EFFECT OF TRACE B AND Ga ON TRANSFORMATION CONTROL OF Mn-Si-Cr AS-ROLLED DUAL PHASE STEELS |
HE Zefu;LIU Tianmo;WU Yunjian Chongqing University |
|
Cite this article:
HE Zefu;LIU Tianmo;WU Yunjian Chongqing University. EFFECT OF TRACE B AND Ga ON TRANSFORMATION CONTROL OF Mn-Si-Cr AS-ROLLED DUAL PHASE STEELS. Acta Metall Sin, 1989, 25(3): 73-75.
|
Abstract Trace of B and Ga can substitute for Mo in Mn-Si-Cr dual phase steels. Thetechnological properties and CCT curves of steels treated with B and Ga are similar to those forMn-Si-Cr-Mo steel.
|
Received: 18 March 1989
|
1 花井谕,渡辺国男,江坂一彬.铁钢,1982;68:1306 2 Barr R Q. Alloys for the Eighties, Connecticut: Climax Molybdenum Company, 1978: 37 3 马鸣图,吴宝榕.国外金属材料,1982;(10) : 9 4 何泽福,夏进,钱小蓉.重庆大学学报,1985;(1) : 83 5 Coldren A P, Eldis G T. J Met, 1980; 32(3) : 41 6 刘富国,黄文轩,何泽福.钢铁钒钛,1982;(3) :1 7 Kubaschewki O. Iron-Binary Phase Diagrams, Berlin: Springer-Verlag, 1982: 38 |