Revisiting the Development of Eutectic High-Entropy Alloys over the Past Decade (2014-2024): Design, Manufacturing, and Applications
WANG Zhijun1(), BAI Xiaoyu1, WANG Jianbin1, JIANG Hui2, JIAO Wenna3, LI Tianxin4, LU Yiping3,5()
1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China 2 School of Mechanical and Electronic Engineering, Shandong University of Science and Technology, Qingdao 266590, China 3 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China 4 College of Materials and Metallurgy, Guizhou University, Guiyang 550025, China 5 Liaoning Engineering Research Center of High-Entropy Alloy Materials, Dalian University of Technology, Dalian 116024, China
Cite this article:
WANG Zhijun, BAI Xiaoyu, WANG Jianbin, JIANG Hui, JIAO Wenna, LI Tianxin, LU Yiping. Revisiting the Development of Eutectic High-Entropy Alloys over the Past Decade (2014-2024): Design, Manufacturing, and Applications. Acta Metall Sin, 2025, 61(1): 1-11.
Eutectic alloys are a class of multi-phase materials named for their formation through eutectic reactions during solidification. They have a long history as the most widely used casting alloys. High-entropy alloys (HEAs), on the other hand, are a novel class of multi-principal element alloys that have rapidly developed since their conceptualization in 2004. Combining the advantages of eutectic alloys and HEAs, eutectic high-entropy alloys (EHEAs) were first proposed in 2014. Over a decade, EHEAs have been systematically investigated by focusing on alloy design, microstructure/performance optimization, large-scale fabrication, and potential applications. Their unique microstructures and excellent comprehensive properties have made EHEAs promising materials across various domains, garnering significant attention in recent years. By revisiting the advances in composition design, manufacturing, and applications of EHEAs over the past decade, this review offered insights into future trends and developments in this rapidly evolving field.
Corresponding Authors:
WANG Zhijun, professor, Tel: 13484671484, E-mail: zhjwang@nwpu.edu.cn; LU Yiping, professor, Tel: (0411)84709400, E-mail: luyiping@dlut.edu.cn
Fig.1 Strategies to design eutectic high-entropy alloys (EHEAs) (a) calculated pseudo-binary-phase diagram for FeCoNiCrNb x alloys[22] (b1-b4) microstructures of (CoCrFeNi)Mx EHEAs obtained by the simple mixing method[23] (c) empirical design criteria for EHEAs based on the relationship between valence electron concentration (VEC) and atomic size difference (δr)[25] (d) empirical design criteria for EHEAs based on the relationship between mixed enthalpy of solid solution (ΔH) and VEC of solid solution (VECss) (IMC—intermetallic compound)[26]
Fig.2 Schematic diagram of designing EHEAs with machine learning[27] (xi is the ith input parameter, y is the output parameter. The f1(x) and f2(x) are the internal layer functions in an artificial neural network model)
Fig.3 Typical solidification microstructures of EHEAs (a) ultrafine eutectic microstructure (A and B show the dendritic and inter-dendritic regions, respectively)[34] (b) lamellar microstructure[38] (c) mixed lamellar/irregular microstructure[39]
Fig.4 Microstructures of EHEAs tailored by various processing methods (a) BSE image, EBSD phase, and Inverse pole figures (IPFs) of the directionally solidified Al19Fe20Co20Ni41 EHEA, showing a herringbone-like eutectic microstructure (BEC—branched eutectic colonies, AEC—aligned eutectic colonies)[48] (b) EBSD IPF map of as-printed AlCoCrFeNi2.1 EHEA, showing ultrafine nanolamellar eutectic colonies with different crystallographic orientations (Inset shows the EBSD phase map)[50] (c) EBSD phase map of the anomalous eutectic structure in remelted additive manufactured Ni32Co30Cr10Fe10Al18 EHEA[51] (d) EBSD phase map of equiaxed ultrafine-grained structure in the 90% cold-rolled AlCoCrFeNi2.1 EHEA after isothermal annealing[53] (e) SEM image and EBSD phase map of the AlCoCrFeNi2.1 EHEA cold-rolled by 84%-86% followed by non-isothermally annealing, showing heterogeneous duplex microstructure consisting of lamellar and ultrafine-grained structure[52] (f) IPFs of the phase-selectively recrystallized Ni30Co30Cr10Fe10Al18W2 EHEA, showing the microstructure with a fully recrystallized fcc phase embedded in the skeleton of a B2 phase[54]
