郭建亭; 袁超; 侯介山 . 稀土元素在NiAl合金中的作用[J]. 金属学报, 2008, 44(5): 513-520 .
[1]Guo J T,Huai K W,Gao Q,Ren W L,Li G S.Inter- metallics,2007;15:727 [2]Guo J T,Du X H,Li G S.In:Lecomte-Beckers J,Carton M,Schubert F,Ennis P J,eds.,Materials for Advanced Power Engineeing 2006,Jiilich:Forschungszentrum Jülich GmbH,2006:819 [3]Ren W L,Guo J T,Zhou J Y.J Rare Earths,2002;20: 295 [4]Ren W L,Guo J T,Li G S,Zhou J Y.Mater Lett,2003; 57:1374 [5]Ren W L,Guo J T,Li G S,Zhou J Y.J Mater Sci Technol, 2004;20:163 [6]Zhang G Y,Guo J T,Ye H Q.J Chin Rare Earths,2005; 23:75 (张光业,郭建亭,叶恒强.中国稀土学报,2005;23:75) [7]Zhang G Y,Guo J T,Ye H Q.J Aeronaut Mater,2005; 25(2):6 (张光业,郭建亭,叶恒强.航空材料学报,2005;25(2):6) [8]Gao Q,Guo J T,Huai K W,Li H T,Zhang J S.J Mater Sci Technol,2006;22:179 [9]Gao Q,Guo J T.In:Shi C X,Zhong Z Y,eds.,High Temperature Structural Materials.for Power and Energy Application,Beijing:Metallurgical Industry Press,2007: 573 (高强,郭建亭.见:师昌绪,仲增墉主编,动力与能源用高温结构材料,北京:冶金工业出版社,2007:573) [10]Xie Y,Guo J T,Zhou L Z,Liang Y C,Ye H Q.Acta Metall Sin,2008;44:529 (谢亿,郭建亭,周兰章,梁永纯,叶恒强.金属学报,2008;44:529) [11]Liang Y C,Guo J T,Zhou L Z,Xie Y,Hu Z Q.Acta Metall Sin,2008;44:535 (梁永纯,郭建亭,周兰章,谢亿,胡壮麒.金属学报,2008;44:535) [12]Gao Q,Guo J T,Huai K W,Zhang J S.Mater Lett,2005; 59:2859 [13]Sheng L Y,Guo J T,Tian Y X,Zhou L Z,Ye H Q.Acta Metall Sin,2008;44:524 (盛立远,郭建亭,田玉新,周兰章,叶恒强.金属学报,2008;44:524) [14]Chen Y X,Cui C Y,He L L,Guo J T,Li D X.Acta Metall Sin,1999;35(Suppl.2):S444 (陈玉喜,崔传勇,贺连龙,郭建亭,李斗星.金属学报,1999;35(增刊2):S444) [15]Rare Earths Research Group.Rare Eart.Vol.2,Beijing: Metallurgical Industry Press,1978:25 (《稀土》编写组.稀土(下).北京:冶金工业出版社,1978:25) [16]Cine H E,Walter J L,Koch E F,Osika L M.Acta Metall, 1971;19:405 [17]Chen X F,Johson D R,Noebe R D,Oliver B F.J Mater Res,1995;10:1159 [18]Guo J T.Ordered Intermetallic Compound NiAl Alloy. Beijing:Science Press,2003:58 (郭建亭.有序金属间化合物镍铝合金.北京:科学出版社,2003:58) [19]Guo J T,Xu C M.Oxid Met,2002;58:457 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|