金属学报  2009, Vol. 45 Issue (1): 25-31    
  论文 本期目录 | 过刊浏览 |
金属合金等温相变的体激活能及相变机制 I. 钢的中温(贝氏体)等温相变
康沫狂1;张明星2;刘峰1;朱明1
1 西北工业大学材料学院;西安 710072 
2 Division of Materials; School of Engineering; University of Queensland; Brisbane; QLD 4072; Australia
OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM I. Medium Temperature (Bainite) Isothermal Transformation in Steels
KANG Mokuang1; ZHANG Mingxing2; LIU Feng1; ZHU Ming1
1 School of Materials; Northwestern Polytechnical University; Xi'an 710072
2 Division of Materials; School of Engineering; University of Queensland; Brisbane; QLD 4072; Australia
引用本文:

康沫狂 张明星 刘峰 朱明. 金属合金等温相变的体激活能及相变机制 I. 钢的中温(贝氏体)等温相变[J]. 金属学报, 2009, 45(1): 25-31.
. OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM I. Medium Temperature (Bainite) Isothermal Transformation in Steels[J]. Acta Metall Sin, 2009, 45(1): 25-31.

全文: PDF(1109 KB)  
摘要: 

钢的中温(贝氏体)等温处理获得的上、下贝氏体和粒状组织, 都具有各自独立的C曲线;在转变初期均能获得单一的组织, 而在转变的中、后期通常可获得相邻两组织的复合体. 必须用单一组织和Arrhenius关系求相变产物的体激活能. 将体激活能、组织形貌和体自由能曲线相结合可诠释下述论点: 下或上贝氏体是碳原子扩散控制下在奥氏体中的贫碳或极贫碳区, 进行“军队型”(队列式)原子无扩散马氏体样切变相变; 而粒状组织是碳原子扩散控制下在奥氏体中的最贫碳区, 发生“平民型”(非队列式)原子无扩散界面控制相变.

关键词 : 贝氏体相变,  体激活能,  粒状组织,  粒状贝氏体,  马氏体样切变,  界面控制相变,  钢    
Abstract:

Upper bainite, lower bainite and granular structure in isothermally treated steels have all themselves C curves. A single microstructure is always produced in the primary stage, whereas the nearby two-microstructure complex is usually produced in the medium or final stage of the transformation. Only a single microstructure and Arrhenius equation must be used to deduce the overall activation energy for the transformation product. A combination of overall activation energy, morphology and free energy curve can explain the bainitic transformation mechanism and granular structure formation mechanism. The former follows military atom diffusionless martensite-like shear, which occurred in carbon-depleted region controlled by carbon atom diffusion in austenite, and the latter results from civilian atom diffusionless interface control transformation, which occurred in the most carbon--depleted region controlled by carbon atom diffusion in austenite.

Key words: bainite transformation    overall activation energy    granular structure    granular bainite    martensite-like shear    interface control transformation    steel
收稿日期: 2008-04-10     
ZTFLH: 

