Please wait a minute...
金属学报  1996, Vol. 32 Issue (8): 845-851    
  论文 本期目录 | 过刊浏览 |
PD_3重轨钢氢压裂纹的形核机制
黄一中;黄长河;王燕斌;褚武扬;梅冬生;程兴德;苏世怀;俞梦文
北京科技大学;攀枝花钢铁公司
INITIATION OF HYDROGEN PRESSURE BUBBLES IN STEEL PD_3
HUANG Yizhong; HUANG Changhe;WANG Yanbin; CHU Wuyang (University of Science and Technology Beijing; Beijing 100083); MEI Dongsheng;CHENG Xingde;SU Shihuai; YU Mengwen(Company of Iron and Steel of Panzhihua; Panzhihua617067)(Manuscript received 1995-07-25; in revised form 1996-04-16)
引用本文:

黄一中;黄长河;王燕斌;褚武扬;梅冬生;程兴德;苏世怀;俞梦文. PD_3重轨钢氢压裂纹的形核机制[J]. 金属学报, 1996, 32(8): 845-851.
, , , , , , , . INITIATION OF HYDROGEN PRESSURE BUBBLES IN STEEL PD_3[J]. Acta Metall Sin, 1996, 32(8): 845-851.

全文: PDF(607 KB)  
摘要: 在透射电镜中原位观察了PD_3重轨钢氢气泡及氢压裂纹的形核过程.结果表明,充氢时先形成氢气泡,随氢压增大,周围局部屈服,但在气泡壁附近存在无位错区,其中的应力可能很高.当气泡中的氢压升高到等于被富集氢降低了的原子键合力时,氢压裂纹就在气泡壁上形核.
关键词 : PD_3重轨钢,  氢气泡,  氢压裂纹    
Abstract:The initiating process of the hydrogen bubbles and microcracks caused by the hydrogen pressure was observed by TEM. The results showed that hydrogen charging can generate bubbles and then cause a great reduce of the cohesive strength. As soon as the hydrogen pressure within the bubble reaches to the cohesive strength decreased by hydrogen,microcrack will initiate at the wall of the bubbles. Correspondent: HUANG Yizhong,( Department of Materials Physics, University of Scicnce and Technology Beijing, Beijing 100083)
Key words: steel PD_3    hydrogen bubble    hydrogen pressure microcrack
收稿日期: 1996-08-18     
1陈廉,徐永波,尹万全.金属学报,1978;14:2532陈廉,刘民治,尹万全.金属学报,1979;15:4463褚武扬,肖纪美,李世琼.金属学报,1981;17:104AkhurstKN,PumgheregPH.HydrogeninMetalsPergamon,1977:31315RaviK,RamaswamyV,NamboodhiriTKGMaterSciEng,1993;A169:1116RevieRW,SastriVS,ShehataMT.Corrosion,1993,49:177LimLC.ActaMetall,1987;35:16638蒋兴纲,褚武扬,肖纪美.中国科学,1994;B24:6689TromansD.ActaMetallMaler,1994;42:204310褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社,1988:26811TimosherkS著,徐芝纶、吴永稹合译.弹性理论.北京:高等教育出版社,1964:6312BaiQX,ChuWY,HsiaoJM.SciMetall,1987;21:61313ZhangTY,ChuWY,HisaoJM.MetallTrans,1985;16A:164914ThompsonAW,KnottJN.MetallTrans,1993;24A:52315陈奇志,褚武扬,肖纪美.中国科学,1994;A24:291
[1] 丁宗业, 胡侨丹, 卢温泉, 李建国. 基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究[J]. 金属学报, 2022, 58(4): 567-580.