| (Zr,Ti)(V,Mn,Pd,Ni,Fe)_2系贮氢电极合金的循环稳定性 |
| 杨晓光;雷永泉;张文魁;朱光明;王启东 |
| 浙江大学 |
|
| ELECTROCHEMICAL CYCLING STABILITY OF (Zr,Ti)(V,Mn,Pd,Ni,Fe)_2 HYDRIDE ELECTRODES |
| YANG Hiaoguang; LEI Yongquan; ZHANG Wenkui; ZHU Guangming;WANG Qidong (Zhejiang University; Hangzhou 310027) (Manuscript received 1995-11-21 ; in revised form 1996-04-26) |
引用本文:
杨晓光;雷永泉;张文魁;朱光明;王启东. (Zr,Ti)(V,Mn,Pd,Ni,Fe)_2系贮氢电极合金的循环稳定性[J]. 金属学报, 1996, 32(8): 852-856.
,
,
,
,
.
ELECTROCHEMICAL CYCLING STABILITY OF (Zr,Ti)(V,Mn,Pd,Ni,Fe)_2 HYDRIDE ELECTRODES[J]. Acta Metall Sin, 1996, 32(8): 852-856.
| 1VanHH,BuschowKHJ,MiedemaAR.JLess-CommonMet,1974;53:652藤谷伸,安山茂幸,古川明男,米崎孝.日本金属学会志,1992;56:9653LiZB,LeiYQ,WangQD,WuJ.JLess-CommonMet,1991,172-174:2674SawaH,WakaoS.MaterTransJIM,1990;31:5875LeiYQ,YangXG,WangQD,WuJ.JAlloysComp,1995;231:5736江建军,雷永泉,王春生,吴京,王启东.金属学报,1995;31:B3797GaoXP,SongDY,ZhangYS,WangGS,ShenPW.JAlloysComp,1995,223:7758AuM,PourarianF,SimizuS,SankarSG,ZhangL.JAlloysComp,1995,223:19LeiYQ,YangXG,WangQD,WuJ.TransNonferrousMetSocChina,1995;5:6110ZuttelA,MeliF,SchlapbachL.JAlloysComp,1994;206:3111SakaiT,MiyamuraH,KuriyamaN,IshikawaH,UeharaI.ZPhysChemNeueFolge,1994;183:33312LiangGX,WangED,FangSS.JAlloysComp,1995,223:11113杨晓光.湘江大学博士学位论文,1995 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|