| 定向凝固Ni-20Al-30Fe合金变形的TEM原位观察 |
| 张万明 郑启 孙晓峰 于洋 胡壮麒 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
张万明; 郑启; 孙晓峰; 于洋; 胡壮麒 . 定向凝固Ni-20Al-30Fe合金变形的TEM原位观察[J]. 金属学报, 1999, 35(4): 375-378 .
[1] Inoue A, Masumoto T, TOmioka H. J Mater Set, 1984; 19:3097 [2] Guha S, Munroe P R, Baker I. Mater Sci Egg, 1991; A131:127 [31 Huang S C, Field R D, Krueger D D. Metall aams, 1990;21A: 959 [4] Misra A, Gibala R. Metall Mater Trans,1997; 28A: 795 [5] Chen J, Zheng Q, Li Y A, Yu Y, Tang Y J, Hu Z Q. ScrMetall Mater, 1995; 33: 675 [6] Misra A, Kim J T, Gibala R. Metall Mater frans, 1997; 28A:135 [7] Darolia R, Lahrman D, Field R D. Scr Metall Mated 1992;26: 1007 [8] Brzeski J M, Hack J E, Darolia R D, Field R D. Mater SciEng, 1993; 170A: 11 [9] Levit V I, Bul I A, Hu J, Kaufinan M J. Scs Mated 1996;34: 1925 [10] Shen Z, Wagoner R H, Clark W A T. Acta Metall, 1988; 36:3231 [11] Lee T C, Robertson I M, Birnbaum H K. Metall Trans,1990;21A: 2437 [12] Noebe R D, misra A, Gibala R. ISIJ Int,1991; 31: 1172 [13] Das E S P, Marcinkowskj M J. Mater Set Eng, 1971; 8: 189 [14] Hingwt A K, Subraznanian K N. i Mater Sci, 1975; 10: 183 [15] Nilsen C F, Subramanian K N. i Mater Set, 1984; 19: 748N |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|