Fig.5 Mechanical properties of EHEAs with different microstructures (a) directionally solidified Al19Fe20Co20Ni41 EHEA with herringbone-like microstructure (Inset shows the strain-hardening rate curves. MDIH and MBIH refer to multi-slip dislocation-induced hardening and microband-induced hardening, respectively; εU—uniform strain; σy—yield strength of Al19Fe20Co20Ni41 EHEA; σUTS—ultimate tensile strength of Al19Fe20Co20Ni41 EHEA)[48] (b) as-printed and annealed AlCoCrFeNi2.1 EHEA with ultrafine nanolamellar structure (Inset shows the schematic of a dogbone-shaped specimen under tensile loading. σu—ultimate tensile strength of AlCoCrFeNi2.1 EHEA; σ0.2—yield strength of AlCoCrFeNi2.1 EHEA)[50] (c) additive manufactured Ni32Co30Cr10Fe10Al18 EHEA with anomalous eutectic structure[51] (d) ultrafine-grained AlCoCrFeNi2.1 EHEA (CR—cold rolling)[53] (e) heterogeneous-grained AlCoCrFeNi2.1 EHEA (Inset shows the loading-unloading-reloading behavior of the DPHL700 and the as-cast EHEA, DPHL—dual-phase heterogeneous lamella, UFG EHEA—ultrafine-grain EHEA, CH EHEA—complex and hierarchical EHEA)[52] (f) phase-selectively recrystallized Ni30Co30Cr10Fe10Al18W2 EHEA (AC—as-cast, FR—fully recrystallization, PSR—phase-selective recrystallization)[54]
Fig.6 Examples of industrial production of EHEA (a) ton-class EHEA ingot prepared by vacuum induction melting (b) 200 mm wide cold-rolled sheet (c) large marine propeller
1
Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes[J]. Adv. Eng. Mater., 2004, 6: 299
2
Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys[J]. Mater. Sci. Eng., 2004, A375-377: 213
3
Miracle D B, Miller J D, Senkov O N, et al. Exploration and development of high entropy alloys for structural applications[J]. Entropy, 2014, 16: 494
4
Otto F, Dlouhý A, Somsen C, et al. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy[J]. Acta Mater., 2013, 61: 5743
5
Senkov O N, Wilks G B, Scott J M, et al. Mechanical properties of Nb25Mo25Ta25W25 and V20Nb20Mo20Ta20W20 refractory high entropy alloys[J]. Intermetallics, 2011, 19: 698
6
Wu S Y, Qiao D X, Zhao H L, et al. A novel NbTaW0.5(Mo2C) x refractory high-entropy alloy with excellent mechanical properties[J]. J. Alloys Compd., 2021, 889: 161800
7
Senkov O N, Scott J M, Senkova S V, et al. Microstructure and room temperature properties of a high-entropy TaNbHfZrTi alloy[J]. J. Alloys Compd., 2011, 509: 6043
8
Lilensten L, Couzinié J P, Perrière L, et al. Study of a bcc multi-principal element alloy: Tensile and simple shear properties and underlying deformation mechanisms[J]. Acta Mater., 2018, 142: 131
Akrami S, Edalati P, Fuji M, et al. High-entropy ceramics: Review of principles, production and applications[J]. Mater. Sci. Eng., 2021, R146: 100644
11
Huang Y, Yeh J W, Yang A C M. “High-entropy polymers”: A new route of polymer mixing with suppressed phase separation[J]. Materialia, 2021, 15: 100978
12
Tiwary C S, Pandey P, Sarkar S, et al. Five decades of research on the development of eutectic as engineering materials[J]. Prog. Mater. Sci., 2022, 123: 100793
13
Lu Y P, Dong Y, Guo S, et al. A promising new class of high-temperature alloys: Eutectic high-entropy alloys[J]. Sci. Rep., 2014, 4: 6200
doi: 10.1038/srep06200
