| Ti-55合金中的热塑剪切带 |
| 禹金强 沈乐天 周惠华 徐永波 白以龙 |
| 中国科学院金属研究所疲劳和断裂国家重点实验室; 沈阳 110015 |
|
引用本文:
禹金强; 沈乐天; 周惠华; 徐永波; 白以龙 . Ti-55合金中的热塑剪切带[J]. 金属学报, 1999, 35(4): 379-383 .
[1]Rogres H C. Ann Rev Mater Sci,1979; 9: 283 [2] Wittman C L,Meyers M A, Pak R H. Metall Trans,1990;21A: 706 [3] Giovanola J H. Mech Mated 1988; 7: 73 [4] Xu Y B, Bai Y L, Xue Q, Shen L T. Acta Mated 1996; 44:1917 [5] Zurek A K. Metall Tans,1994; 25A: 2483 [6] Cho K, Chi Y C, Duffy J. Metall Trans,1990; 21A: 1161 [7] Glenn R C, Leslie W C. Metall Trans, 1971; 2: 2945 [8] Wingrove A L. J Aust Inst Met, 1971; 16: 67 [9] Meyers M A, Wittman C L. Metall Trans,1990; 21A: 3153 [10] Hartley K A, Duals J, Hawley R H. J Mech PheS Solids,1987; 35: 283 [11] Giovanola J H. MeCh Mater, 1988; 7: 59 [12] Zhong W L, Zhang Y, Xu Y B, Shen L T, Bat Y L. ActaMetall Sin, 1999; 35: 384(钟万里,张匀,徐永波,沈乐天,白以龙.金属学报,1999;35: 384) [13] Stock T A C, Wingrove A L. J Mech Ear Sci,1971; 13: 110 [14] Timothy S P, Hutchings J M. In: Blazynski T E ed., Proc7th Int Conf on High Enerpy Rate Fabrication, University ofBeeds., 1981: 9 [15] Staish V K, Prasad Y V, Biswas R K. Metall Mater Trans,1994; 25A: 2173 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|