| 水淬工艺对TWIP钢显微组织和力学性能的影响 |
| 李激光1;丁亚杰1; 彭兴东1;刘津伟2 |
1.辽宁科技大学材料科学与工程学院; 鞍山 114051
2.鞍钢工程事业部; 鞍山 114021 |
|
| EFFECTS OF WATER QUENCHING PROCESS ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF TWIP STEEL |
| LI Jiguang1; DING Yajie1; PENG Xingdong1; LIU Jinwei2 |
1.School of Materials Science and Engineering; University of Science and Technology Liaoning; Anshan 114051
2.Department of Engineering; Anshan Iron and Steel Company; Anshan 114021 |
引用本文:
李激光 丁亚杰 彭兴东 刘津伟. 水淬工艺对TWIP钢显微组织和力学性能的影响[J]. 金属学报, 2010, 46(2): 221-226.
.
EFFECTS OF WATER QUENCHING PROCESS ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF TWIP STEEL[J]. Acta Metall Sin, 2010, 46(2): 221-226.
| [1] Willian P. Adv Mater Process, 2000; 158(5): 38
[2] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438
[3] Vercammen S, Blanpain B, Cooman B C C. J Acta Mater, 2004; 52: 2005
[4] Wang S H, Liu Z Y, Wang G D. J Northeast Univ (Nat Sci), 2008; 29: 1283
(王书晗, 刘振宇, 王国栋. 东北大学学报(自然科学版), 2008; 29: 1283)
[5] Mi Z L, Tang D, Dai Y J, Wang H Q, Li S S. Acta Metall Sin (Engl Lett), 2007; 20: 441
[6] Grassel O, Kruger L, Frommeyer G, Meyer L W. Int J Plast, 2005; 16: 1404
[7] Vercammen S, Blanpain B, Cooman B C,Wollants P. Acta Mater, 2004; 52: 2007
[8] Bouaziz O, Allain S, Scott C. Scr Mater, 2008; 58: 484
[9] Hamada A S, Somani M C, Karjalainen L P. ISIJ Int, 2007; 47: 907
[10] Yang J X. Physical Basis of Metal Plastic Deformation. Beijing: Metallurgical Industry Press, 1988: 185
(杨觉先. 金属塑性变形物理基础. 北京: 冶金工业出版社, 1988: 185)
[11] Fullman R L, Fisher J C. J Appl Phys, 1951; 22: 1350
[12] Form W, Gindraux G, Mlyncar V. Met Sci, 1980; 14: 16
[13] Mackanzie J K. Acta Metall, 1964; 12: 223
[14] Yu Y N. Principles of Metallography. Beijing: Metallurgical Industry Press, 2000: 65
(余永宁. 金属学原理. 北京: 冶金工业出版社, 2000: 65)
[15] Zhu R F, Zhao Z Q, L¨u Y P, Li S T, Wang S Q. J Shangdong Univ Technol, 1997; 27(1): 50
(朱瑞富, 朝志强, 吕宇鹏, 李士同, 王世清. 山东工业大学学报, 1997; 27(1): 50)
[16] Wei X C, Li L, Fu R Y, Shi W. J Iron Steel Rec Int, 2003; 10: 49
[17] Byun T S, Farrell K, Lee E H, Hunn J D, Mansur L K. J Nucl Mater, 2001; 298: 269
[18] Wang Z C, Kim S T, Lee C Q, Lee T H. J Mater Prot Technol, 2004; 151: 141 |
|