MICROSTRUCTURE AND MECHANICAL BEHAVIOUR OF Al-Li-Zr AND Al-Li-Cu-Mg-Zr ALLOYS
YIN Zhimin;AUST K. T.;WEATHERLY G. C. Central-South University of Technology; Changsha. Hunan; University of Toronto; Toronto; ONT; Canada
Cite this article: 

YIN Zhimin;AUST K. T.;WEATHERLY G. C. Central-South University of Technology; Changsha. Hunan; University of Toronto; Toronto; ONT; Canada. MICROSTRUCTURE AND MECHANICAL BEHAVIOUR OF Al-Li-Zr AND Al-Li-Cu-Mg-Zr ALLOYS. Acta Metall Sin, 1988, 24(5): 347-353.

Download:  PDF(2130KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The aging response, tensile and impact properties of two kinds of Al-Li based alloys have been studied. The microstructure, deformation as well as frac-ture behaviour have been observed by SEM and TEM. It has been found that themechanism of deformation and fracture for different heat-treated alloys with thesame chemical composition is quite different. The cause led to the drop of ductili-ty, toughness as well as anisotropy in peak-aged alloys have been analysed. Finally,possible methods to improve the ductility and toughness of the alloys have beendiscussed.
Key words:  Al-Li based alloy      microstructure      mechanical properties     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/347

1 Starke E A Jr. Sanders T H Jr., Aluminium-Lithium Alloys, TMS-AIME, 1981:
2 Starke E A Jr. Sanders T H Jr., Aluminium-Lithium Alloys Ⅱ, TMS-AIME, 1984
3 Sanders T H Jr. Proc 3rd Int Al-Li Conf, Oxford. UK, July, 1985, London The Institute of Metals, 1986
4 Guyot P. Proc CBECIMAT, Ⅵ, Rio de Janeiro, Brazil, Puc/R J, 1984; 387
5 Honeycomb R W K. The Plastic Deformation of Metals, Edward Arnoid Reprinted, London, England, 1977: 322
6 Dinsdale K, Harris S J, Nobel B. In: Starke E A Jr. Sanders T H, eds., Aluminum-Lithium Alloys, TMS-AIME, 1981: 101
7 Starke E A Jr., Sanders T H Jr., Palmer I G. J Met, 1981; 33(8) : 24
8 尹志民.铝-锂合金的形变热处理与组织性能.(待发表)D
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!