| 定向凝固Ti--43Al--3Si 合金的组织演化规律 II. 稳态生长区组织演化规律 |
| 李新中;樊江磊;郭景杰;苏彦庆;傅恒志 |
| 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001 |
|
| STRUCTURE EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ti--43Al--3Si ALLOY II. Microstructure Evolution in the Steady--State Growth Region |
| LI Xinzhong;FAN Jianglei;GUO Jingjie;SU Yanqing;FU Hengzhi |
| School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001 |
引用本文:
李新中 樊江磊 郭景杰 苏彦庆 傅恒志. 定向凝固Ti--43Al--3Si 合金的组织演化规律 II. 稳态生长区组织演化规律[J]. 金属学报, 2009, 45(3): 308-313.
,
,
,
,
.
STRUCTURE EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ti--43Al--3Si ALLOY II. Microstructure Evolution in the Steady--State Growth Region[J]. Acta Metall Sin, 2009, 45(3): 308-313.
| [1] Dimiduk D M. Mater Sci Eng, 1999; A263: 281
[2] Yamaguchi M, Inui H, Yokoshima S, Kishida K, Johnson D R. Mater Sci Eng, 1996; A213: 25
[3] Kim Y W. JOM, 1994; 4: 14
[4] Zhang Y G, Han Y F, Chen G L, Guo J T, Wan X J, Feng D. Intermetallics Structural Materials. Beijing: National Defence Industry Press, 2001: 705
(张永刚, 韩雅芳, 陈国良, 郭建亭, 万晓景, 冯涤. 金属间化合物结构材料. 北京: 国防工业出版社, 2001: 705)
[5] Johnson D R, Chihara K, Inui H, Yamaguchi M. Acta Mater, 1998; 46: 6529
[6] Chen G L, Lin J P. Ordered Intermetallics Structure Materials. Beijing: Metallurgical Industry Press, 1998: 35
(陈国良, 林均品. 有序金属间化合物结构材料. 北京: 冶金工业出版社, 1998: 35)
[7] Kim S E, Lee Y T, Inui M H, Yamaguichi M. Mater Sci Eng, 2002; A239–331: 25
[8] Kim S E, Lee Y T, Oh M H, Inui H, Yamaguchi M. Intermetallics, 2000; 8: 399
[9] Yamaguchi M, Johnson D R, Lee H N, Inui H. Intermetallics, 2000; 8: 511
[10] Yamanaka T, Johnson D R, Inui H, Yamaguchi M. Intermetallics, 1999; 7: 779
[11] Johnson D R, Masuda Y, Inui H, Yamaguchi M. Acta Mater, 1997; 45: 2523
[12] Johnson D R, Inui H, Yamaguchi M. Acta Mater, 1996; 44: 2523
[13] Lee H N, Johnson D R, Inui H, Oh M H, Wee D M, Yamaguchi M. Mater Sci Eng, 2002; A329–331: 19
[14] Fan J L, Li X Z, Guo J J, Su Y Q, Fu H Z. Acta Metall Sin, 2008; 45: 302
(樊江磊, 李新中, 郭景杰, 苏彦庆, 傅恒志. 金属学报, 2008; 45: 302)
[15] Johnson D R, Inui H, Muto S, Omiya Y, Yamanaka T. Acta Mater, 2006; 54: 1077
[16] Sun F S, Froes F H. Mater Sci Eng, 2003; A345: 262 |
|