pmid: 25160691
14
Gao X Z, Lu Y P, Zhang B, et al. Microstructural origins of high strength and high ductility in an AlCoCrFeNi2.1 eutectic high-entropy alloy[J]. Acta Mater., 2017, 141: 59
15
Chang I, Cai Q. From simple binary to complex multicomponent eutectic alloys[J]. Prog. Mater. Sci., 2022, 123: 100779
16
Chanda B, Potnis G, Jana P P, et al. A review on nano-/ultrafine advanced eutectic alloys[J]. J. Alloys Compd., 2020, 827: 154226
17
Yan P X, Chang J, Wang W L, et al. Eutectic growth kinetics and microscopic mechanical properties of rapidly solidified CoCrFeNiMo0.8 high entropy alloy[J]. Acta Mater., 2022, 237: 118149
18
Wang X, Zhai W, Li H, et al. Ultrasounds induced eutectic structure transition and associated mechanical property enhancement of FeCoCrNi2.1Al high entropy alloy[J]. Acta Mater., 2023, 252: 118900
19
Lu Y P, Dong Y, Jiang H, et al. Promising properties and future trend of eutectic high entropy alloys[J]. Scr. Mater., 2020, 187: 202
20
Miracle D B, Senkov O N. A critical review of high entropy alloys and related concepts[J]. Acta Mater., 2017, 122: 448
21
Liu W H, He J Y, Huang H L, et al. Effects of Nb additions on the microstructure and mechanical property of CoCrFeNi high-entropy alloys[J]. Intermetallics, 2015, 60: 1
22
He F, Wang Z J, Cheng P, et al. Designing eutectic high entropy alloys of CoCrFeNiNb x [J]. J. Alloys Compd., 2016, 656: 284
23
Jiang H, Han K M, Gao X X, et al. A new strategy to design eutectic high-entropy alloys using simple mixture method[J]. Mater. Des., 2018, 142: 101
24
Lu Y P, Jiang H, Guo S, et al. A new strategy to design eutectic high-entropy alloys using mixing enthalpy[J]. Intermetallics, 2017, 91: 124
25
Chanda B, Das J. An assessment on the stability of the eutectic phases in high entropy alloys[J]. J. Alloys Compd., 2019, 798: 167
26
Jin X, Zhou Y, Zhang L, et al. A new pseudo binary strategy to design eutectic high entropy alloys using mixing enthalpy and valence electron concentration[J]. Mater. Des., 2018, 143: 49
27
Wu Q F, Wang Z J, Hu X B, et al. Uncovering the eutectics design by machine learning in the Al-Co-Cr-Fe-Ni high entropy system[J]. Acta Mater., 2020, 182: 278
28
Jiang H, Li L, Ni Z L, et al. Effect of Nb on microstructure and properties of AlCoCrFeNi2.1 high entropy alloy[J]. Mater. Chem. Phys., 2022, 290: 126631
29
Dong Y, Lu Y P. Effects of tungsten addition on the microstructure and mechanical properties of near-eutectic AlCoCrFeNi2 high-entropy alloy[J]. J. Mater. Eng. Perform., 2018, 27: 109
30
Wang J B, Wang Z J, Shi X B, et al. Alloying behavior of W and Mo in the as-cast dual-phase FeNiCrAl multi-component alloys[J]. J. Alloys Compd., 2023, 951: 169951
31
Chen X H, Xie W Y, Zhu J, et al. Influences of Ti additions on the microstructure and tensile properties of AlCoCrFeNi2.1 eutectic high entropy alloy[J]. Intermetallics, 2021, 128: 107024
32
Chen Z H, Wang J B, Jia Y H, et al. Significantly improving the high-temperature tensile properties of Al17Cr10Fe36Ni36Mo1 alloys by microalloying Hf[J]. Materials, 2023, 16: 6836
33
Jia Y H, Wang Z J, Wu Q F, et al. Boron microalloying for high-temperature eutectic high-entropy alloys[J]. Acta Mater., 2024, 262: 119427
34
Lu Y P, Gao X X, Dong Y, et al. Preparing bulk ultrafine-microstructure high-entropy via alloys direct solidification[J]. Nanoscale, 2018, 10: 1912
35
Huo W Y, Zhou H, Fang F, et al. Microstructure and properties of novel CoCrFeNiTa x eutectic high-entropy alloys[J]. J. Alloys Compd., 2018, 735: 897
36
Ye X C, Lei H F, Liu X W, et al. Design of synergistic alloying CoCrFeNi eutectic high entropy alloy based on infinite solid solution[J]. Mater. Lett., 2023, 343: 134395
37
Liu X, Yang Z S, Cui D C, et al. Enhancing the yield strength of casting eutectic high-entropy alloys via coherent precipitates[J]. Metall. Mater. Trans., 2023, 54A: 4620
