Please wait a minute...
金属学报  2009, Vol. 45 Issue (6): 657-662    
  论文 本期目录 | 过刊浏览 |
晶体学织构对金属板材宏观各向异性影响的模拟
花福安; 邸洪双;李建平;刘相华; 王国栋
(东北大学轧制技术及连轧自动化国家重点实验室; 沈阳 110004)
SIMULATION OF EFFECTS OF CRYSTALLOGRAPHIC TEXTURES ON THE MACROSCOPIC ANISOTROPY OF METAL SHEET
HUA Fuan; DI Hongshuang; LI Jianping; LIU Xianghua; WANG Guodong
State Key Laboratory of Rolling and Automation; Northeastern University; Shenyang 110004
引用本文:

花福安 邸洪双 李建平 刘相华 王国栋. 晶体学织构对金属板材宏观各向异性影响的模拟[J]. 金属学报, 2009, 45(6): 657-662.
, , , , . SIMULATION OF EFFECTS OF CRYSTALLOGRAPHIC TEXTURES ON THE MACROSCOPIC ANISOTROPY OF METAL SHEET[J]. Acta Metall Sin, 2009, 45(6): 657-662.

全文: PDF(1146 KB)  
摘要: 

基于多晶体黏塑性自洽方法, 建立了金属板材的Lankford 系数(r值)、屈服应力和屈服面的计算模型. 以fcc多晶体为例, 模拟分析了理想织构组分对宏观各向异性的影响. 模拟结果表明, 具有Cube和Goss织构的板材, 其r值在45°附近最小, Cube织构的r值具有对称性, 而Goss织构90°的r值远大于0°的r值; 具有Cu, Bs和S织构的板材, 其最大r值均出现在45°附近, 0°和90°的r值均具有一定的不对称性. 各理想织构的单轴拉伸屈服应力呈现出与r值相对应的变化规律, 屈服面的形状也表现出相应的变化. 上述模拟结果与Taylor--Bishop--Hill (TBH) 模型以及唯象方法的计算结果定性符合.

关键词 : 晶体学织构,  各向异性,  r值,  屈服面,  黏塑性自洽模型    
Abstract:

The macroscopic anisotropies, which are caused primarily by crystallographic textures, have significant effects on the formability of metal sheets and were extensively investigated experimentally and theoretically. Among the numerous theoretical investigations, the phenomenological approach is based on the classical theory of plasticity, in which the plastic behavior of metals is assumed to be well described by analytical functions proposed by Hill, Hosford and Barlat etc.. Because of its simplicity, the phenomenological approach is widely used in finite element method for plastic forming analysis, but this method lacks direct connection between textures and the revealed anisotropies. An alternative is the Taylor--Bishop--Hill (TBH) model which adopts the crystal plastic theory and explicitly takes the crystallographic textures into account, and thus can be used to analyze the anisotropic phenomena on a physical basis. However, implementation of the TBH model into the analysis of industrial forming process is a real tedious task, needing large amount of computational skill and computer resources. Besides, the TBH polycrystalline model does not satisfy the stress equilibrium condition between grains. The viscoplastic self--consistent (VPSC) model for polycrystalline is also a crystal plastic scheme, but it satisfies both strain compatibility and stress equilibrium conditions. In this study, mathematical models for the Lankford coefficient (r value), uniaxial tensile yield stress and yield locus were established based on the polycrystalline VPSC scheme. The effects of ideal crystallographic textures on the macroscopic anisotropy of fcc materials were analyzed. The results show that the minimum r values of Cube and Goss textures appear at an angle of about 45° from the rolling direction (RD), the r values of Cube at 0° and 90° are both approximately equal to unity whereas the r value of Goss at 90° is much higher than that of 0°. For the Cu, Bs and S textures, their maximum r values appear at the angle of about 45° from RD, and their r values of 0° and 90° present some asymmetries. The uniaxial tensile yield stresses of these ideal textures exhibit corresponding characteristics to their r values and the shape of yield locus also varies accordingly. The simulation results are in agreement qualitatively with those of TBH model and phenomenological theory.

Key words: crystallographic texture    anisotropy    r value    yield locus    viscoplastic self--consistent model
收稿日期: 2008-11-24     
ZTFLH: 

TG113.25

 
基金资助:

