[8] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[9] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[10] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[11] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[12] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[13] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[14] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[15] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
No Suggested Reading articles found!