38
Jiang H, Jiang L, Qiao D X, et al. Effect of niobium on microstructure and properties of the CoCrFeNbNi x high entropy alloys[J]. J. Mater. Sci. Technol., 2017, 33: 712
doi: 10.1016/j.jmst.2016.09.016
39
Jin X, Liang Y X, Bi J, et al. Enhanced strength and ductility of Al0.9CoCrNi2.1 eutectic high entropy alloy by thermomechanical processing[J]. Materialia, 2020, 10: 100639
40
Lu Y P, Gao X Z, Jiang L, et al. Directly cast bulk eutectic and near-eutectic high entropy alloys with balanced strength and ductility in a wide temperature range[J]. Acta Mater., 2017, 124: 143
41
Dong Y, Yao Z Q, Huang X, et al. Microstructure and mechanical properties of AlCo x CrFeNi3 - x eutectic high-entropy-alloy system[J]. J. Alloys Compd., 2020, 823: 153886
42
Wu Q F, Wang Z J, Zheng T, et al. A casting eutectic high entropy alloy with superior strength-ductility combination[J]. Mater. Lett., 2019, 253: 268
43
Shukla S, Wang T H, Cotton S, et al. Hierarchical microstructure for improved fatigue properties in a eutectic high entropy alloy[J]. Scr. Mater., 2018, 156: 105
44
Lu J, Zhang H, Chen Y, et al. Y-doped AlCoCrFeNi2.1 eutectic high-entropy alloy with excellent oxidation resistance and structure stability at 1000 oC and 1100 oC[J]. Corros. Sci., 2021, 180: 109191
45
Wang L, Yao C L, Shen J, et al. Microstructures and room temperature tensile properties of as-cast and directionally solidified AlCoCrFeNi2.1 eutectic high-entropy alloy[J]. Intermetallics, 2020, 118: 106681
46
Jiang X, Li Y, Shi P J, et al. Synergistic control of microstructures and properties in eutectic high-entropy alloys via directional solidification and strong magnetic field[J]. J. Mater. Res. Technol., 2024, 28: 4440
47
Wischi M, Campo K N, Starck L F, et al. Microstructure and mechanical behavior of the directionally solidified AlCoCrFeNi2.1 eutectic high-entropy alloy[J]. J. Mater. Res. Technol., 2022, 20: 811
48
Shi P J, Li R G, Li Y, et al. Hierarchical crack buffering triples ductility in eutectic herringbone high-entropy alloys[J]. Science, 2021, 373: 912
doi: 10.1126/science.abf6986
pmid: 34413235
49
Guo Y N, Su H J, Zhou H T, et al. Unique strength-ductility balance of AlCoCrFeNi2.1 eutectic high entropy alloy with ultra-fine duplex microstructure prepared by selective laser melting[J]. J. Mater. Sci. Technol., 2022, 111: 298
50
Ren J, Zhang Y, Zhao D X, et al. Strong yet ductile nanolamellar high-entropy alloys by additive manufacturing[J]. Nature, 2022, 608: 62
51
Zhou K X, Li J J, Wu Q F, et al. Remelting induced fully-equiaxed microstructures with anomalous eutectics in the additive manufactured Ni32Co30Cr10Fe10Al18 eutectic high-entropy alloy[J]. Scr. Mater., 2021, 201: 113952
52
Shi P J, Ren W L, Zheng T X, et al. Enhanced strength-ductility synergy in ultrafine-grained eutectic high-entropy alloys by inheriting microstructural lamellae[J]. Nat. Commun., 2019, 10: 489
doi: 10.1038/s41467-019-08460-2
pmid: 30700708
53
Wani I S, Bhattacharjee T, Sheikh S, et al. Tailoring nanostructures and mechanical properties of AlCoCrFeNi2.1 eutectic high entropy alloy using thermo-mechanical processing[J]. Mater. Sci. Eng., 2016, A675: 99
54
Wu Q F, He F, Li J J, et al. Phase-selective recrystallization makes eutectic high-entropy alloys ultra-ductile[J]. Nat. Commun., 2022, 13: 4697
doi: 10.1038/s41467-022-32444-4
pmid: 35948571
55
Xiong T, Zheng S J, Pang J Y, et al. High-strength and high-ductility AlCoCrFeNi2.1 eutectic high-entropy alloy achieved via precipitation strengthening in a heterogeneous structure[J]. Scr. Mater., 2020, 186: 336
56
Lu Y P, Wu X X, Fu Z H, et al. Ductile and ultrahigh-strength eutectic high-entropy alloys by large-volume 3D printing[J]. J. Mater. Sci. Technol., 2022, 126: 15
