| 搅拌摩擦加工对铸造7075铝合金微观组织的影响 |
| 刘峰超 马宗义 |
| 中国科学院金属研究所 |
|
| EFFECT OF FRICTION STIR PROCESSING ON THE MICROSTRUCTURE OF CAST 7075 ALUMINUM ALLOY |
引用本文:
刘峰超; 马宗义 . 搅拌摩擦加工对铸造7075铝合金微观组织的影响[J]. 金属学报, 2008, 44(3): 319-324 .
[1]Mishra R S,Mahoney M W,McFadden S X,Mara N A, Mukherjee A K.Scr Mater,2000;42:163 [2]Mishra R S,Mahoney M W.Mater Sci Forum,2001;357- 359:507 [3]Mishra R S,Mahoney M W,McFadden S X,Mara N A, Mukherjee A K.Scr Mater,1999;42:163 [4]Ma Z Y,Mishra R S,Mahoney M W.Acta Mater,2002; 50:4419 [5]Ma Z Y,Mishra R S.Acta Mater,2003;51:3551 [6]Dutta A,Charit L,Johannes L B,Mishra R S.Mater Sci Eng,2005;A395:173 [7]Johannes L B,Mishra R S.Mater Sci Eng,2007;A464: 255 [8]Mishra R S.Adv Mater Processes,2004;162:45 [9]Ma ZY,Mishra RS,Mahoney M W.Scr Mater,2004;50: 931 [10]Charit I,Mishra R S.Acta Mater,2005;53:4211 [11]Johannes LB,Charit I,Mishra R S,Verma R.Mater Sci Eng,2007;A464:351 [12]Ma Z Y,Sharma S R,Mishra R S.Mater Sci Eng,2006; A433:269 [13]Arbegast W J,Hartley P J.In:Proce Fifith Int Conf of Trends in Welding Research,Pine Mounatain,GA,1998: 541 [14]Zhao Y H,Lin S B,Wu L,Qu F X.Mater Lett,2005;59: 2948 [15]Ma Z Y,Sharma S R,Mishra R S.Mater Sci Eng,2006; A433:269 [16]Elangovan K,Balasubramanian V.Mater Design,in press [17]Su J Q,Nelson T W,Sterling C J.Mater Sci Eng,2005; A405:277 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|