“十一五”国家科技支撑计划资助项目2006BAE03A08

作者简介: 花福安, 男, 1965年生, 博士

[1] Lankford W T, Snyder S C, Bauscher J A. Trans ASM,1950; 42: 1197
[2] Taylor G I. J Inst Met, 1938; 62: 307
[3] Bishop J F W, Hill R. Philos Mag, 1951; 42: 414
[4] Bishop J F W, Hill R. Philos Mag, 1951; 42: 1298
[5] Hill R. Proc R Soc London, 1948; 193A: 281
[6] Hosford W F. J Appl Mech Trans ASME, 1972; 39: 607
[7] Barlat F, Lian J. Int J Plast, 1989; 5: 51
[8] Molinari A, Canova G R, Ahzi S. Acta Metall, 1987; 35:2983
[9] Lebensohn R A, Tom´e C N. Acta Metall Mater, 1993; 41:2611
[10] Kocks U F, Tome C N,Wenk H R. Texture and Anisotropy. Cambridge: Cambridge University Press, 1998: 468
[11] Choi S H, Barlat F. Scr Mater, 1999; 41: 981
[12] Choi S H, Bremi J C, Barlat F, Oh K H. Acta Mater, 2000; 48: 1853
[13] Vicente Alvarez M A, Perez T. Metall Mater Trans, 2007; 38A: 17
[14] Walde T. Int J Refract Met Hard Mater, 2008; 26: 396
[15] Bunge H J. Kristall Technik, 1970; 5: 145
[16] Van Houtte P. Text Microstruct, 1987; 7: 29
[17] Sarma G B , Radhakrishnan B, Zacharia T. Comput Mater Sci, 1998; 12: 105
[18] Savoie J, Jonas J J, Macewen S R, Perrin R. Text Microstruct , 1995; 23: 149
[19] Ren B. PhD Thesis, University of Kentucky, Kentucky, 1994
[20] Choi S H, Cho J H, Barlat F, Chung K, Kwon J W, Oh K H. Metall Mater Trans, 1999; 30A: 337
[21] Lequeu Ph, Gilormini P, Montheillet F, Bacroix B, Jonas J J. Acta Metall, 1987; 35: 1159
[22] Barlat F, Richmond O. Mater Sci Eng, 1987; 95: 15
[23] Barlat F, Maeda Y, Chung K. J Mech Phys Solids, 1997;45: 1727

[1] 张子轩, 于金江, 刘金来. 镍基单晶高温合金DD432的持久性能各向异性[J]. 金属学报, 2023, 59(12): 1559-1567.
[2] 葛进国, 卢照, 何思亮, 孙妍, 殷硕. 电弧熔丝增材制造2Cr13合金组织与性能各向异性行为[J]. 金属学报, 2023, 59(1): 157-168.
[3] 高钰璧, 丁雨田, 李海峰, 董洪标, 张瑞尧, 李军, 罗全顺. 变形速率对GH3625合金弹-塑性变形行为的影响[J]. 金属学报, 2022, 58(5): 695-708.
[4] 卢磊, 赵怀智. 异质纳米结构金属强化韧化机理研究进展[J]. 金属学报, 2022, 58(11): 1360-1370.
[5] 王迪, 黄锦辉, 谭超林, 杨永强. 激光增材制造过程中循环热输入对组织和性能的影响[J]. 金属学报, 2022, 58(10): 1221-1235.
[6] 左良, 李宗宾, 闫海乐, 杨波, 赵骧. 多晶Ni-Mn-X相变合金的织构化与功能行为[J]. 金属学报, 2021, 57(11): 1396-1415.
[7] 毕胜, 李泽琛, 孙海霞, 宋保永, 刘振宇, 肖伯律, 马宗义. 高能球磨结合粉末冶金法制备碳纳米管增强7055Al复合材料的微观组织和力学性能[J]. 金属学报, 2021, 57(1): 71-81.
[8] 刘金来, 叶荔华, 周亦胄, 李金国, 孙晓峰. 一种单晶高温合金的弹性性能的各向异性[J]. 金属学报, 2020, 56(6): 855-862.
[9] 胡斌,李树索,裴延玲,宫声凯,徐惠彬. <111>取向小角偏离对一种镍基单晶高温合金蠕变性能的影响[J]. 金属学报, 2019, 55(9): 1204-1210.
[10] 王莉,何禹锋,申健,郑伟,楼琅洪,张健. 第二取向对第三代单晶高温合金热疲劳过程中冷却孔孔周氧化行为的影响研究[J]. 金属学报, 2019, 55(11): 1417-1426.
[11] 何贤美, 童六牛, 高成, 王毅超. Nd含量对磁控溅射Si(111)/Cr/Nd-Co/Cr薄膜结构与磁性的影响[J]. 金属学报, 2019, 55(10): 1349-1358.
[12] 马晓琴, 詹清峰, 李金财, 刘青芳, 王保敏, 李润伟. 倾斜溅射对CoFeB薄膜条纹磁畴结构与磁各向异性的影响[J]. 金属学报, 2018, 54(9): 1281-1288.
[13] 黄明亮, 孙洪羽. 倒装芯片无铅凸点β-Sn晶粒取向与电迁移交互作用[J]. 金属学报, 2018, 54(7): 1077-1086.
[14] 王强, 董蒙, 孙金妹, 刘铁, 苑轶. 强磁场下合金凝固过程控制及功能材料制备[J]. 金属学报, 2018, 54(5): 742-756.
[15] 李旭东, 毛萍莉, 刘晏宇, 刘正, 王志, 王峰. 高应变速率下Mg-3Zn-1Y镁合金的各向异性及变形机制[J]. 金属学报, 2018, 54(4): 557-565.