doi: 10.1016/j.jmst.2022.04.004
57
Reddy S R, Yoshida S, Sunkari U, et al. Engineering heterogeneous microstructure by severe warm-rolling for enhancing strength-ductility synergy in eutectic high entropy alloys[J]. Mater. Sci. Eng., 2019, A764: 138226
58
Wen X, Cui X F, Jin G, et al. In-situ synthesis of nano-lamellar Ni1.5CrCoFe0.5Mo0.1Nb x eutectic high-entropy alloy coatings by laser cladding:Alloy design and microstructure evolution[J]. Surf. Coat. Technol., 2021, 405: 126728
59
Xiao Y K, Chang X P, Peng X H. Low-density NiAlFeCrMoV eutectic high-entropy alloys with excellent mechanical and wear properties[J]. J. Mater. Res. Technol., 2022, 21: 4908
60
Chen X, Qi J Q, Sui Y W, et al. Effects of aluminum on microstructure and compressive properties of Al-Cr-Fe-Ni eutectic multi-component alloys[J]. Mater. Sci. Eng., 2017, A681: 25
61
Zhang Y L, Li J G, Wang X G, et al. The interaction and migration of deformation twin in an eutectic high-entropy alloy AlCoCrFeNi2.1 [J]. J. Mater. Sci. Technol., 2019, 35: 902
doi: 10.1016/j.jmst.2018.09.067
62
Li Y, Shi P J, Wang M Y, et al. Unveiling microstructural origins of the balanced strength-ductility combination in eutectic high-entropy alloys at cryogenic temperatures[J]. Mater. Res. Lett., 2022, 10: 602
63
Li J S, Zhou J, Liu Y F, et al. Microstructural origins of impact resistance of AlCoCrFeNi2.1 eutectic high-entropy alloy[J]. Mater. Sci. Eng., 2024, A890: 145921
64
Bhattacharjee T, Zheng R X, Chong Y, et al. Effect of low temperature on tensile properties of AlCoCrFeNi2.1 eutectic high entropy alloy[J]. Mater. Chem. Phys., 2018, 210: 207
65
Duan X T, Han T Z, Guan X, et al. Cooperative effect of Cr and Al elements on passivation enhancement of eutectic high-entropy alloy AlCoCrFeNi2.1 with precipitates[J]. J. Mater. Sci. Technol., 2023, 136: 97
66
Dong J X, Wu H X, Chen Y, et al. Study on self-lubricating properties of AlCoCrFeNi2.1 eutectic high entropy alloy with electrochemical boronizing[J]. Surf. Coat. Technol., 2022, 433: 128082
67
Miao J W, Wang M L, Zhang A J, et al. Tribological properties and wear mechanism of AlCr1.3TiNi2 eutectic high-entropy alloy at elevated temperature[J]. Acta Metall. Sin., 2023, 59: 267
Miao J W, Yao H W, Wang J, et al. Surface modification for AlCoCrFeNi2.1 eutectic high-entropy alloy via laser remelting technology and subsequent aging heat treatment[J]. J. Alloys Compd., 2022, 894: 162380
69
Peng P, Feng X N, Li S Y, et al. Effect of heat treatment on microstructure and mechanical properties of as-cast AlCoCrFeNi2.1 eutectic high entropy alloy[J]. J. Alloys Compd., 2023, 939: 168843
70
Lu J, Zhang H, Li L, et al. Y-Hf Co-doped AlCoCrFeNi2.1 eutectic high-entropy alloy with excellent oxidation and spallation resistance under thermal cycling conditions at 1100 oC and 1200 oC[J]. Corros. Sci., 2021, 187: 109515
71
Huang Y H, Wang J B, Wang Z J, et al. Corrosion behavior of high strength AlCrFeNi multi-principal-component alloy in lead-bismuth alloy[J]. Nucl. Power Eng., 2023, 44(S1): 137
Han X, Chen Q, Chen Q X, et al. Eutectic dual-phase microstructure modulated porous high-entropy alloys as high-performance bifunctional electrocatalysts for water splitting[J]. J. Mater. Chem., 2022, 10A: 11110
73
Li P, Sun H T, Wang S, et al. Rotary friction welding of AlCoCrFeNi2.1 eutectic high entropy alloy[J]. J. Alloys Compd., 2020, 814: 152322
74
Shen J J, Agrawal P, Rodrigues T A, et al. Gas tungsten arc welding of as-cast AlCoCrFeNi2.1 eutectic high entropy alloy[J]. Mater. Des., 2022, 223: 111176
75
Li P, Sun H T, Dong H G, et al. Microstructural evolution, bonding mechanism and mechanical properties of AlCoCrFeNi2.1 eutectic high entropy alloy joint fabricated via diffusion bonding[J]. Mater. Sci. Eng., 2021, A814: 141211