| γ/γ'--αMo定向共晶合金激光快凝的微观组织研究 |
| 金涛;孙晓峰;赵乃仁;刘金来; 张静华; 胡壮麒 |
| (中国科学院金属研究所; 沈阳 110016) |
|
| STUDY OF MICROSTRUCTURES IN γ/γ'--αMo DIRECTIONAL EUTECTOID ALLOY INDUCED BY LASER RAPID MELTING SOLIDIFICATION |
| JIN Tao; SUN Xiaofeng; ZHAO Nairen; LIU Jinlai; ZHANG Jinghua; HU Zhuangqi |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
金涛 孙晓峰 赵乃仁 刘金来 张静华 胡壮麒. γ/γ'--αMo定向共晶合金激光快凝的微观组织研究[J]. 金属学报, 2009, 45(5): 527-535.
,
,
,
,
.
STUDY OF MICROSTRUCTURES IN γ/γ'--αMo DIRECTIONAL EUTECTOID ALLOY INDUCED BY LASER RAPID MELTING SOLIDIFICATION[J]. Acta Metall Sin, 2009, 45(5): 527-535.
| [1] Narasimhan S L, Copley S M, van Stryland E W, Basset M. Metall Mater Trans, 1979; 10A: 654
[2] Gaumann M, Bezencon C, Canalis P, KurzW. Acta Mater,2001; 49: 1051
[3] Yang S, Huang W D, Liu W J, Zhong M L, Zhou Y H. Acta Mater, 2002; 50: 315
[4] Liu W P, Dupont J N. Acta Mater, 2004; 52: 4833
[5] Zhang J H, ZhangY S, Zhang Z Y, Xu Y B, Tang Y J, HuZ Q. Acta Metall Sin, 1983; 19: A309
(张静华, 张玉生, 张志亚, 徐永波, 唐亚俊,胡壮麒. 金属学报, 1983; 19: A309)
[6] Hu Z Q, Zhang J H, Tang Y J,Yu Y, Zhang Y S. ActaMetall Sin, 1985; 21: A329
(胡壮麒, 张静华, 唐亚俊, 于 \ \ 洋, 张玉生. 金属学报, 1985; 21: A329)
[7] Dai J Y, Li D X, Ye H Q, Jin Z X, Zhang J H. J Mater Sci, 1995; 30: 253
[8] Dai J Y, Li D X, Ye H Q, Jin Z X, Zhang J H. J Mater Sci, 1995; 30: 2484
[9] Okamoto P, Thomas G. Acta Mater, 1971; 19: 825
[10] Tendeloo G V, Ridder R D, Amelinckx S. Phys Status Solidi, 1975; 27: 457 |
|