| Cu-Zn-Al双程记忆合金中Ⅱ类孪晶的界面观察 |
| 刘明 张修睦 |
| 四川联合大学金属材料系;成都 610065 |
|
引用本文:
刘明; 张修睦 . Cu-Zn-Al双程记忆合金中Ⅱ类孪晶的界面观察[J]. 金属学报, 1999, 35(4): 371-374 .
[1] Schroeder T A, Wayman C M. Acta Metall, 1977; 25: 1375 [2] Adachi K, Perkins J. Metall Trans,1985; 16A:1551 [3] Kajiwara S, Nishiyama i. Jpn J Appl Phys, 1964; 3: 749 [4] Delaey L, Warlimont H. Z Metallkd, 1966; 57: 793 [5] Otsuka K, Shimizu K. Trans Jpn Inst Met, 1974; 15:109 [6] Schroeder T A, Wayman C M. Acta Metall, 1977; 25: 1375 [7] Chakrovorty S, Wayman C M. Metall aams, 1976; 7A: 569 [8] Katata T, Saka H. PhiloB Mag, 1989; A59: 677 [9] Lovey F C, Van Tendeloo G, Van Landuyt J, Amelinckx S.Scs Metall, 1985; 19: 1223 [10] Cook J M, O'Keefe M A, Smith D J, Stobbs W M. i Microsc,1983; 129: 295 [11] Otsufor K. jpn J Acal Phal, 1971; 10: 571 [12] Tas H, Delaey L, Deruyttere A. Metall bens, 1973; 4: 2833 [13] Saburi T, Nenno S. In: Wayman C M ed., Proc Int Conf onSolid to Solid Phase Transformations,New York: AmericanInstitute of Mine Engineerings, 1982: 1455 [14] Liu M, Zhang X M, Liu M Z, Liu R S. Acta Metall Sin (EnglLett), 1997; 10: 157 [15] Liu M, Zhang X M, Liu M Z, Li Y Y. In: C-MRS eds., Sym-posia Proc 1996 C-MRS. I-3, Beijing: Chemistry IndustryPress, 1996: 296 [16] Hara T, Ohba T, Otsuka K, Bando Y, Nenno S. In: PerkinsJ ed., ICOMAT-92, California: Monterey institute of Ad-vanced Studies, 1992: 257 [17] Nishda M, Yamauchi K, Itai I, Ohgi H, Chiba A. Acta MetallMated 1995; 43: 1229 [18] Zhang J X, Cai W, Zheng Y F, Zhao L C. Mater Lett, 1998;34: 351 [19]Yang J H, Liu M Z, Li N. i Funct Mater, 1993; 3: 255(杨晋红,刘民治,李宁.功能材料,1993;3: 255) [20] Liu M Z, Huang W X, Liu R S, Li N. In: Xu X, Yao X eds.,'94 Chinese Natural Science FOundation intellectual Facul- ties Condrence Proceedings, Chengdu: Chengdu ElectrollicScience & Technology University Publishers, 1994: 29(刘民治,黄婉霞,刘蓉生,李宁.见:徐熹,姚希主编,'94 国家自然科学基金智能材料研讨会文集,成都:成都电子科技大学出版社,1994: 29) [21] Pirouz P, Yang J W. Ultramicroscopy, 1993; 51: 189 [22] Wang R H, Luo C P, Gui J N, Ren Q, Chen J. J Phys:Condens Matted 1992; 4: 2397 [23] Jaswon M A, Dove D B. Acta Crystallopn 1960; 13: 232 [24] Adachi K, Perkins J, Wayman C M. Acta Metall, 1986; 34:24 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|