TG111.5

 
作者简介: 康沫狂, 男, 1920年生, 资深教授

[1] Davenport E S, Bain E C. Trans AIME, 1930; 90: 117
[2] Ko T (柯俊), Cottrel S A. J Iron Steel Inst, 1952; 172: 307
[3] Hillert M. Acta Metall, 1959; 7: 653
[4] Vasudevan P, Graham L W, Axon H J. J Iron Steel Inst,1958; 190: 386
[5] Radcliffe S V, Rollason E C. J Iron Steel Inst, 1959; 191: 56
[6] Yu D G, Shi D K. In: Heat Treatment Institution of CMES, ed., Proc First Conf Heat Treatment Institution of CMES. Beijing: China Machine Press, 1996: 105
(俞德刚, 石德珂. 见: 中国机械工程学会热处理学会主编, 中国机械工程学会热处理学会第1届年会论文集, 北京: 机械工业出版社, 1966: 105))
[7] Barford J. J Iron Steel Inst, 1966; 204: 609
[8] Kang M K, Chen D M, Yang S P, Hu G L. Metall Trans, 1992; 23A: 785
[9] Borgenstam A, Hillert M. Acta Mater, 1997; 45: 651
[10] Gupta C, Dey G K, Chakravatty J K, Srivatav D, Banerjee S. Scr Mater, 2005; 53: 559
[11] Venkatraman M, Mohanty O N, Ghosh R N. Scand J Metall, 2001; 30: 8
[12] Kang M K, Zhu M. Acta Metall Sin, 2005; 41: 673
(康沫狂, 朱明. 金属学报, 2005; 41: 673)
[13] Xu N K, Guan D H, Kang M K. Phys Test Chem Anal (Phys Test), 1983; 19(4): 2
(许念坎, 管敦惠, 康沫狂. 理化检验(物理分册), 1983; 19(4): 2)
[14] Kang M K, Sun J L, Yang Q M. Metall Trans, 1990; 21A: 853
[15] Kang M K, Zhu M, Zhang M X. J Mater Sci Technol, 2005; 21: 437
[16] Wmanski R S, Fikelxichian B N, Blanger M E, Kixiskin S T, Fastov N S, Golerik S S. Physical Metallography. Moscow: Metallurgist, 1955: 376
(Уманский Я С, Финкельштейн  Б Н, Блантер  М  Е, Кишкин  С Т, Фастов Н  С, Горелик С С.  Физическое Металловедение. Москва: Металлургиздата, 1955: 376)
[17] Porter D A, Easterling K E. Phase Transformation in Metals and Alloys. New York: Van Nostrand Reinhold Company, 1981: 172, 349
[18] Hillert M; translated by Lai H Y, Liu G X. Diffusion and Thermodynamics in Alloys. Teaching Materials in Beijing Science and Technology University, Beijing: Metallurgical Industry Press, 1984: 122
(Hillet M著; 赖和怡, 刘国勋译. 合金扩散和热力学. 在北京科技大学讲学稿, 北京: 冶金工业出版社, 1984: 122)[19] Bhadeshia H K D H, Edmonds D V. Metall Trans, 1979; 10A: 895
[20] Hou Z S, Zhao X G, Hou W Y, Liang W. Trans Mater Heat Treat, 2005; 26(3): 6
(侯增寿, 赵兴国, 侯文义, 梁 \ \ 伟. 材料热处理学报, 2005; 26(3): 6)
[21] Wits J J, Kop T A, van Leeuwen Y, Seitsma J, van der Zwaag S. Mater Sci Eng, 2000; A283: 234
[22] Entin РИ; translated by Li P L. Austenite Transformation in Steels. Beijing: China Industry Press, 1965: 167
(Ентин R I著; 李培良译. 钢中奥氏体转变. 北京: 中国工业出版社, 1965: 167 )

[1] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[2] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[3] 张奇亮, 王玉超, 李光达, 李先军, 黄一, 徐云泽. EH36钢在不同粒径沙砾冲击下的冲刷腐蚀耦合损伤行为[J]. 金属学报, 2023, 59(7): 893-904.
[4] 陈润农, 李昭东, 曹燕光, 张启富, 李晓刚. 9%Cr合金钢在含Cl-环境中的初期腐蚀行为及局部腐蚀起源[J]. 金属学报, 2023, 59(7): 926-938.
[5] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[6] 李小涵, 曹公望, 郭明晓, 彭云超, 马凯军, 王振尧. 低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为[J]. 金属学报, 2023, 59(7): 884-892.
[7] 李谦, 刘凯, 赵天亮. 弹性拉应力下Q235碳钢在5%NaCl盐雾中的成锈行为及其机理[J]. 金属学报, 2023, 59(6): 829-840.
[8] 王周头, 袁清, 张庆枭, 刘升, 徐光. 冷轧中碳梯度马氏体钢的组织与力学性能[J]. 金属学报, 2023, 59(6): 821-828.
[9] 赵亚峰, 刘苏杰, 陈云, 马会, 马广财, 郭翼. 铁素体-贝氏体双相钢韧性断裂过程中的夹杂物临界尺寸及孔洞生长[J]. 金属学报, 2023, 59(5): 611-622.
[10] 刘继浩, 周健, 武会宾, 马党参, 徐辉霞, 马志俊. 喷射成形M3高速钢偏析成因及凝固机理[J]. 金属学报, 2023, 59(5): 599-610.
[11] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[12] 王滨, 牛梦超, 王威, 姜涛, 栾军华, 杨柯. 含Cu马氏体时效不锈钢的组织与强韧性[J]. 金属学报, 2023, 59(5): 636-646.
[13] 韩恩厚, 王俭秋. 表面状态对核电关键材料腐蚀和应力腐蚀的影响[J]. 金属学报, 2023, 59(4): 513-522.
[14] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[15] 李民, 王继杰, 李昊泽, 邢炜伟, 刘德壮, 李奥迪, 马颖澈. Y对无取向6.5%Si钢凝固组织、中温压缩变形和软化机制的影响[J]. 金属学报, 2023, 59(3): 399-412.