晶体学织构对金属板材宏观各向异性影响的模拟 |
花福安; 邸洪双;李建平;刘相华; 王国栋 |
(东北大学轧制技术及连轧自动化国家重点实验室; 沈阳 110004) |
|
SIMULATION OF EFFECTS OF CRYSTALLOGRAPHIC TEXTURES ON THE MACROSCOPIC ANISOTROPY OF METAL SHEET |
HUA Fuan; DI Hongshuang; LI Jianping; LIU Xianghua; WANG Guodong |
State Key Laboratory of Rolling and Automation; Northeastern University; Shenyang 110004 |
引用本文:
花福安 邸洪双 李建平 刘相华 王国栋. 晶体学织构对金属板材宏观各向异性影响的模拟[J]. 金属学报, 2009, 45(6): 657-662.
,
,
,
,
.
SIMULATION OF EFFECTS OF CRYSTALLOGRAPHIC TEXTURES ON THE MACROSCOPIC ANISOTROPY OF METAL SHEET[J]. Acta Metall Sin, 2009, 45(6): 657-662.
[1] Lankford W T, Snyder S C, Bauscher J A. Trans ASM,1950; 42: 1197
[2] Taylor G I. J Inst Met, 1938; 62: 307
[3] Bishop J F W, Hill R. Philos Mag, 1951; 42: 414
[4] Bishop J F W, Hill R. Philos Mag, 1951; 42: 1298
[5] Hill R. Proc R Soc London, 1948; 193A: 281
[6] Hosford W F. J Appl Mech Trans ASME, 1972; 39: 607
[7] Barlat F, Lian J. Int J Plast, 1989; 5: 51
[8] Molinari A, Canova G R, Ahzi S. Acta Metall, 1987; 35:2983
[9] Lebensohn R A, Tom´e C N. Acta Metall Mater, 1993; 41:2611
[10] Kocks U F, Tome C N,Wenk H R. Texture and Anisotropy. Cambridge: Cambridge University Press, 1998: 468
[11] Choi S H, Barlat F. Scr Mater, 1999; 41: 981
[12] Choi S H, Bremi J C, Barlat F, Oh K H. Acta Mater, 2000; 48: 1853
[13] Vicente Alvarez M A, Perez T. Metall Mater Trans, 2007; 38A: 17
[14] Walde T. Int J Refract Met Hard Mater, 2008; 26: 396
[15] Bunge H J. Kristall Technik, 1970; 5: 145
[16] Van Houtte P. Text Microstruct, 1987; 7: 29
[17] Sarma G B , Radhakrishnan B, Zacharia T. Comput Mater Sci, 1998; 12: 105
[18] Savoie J, Jonas J J, Macewen S R, Perrin R. Text Microstruct , 1995; 23: 149
[19] Ren B. PhD Thesis, University of Kentucky, Kentucky, 1994
[20] Choi S H, Cho J H, Barlat F, Chung K, Kwon J W, Oh K H. Metall Mater Trans, 1999; 30A: 337
[21] Lequeu Ph, Gilormini P, Montheillet F, Bacroix B, Jonas J J. Acta Metall, 1987; 35: 1159
[22] Barlat F, Richmond O. Mater Sci Eng, 1987; 95: 15
[23] Barlat F, Maeda Y, Chung K. J Mech Phys Solids, 1997;45: 1727 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|