| 热等静压和热处理对快凝NiAl--Cr(Mo)--Hf共晶合金显微组织和压缩性能的影响 |
| 盛立远; 郭建亭; 章炜; 谢亿; 周兰章; 叶恒强 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| EFFECTS OF HIP AND HEAT TREATMENT ON MICROSTRUCTURE AND COMPRESSIVE PROPERTIES OF RAPIDLY SOLIDIFIED NiAl-Cr(Mo)-Hf EUTECTIC ALLOY |
| SHENG Liyuan; GUO Jianting; ZHANG Wei; XIE Yi; ZHOU Lanzhang; YE Hengqiang |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
盛立远 郭建亭 章炜 谢亿 周兰章 叶恒强. 热等静压和热处理对快凝NiAl--Cr(Mo)--Hf共晶合金显微组织和压缩性能的影响[J]. 金属学报, 2009, 45(9): 1025-1029.
,
,
,
.
EFFECTS OF HIP AND HEAT TREATMENT ON MICROSTRUCTURE AND COMPRESSIVE PROPERTIES OF RAPIDLY SOLIDIFIED NiAl-Cr(Mo)-Hf EUTECTIC ALLOY[J]. Acta Metall Sin, 2009, 45(9): 1025-1029.
| [1] Miracle D B. Acta Metall Mater, 1993; 41: 649
[2] Noebe R D, Bowman R R. Int Mater Rev, 1993; 38: 193
[3] Guo J T. Ordered Intermetallic Compound NiAl Alloy. Beijing: Science Press, 2003: 104
(郭建亭. 有序金属间化合物NiAl合金. 北京: 科学出版社, 2003: 104)
[4] Misra A, Gibala R. Intermetallics, 2000; 8: 1025
[5] Cline H E, Walter J L. Metall Trans, 1970; 1: 2907
[6] Cline H E, Walter J L, Lifshin E, Russell R R. Metall Trans, 1971; 2: 189
[7] Chen X F, Johnson D R, Noebe R D, Olliver B F. J Mater Res, 1995; 10: 1159
[8] Yang J M, Jeng S M, BainK, Amato R A. Acta Mater, 1997; 45: 295
[9] Guo J T, Cui C Y, Qi Y H, Ye H Q. J Alloys Compd, 2002; 343: 142
[10] Guo J T, Sheng L Y, Tian Y X, Ye H Q. Mater Lett, 2008; 62: 3910
[11] Sheng L Y, Guo J T, Tian Y X, Zhou L Z, Ye H Q. Acta Metall Sin, 2008; 44: 524
(盛立远, 郭建亭, 田玉新, 周兰章, 叶恒强. 金属学报, 2008; 44: 524)
[12] Sheng L Y, Guo J T, Zhou L Z, Ye H Q. Mater Sci Eng, 2009; A500: 238
[13] Cao X W. Physics, 1996; 29: 552
(曹效文. 物理, 1996; 29: 552)
[14] Chen H S, Jackson K A. J Cryst Growth, 1971; 8: 184
[15] Sheng L Y, Guo J T, Ye H Q. Mater Des, 2009; 30: 964
[16] Sheng L Y, Zhang W, Guo J T, Wang Z S, Ye H Q. Mater Des, 2009; 30: 2752
[17] Sheng L Y, Guo J T, Zhou L Z, Ye H Q. J Alloy Compd, 2009; 475: 730
[18] Probst–Hein M, Dlouhy A, Eggeler G. Acta Mater, 1999; 47: 2497
[19] Guo J T, Huai K W, Li H T. Metall Mater Trans, 2007; 38A: 35 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|