| EFFECT OF MICROSTRUCTURES OF HIGH STRENGTH STEEL ON SUSCEPTIBILITY OF CADMIUM EMBRITTLEMENT |
| TANG Zhizhong;LIU Minzhi;XIAo Yaotian Chengdu University of Science and Technology Institute of Metal Research Academia Sinica; Shenyang |
|
Cite this article:
TANG Zhizhong;LIU Minzhi;XIAo Yaotian Chengdu University of Science and Technology Institute of Metal Research Academia Sinica; Shenyang. EFFECT OF MICROSTRUCTURES OF HIGH STRENGTH STEEL ON SUSCEPTIBILITY OF CADMIUM EMBRITTLEMENT. Acta Metall Sin, 1989, 25(2): 40-44.
|
|
|
Abstract The effect of different microstructures of steel 30CrMnSiNi2A on thesusceptibility of cadmium embrittlement has been studied and compared under theunique yield strength level. The results show that the tempered martensite exhibitsthe maximum susceptibility to cadmium embrittlement, while the lower bainite showsthe minimum susceptibility. The mixed microstructure of the above two has asusceptibility in between.
|
|
Received: 18 February 1989
|
1 Evans U R,华保定译.金属的腐蚀与氧化,北京:机械工业出版社,1976:342 2 Lynn J C, Warke W R, Gordon Mater Sci Eng. 1975; 18: 51 3 Hildebrand J F. Mater Prot Perform, 1973; 12 (9) : 35 4 Westwood A R C, Preece C M, Kamda M H. In: Leiborwiz H ed., Fracture, Vol. 3, Academic Press, 1971: 589 5 邓日红,彭菊影.航空材料(专刊),1986;1(2) :68 6 伊藤一夫,常陆美朝.电气制钢,1977:48(1) :75F |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|